Mg合金的最新发展及应用前景
曾荣昌  柯伟  徐永波  韩恩厚  朱自勇
中国科学院金属研究所金属腐蚀与防护国家重点实验室;沈阳110016
引用本文:

曾荣昌; 柯伟; 徐永波; 韩恩厚; 朱自勇 . Mg合金的最新发展及应用前景[J]. 金属学报, 2001, 37(7): 673-685 .

全文: PDF(540 KB)  
摘要: 分析了当前Mg及Mg合金的发展状况及趋势,简要介绍了Mg合金及其合金化的特点、常见种类及其使用范围和成分、组织及力学性能特征;着重阐述了Mg合金的腐蚀问题及其防护方法;并详细介绍和讨论了Mg合金在电脑和汽车工业上的应用状况及发展前景;最后,对Mg合金研究的有关问题提出了一些建议.
关键词 : Mg合金,  腐蚀,  防护,  汽车工业    
Key words:
收稿日期: 2001-02-15     
ZTFLH:  TG146.2  
[1] Ball L C J. J Inst Met, 1955; 84: 399
[2] Petersen N H. Proc 47th Annual World Magnesium Conference, McLeen, Virginia: International Magnesium Association (IMA), 199O: 18
[3] Clow B B. Proc Int Conf On Magnesium Alloys and TheirApplications, Oberursel, Germany: DGM Informationsge-sellschagt, 1992: 13
[4] Stanner R J L. Am Sci, 1976; 64: 258
[5] Yang Z C. Ind Mater, 1999; 152: 72(杨智超.工业材料,1999;152:72)
[6] Shigler C M. J Met, 1951; 3: 25
[7] Bailey K G. Proc 40th World Magnesium Conference,Dayton: IMA, 1983: 64
[8] Nemoto S. J Jpn Inst Light Met, 1999; 49: 580(根本 茂.轻金属,1999;49:580)
[9] Brown R E. Light Met Age, 1990; 48(7/8): 6
[10] Brown R E. Light Met Age, 1991; 49(7/8): 6
[11] Brown R E. Light Met Age, 1992; 50(5/6): 21
[12] Brown R E. Light Met Age, 1996; 54(7/8): 50
[13] Froes P H. JOM, 1998; 11: 54
[14] Brown R E. Light Met Age, 1992; 50(5/6): 18
[15] Tsukeda T. J Jpn Inst Light Met, 2000; 50: 254(附田之欣.轻金属,2000;50:254)
[16] Brown R E. Light Met Age, 2000; 58(7/8): 100
[17] Pawlek R P. Metall, 2000; 54: 96
[18] Brown R E. Light Met Age, 2000; 58(3/4): 54
[19] Song G. Ady Egg Mater, 1999; 1: 11
[20] Cui K. Ferrous Materials and Nonferrous Materials. Bei1981: 385)(崔昆,钢铁材料及有色金属材料.北京:机械工业出版社,
[21] Wang Q, Lu Y, Zeng X, Ding W, Zhu Y. Trans NonferrousMet Soc Chin, 1999; 10: 235
[22] Froats A, Aune T K, Hawke D, Unsworth W, Hillis J. In:Metals Handbook, Vol.13, 9 ed., Metals Park, Ohio: ASM,1987: 740
[23] Pomear I J. Light Alloys: Metallurgy of the Light Metals.2 ed., London: Edward Arnold, 1989
[24] Kamdo S, Kojima Y. Mater Jpn, 1999: 38: 286
[251 Baker H. Metals Handbook, Vol.2, 9 ed., Metals Park,Ohio: ASM, 1987: 24
[26] Wei L Y, Dunlop G L, Westengen H. Mater Sci Technol,1996; 12: 741
[27] Villars P, Calvert L O. Pearson's Handbook of Crystallographic Data for Intermetallic Phases. Metals Park,Ohio: ASM, 1985: 1016
[28] Villars P, Calvert L O. Pearson's Handbook of Crystallographic Data for Intermetallic Phases. Metals Park,Ohio: ASM, 1985: 920
[29] Petersen G, Westengen H, Hoier R, Lohne O. Matal SciEng, 1996; 207 A: 115
[30] Fukizawa K, Koike S, Shibata K. Mater Jpn, 2000; 39:17
[31] Ohya T, Takai A. Mater Jpn, 2000; 39: 878
[32] Wei L Y, Dunlop G L, Westengen H. Metall Mater Trans,1995; 26A: 1947
[33] Zhang Z, Couture A. Scr Mater, 1998; 39: 45
[34] Horie T, Iwahori H, Awano Y, Matsui A. J Jpn Inst LightMet, 1999; 49: 272(崛江俊男,岩掘弘昭,粟野洋司,松井 彰.轻金属,1999;49:272)
[35] Chang S Y, Tezuha H, Kamio A. Mater Trans JIM, 1997;38: 526
[36] Bamberger M. Mater Sci Technol, 2001; 17: 15
[37] Fleteren R V. Adv Mater Proc, 1996; 5: 33
[38] Clark J B. Acta Metall, 1968; 16: 141
[39] Partridge P. Metall Rev, 1967; 118: 169
[40] Perov S N, Orgarvic V V, Stephens R I. J Eng MaterTechnol, 1993; 115: 391
[41] Liu Z, Wang Y, Wang Z G, Li F, Shen Z Y. Chin J MaterRes, 2000; 14: 449(刘正,王越,王中光,李峰,申志勇.材料研究学报,2000;14:449)
[42] Mayer H, Lipowsky H, Papakyriacou M, Rosch R, StichA, Zettl B, Tschegg S S. In: Wu X R, Wang Z G eds.,Proc 7th Int Fatigue Congress, Beijing: Higher EducationPress, 1999: 2059
[43] Orgarevic V V, Stephens R I. Ann Rev Mater Sci, 1990;20: 141
[44] Bhambri A K, Kattamis T Z. Metall Trans, 1971; 2: 1689
[45] Yue T M, Ha H U, Musson N J. J Mater Sci, 1995, 30:2277
[46] Eisenmeier G, Ottmueller M, Hoeppel H W, MughrabiH. In: Wu X R, Wang Z G eds., Proc 7th Int FatigueCongress, Beijing: Higher Education Press, 1999: 253
[47] Kobayashi Y, Takano T, Ishikawa K. In: Wu X R, WangZ G eds., Proc 7th Int Fatigue Congress, Beijing: HigherEducation Press, 1999: 2273
[48] Zhu R Z. Corrosion of Metal. Beijing: Metallurgical Industry Press, 1993: 14(朱日彰,金属腐蚀学.北京:冶金工业出版社.1993:14)
[49] Wu X L. Ph Dissertation, Institute of Corrosion andProtection of Metals, The Chinese Academy of Sciences,Shenyang, 1999(武显亮.中国科学院金属腐蚀与防护研究所博士学位论文,沈阳:1999)
[50] Skar J I. Mater Corros, 1999; 50: 2
[51] Maker G L, Kruger J. Int Mater Rev, 1993; 38: 138
[52] Emley E F. Principles of Magnesium Technology. NewYork: Pergamon Press, 1966
[53] Tunold R, Holtan H, Berfe M B H, Lasson A, Hassen RS. Corros Sci, 1977; 17: 353
[54] Albright D L. In: Paris H G, Hunt W H eds., Advancesin Magnesium Alloys and Composites, Phoenix, Arizona:International Magnesium Association and the Non-ferrousMetals Committee, TMS, 1988: 57
[55] Hoch G M. Int Corros Conf Series, Vol.3, Houston, TX:NACE, 1974; 3: 134
[56] Nisancioglu K, Lunder O, Aune T K. Proc 47th AnnualWorld Magnesium Conference, McLeen, Virginia: IMA,1990: 43
[57] Lunder O, Lein J E, Hesjevik S M, Aune T Kr, NisanciogluK. Werkst Korros, 1994; 45: 331
[58] Lubbert K, Kopper J, Wendler-Kalsch E. Mater Corros,1999; 50: 65
[59] Miller W K. In: Jones R H ed., Stress Corrosion Cracking,Metals Park, Ohio: ASM, 1993: 251
[60] Heidenreich R D, Gerould C H, McNulty R E. TransAIME 1946; 166: 15
[61] Fairman L, Bray H J. Corros Sci, 1971; 11: 533
[62] Fairman L, Bray H J. Br Corros J, 1971; 16: 170
[63] Priest D K. In: Robertson D ed., Stress Corrosion Cracking and Embrittlement, New York: Wiley, 1956: 81
[64] Partridge P G. Philos Mag, 1965; 12: 1043
[65] Oryall G, Tromans D. Corrosion, 1971; 27: 334
[66] Wearmouth W R, Dean G P, Parkins R N. Corrosion,1973; 29: 251
[67] Chakrapani D G, Pugh E N. Corrosion, 1975; 31: 247
[68] Ebtehaj K, Hardie D. Corros Sci, 1988; 28: 811
[69] Speidel M O, Blackburn M J, Beck T R, Feeney J A. In:Devereux O ed., Corrosion Fatigue: Chemistry, Mechanics, and Microstructure, Houston, TX: NACE, 1986: 331
[70] Stephens R I, Schrader C D, Lelase K B. J Egg MaterTechnol, 1995; 117: 293
[71] Mayer H, Papakyriacou M, Stanzl-Tschegg S, Tschegg E,Zettl B, Lipowsky H, Rosch R, Stich A. Mater Corros,1999; 50: 81
[72] Mayer H R, Lipowsky H, Papakyriacou M, Rosch R, StichA, Stanzl-Tschegg S. Fatigue Fract Eng Mater Struct,1999; 22: 591
[73] You B S, Park W W, Chung I S. Scr Mater, 2000; 42:1089
[74] Cole G S. In: Ding W N ed., Papers of Sinomag DieCasting Magnesium Seminar Sinochem Beijing EasternGarden, Beijing, 2000: 213
[75] Zeng A P, Xue Y, Qian Y F. Corros Protect, 2000; 21: 56(曾爱平, 薛颖, 钱宇峰. 腐蚀与防护, 2000; 21: 56)
[76] AshworthV, Proctor R P M, Garnt W A. In: Hirvonen J K ed., Ion implantation, Treatise on Materials Science and Technology, New York: Academic Press, 1980: 176
[77] Nakatsugawa I, Martin R, Knystautas E J. Corrosion,1996; 52: 921
[78] Hagans P L. 41th World Magnesium Conf Dayton, Ohio:IMA, 1984: 30
[79] Cai X F. Ind Mater, 1999; 152: 62(蔡幸甫. 工业材料, 1999; 152: 62)
[80] Europaische Forschungsgemeinschaft Magnesiumgusse. V.5. Magnesiumguss Abnehmerseminar und AutomotiveSeminar, Aalen, IMA, 1997
[81] Ruden T J, Albright D L. Ady Mater Proc, 1994; 145: 28
[82] Demmier A. Eur Automot Compon Bus, 1997, 1: 102
[83] Polmear I J. Mater Sci Technol, 1994; 10: 1
[84] Cole G S. In: Ding W N ed., Papers of Sinomag DieCasting Magnesium Seminar Sinochem Beijing EasternGabbed, Beijing, 2000: 1
[1] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] 司永礼, 薛金涛, 王幸福, 梁驹华, 史子木, 韩福生. Cr添加对孪生诱发塑性钢腐蚀行为的影响[J]. 金属学报, 2023, 59(7): 905-914.
[3] 张奇亮, 王玉超, 李光达, 李先军, 黄一, 徐云泽. EH36钢在不同粒径沙砾冲击下的冲刷腐蚀耦合损伤行为[J]. 金属学报, 2023, 59(7): 893-904.
[4] 王宗谱, 王卫国, Rohrer Gregory S, 陈松, 洪丽华, 林燕, 冯小铮, 任帅, 周邦新. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2023, 59(7): 947-960.
[5] 陈润农, 李昭东, 曹燕光, 张启富, 李晓刚. 9%Cr合金钢在含Cl-环境中的初期腐蚀行为及局部腐蚀起源[J]. 金属学报, 2023, 59(7): 926-938.
[6] 赵平平, 宋影伟, 董凯辉, 韩恩厚. 不同离子对TC4钛合金电化学腐蚀行为的协同作用机制[J]. 金属学报, 2023, 59(7): 939-946.
[7] 李小涵, 曹公望, 郭明晓, 彭云超, 马凯军, 王振尧. 低碳钢Q235、管线钢L415和压力容器钢16MnNi在湛江高湿高辐照海洋工业大气环境下的初期腐蚀行为[J]. 金属学报, 2023, 59(7): 884-892.
[8] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[9] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.
[10] 王京阳, 孙鲁超, 罗颐秀, 田志林, 任孝旻, 张洁. 以抗CMAS腐蚀为目标的稀土硅酸盐环境障涂层高熵化设计与性能提升[J]. 金属学报, 2023, 59(4): 523-536.
[11] 韩恩厚, 王俭秋. 表面状态对核电关键材料腐蚀和应力腐蚀的影响[J]. 金属学报, 2023, 59(4): 513-522.
[12] 夏大海, 计元元, 毛英畅, 邓成满, 祝钰, 胡文彬. 2024铝合金在模拟动态海水/大气界面环境中的局部腐蚀机制[J]. 金属学报, 2023, 59(2): 297-308.
[13] 廖京京, 张伟, 张君松, 吴军, 杨忠波, 彭倩, 邱绍宇. Zr-Sn-Nb-Fe-V合金在过热蒸汽中的周期性钝化-转折行为[J]. 金属学报, 2023, 59(2): 289-296.
[14] 常立涛. 压水堆主回路高温水中奥氏体不锈钢加工表面的腐蚀与应力腐蚀裂纹萌生:研究进展及展望[J]. 金属学报, 2023, 59(2): 191-204.
[15] 胡文滨, 张晓雯, 宋龙飞, 廖伯凯, 万闪, 康磊, 郭兴蓬. 共晶高熵合金AlCoCrFeNi2.1 在H2SO4 溶液中的腐蚀行为[J]. 金属学报, 2023, 59(12): 1644-1654.