| 单晶与多晶NbSi2在1023 K氧化行为的对比 |
| 张 芳;张澜庭;郁金星;吴建生 |
| 上海交通大学材料科学与工程学院教育部高温材料及测试重点实验室; 上海 200030 |
|
| A Comparison of the Oxidation Behaviors of Poly-Crystalline and Single Crystalline NbSi2 at 1023 K |
| ZHANG Fang; ZHANG Lanting; YU Jinxing; WU Jiansheng |
| Key Laboratory of the Ministry of Education for High Temperature Materials and Testing; School of Materials Science and Engineering; Shanghai Jiaotong University; Shanghai 200030 |
引用本文:
张芳; 张澜庭; 郁金星; 吴建生 . 单晶与多晶NbSi2在1023 K氧化行为的对比[J]. 金属学报, 2005, 41(6): 645-648 .
,
,
,
.
A Comparison of the Oxidation Behaviors of Poly-Crystalline and Single Crystalline NbSi2 at 1023 K[J]. Acta Metall Sin, 2005, 41(6): 645-648 .
[1]Shah D M,Berczik D.Mater Sci Eng,1992;A155:45 [2]Tanaka K,Nawata K,Inui H,Yamaguchi M,Koiwa M.Intermetallics,2001;9:603 [3]Fitzer V E.In:Benesovsky F,ed.,Plansee Proc 2nd Seminar Reutte/Tyrol,Vienna:Springer,1955:56 [4]Berztiss D A,Cerchiara R R,Gulbransen E A,Pettit F S,Meier G H.Mater Sci Eng,1992;A155:165 [5]Schlichting J.High Temp High Pressures,1978;10:241 [6]Yanagihara K,Przybylski K,Maruyama T.Oxid Met,1997;47:277 [7]Rausch J J.Report No.ARF 2981-4.Armour Research Foundation,Chicago,IL,1961 [8]Pitman S H,Tsakiropoulos P.Mater Res Symp Proc,1995;364:1321 [9]Murakami T,Sasaki S,Ichikawa K,Kitahara A.Inter- metallics,2001;9:621 [10]Zhou J W.Master Dissertation,Shanghai Jiaotong University,2004 (周健威.上海交通大学硕士学位论文,2004) [11]Murakami T,Xu C N,Kitahara A,Kawahara M,Taka-hashi Y,Inui H,Yamaguchi M.Intermetallics,1999;7:1043 [12]Murakami T,Sasaki S,Ichikawa K,Kitahara A.Intermetallics,2001;9:629 [13]McKamey C G,Tortorelli P F,De Van J H,Carmichael C A.J Mater Res,1992;7:2747 [14]Chou T C,Nieh T G.J Mater Res,1993;8:214 [15]Shan A D,Fang W,Hashimoto H,Park Y-H.Scr Mater,2002;46:645 [16]Sannia M,Orru R J,Garay E,Gao G Z,Munir A.Mater Sci Eng,2003;A345:270 [17]Hiroyuki S,Masaru Y,Ken H,Osamu Y.Mater Res Bull,2002;37:1557 [18]Li M S.High Temperature Corrosion of Metals.Beijing:Metallurgical Industry Press,2001:36 (李美栓.金属的高温腐蚀.北京:冶金工业出版社,2001:36) [19]Kurokawa K,Houzumi H,Saeki I,Takahashi H.Mater Sci Eng,1999;A261:292 [20]Liu Y Q,Shao G,Tsakiropolo P.Intermetallics,2001;9:125\ |
|