| 表面机械研磨处理后316L不锈钢的表层结构及硬度的热稳定性 |
| 王爱香;刘 刚;周 蕾;王 科;杨晓华;李 瑛 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室;沈阳 110016;福州大学材料科学与工程学院;福州 350002 |
|
| Thermal Stability of Structure and Hardness of the Surface Layer of 316L Stainless Steel After Surface Mechanical Attrition Treatment |
| WANG Aixiang; LIU Gang; ZHOU Lei; WANG Ke; YANG Xiaohua; LI Ying |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016;School of Materials Science and Engineering; Fuzhou University; Fuzhou 350002 |
引用本文:
王爱香; 刘刚; 周蕾; 王科; 杨晓华; 李瑛 . 表面机械研磨处理后316L不锈钢的表层结构及硬度的热稳定性[J]. 金属学报, 2005, 41(6): 577-582 .
,
,
,
,
,
.
Thermal Stability of Structure and Hardness of the Surface Layer of 316L Stainless Steel After Surface Mechanical Attrition Treatment[J]. Acta Metall Sin, 2005, 41(6): 577-582 .
[1]Lu K,Lu J.J Matr Sci Technol,1999;15:193 [2]Lu K,Lu J.Mater Sci Eng,2004;A375-377:38 [3]Wu X,Tao N,Hong Y,Xu B,Lu J,Lu K.Acta Mater,2002;50:2075 [4]Tao N R,Wang Z B,Tong W P,Sui M L,Lu J,Lu K.Acta Mater,2002;50:4603 [5]Zhang H W,Hei Z K,Liu G,Lu J,Lu K.Acta Mater,2003;51:1871 [6]Yong X P,Liu G,Lu K,Lu J.J Mater Sci Technol,2003;19:1 [7]Liu G,Wang S C,Lou X F,Lu J,Lu K.Scr Mater,2001;44:1791 [8]Lu K.Mater Sci Eng,1996;R16:161 [9]Lu A Q,Liu G,Liu C M.Acta Metall Sin,2004;40:943 (吕爱强,刘刚,刘春明.金属学报,2004;40:943) [10]Ya M,Xing Y M,Dai F L,Lu K,Lu J.Surf Coat Technol, 2003;168:148 [11]Olson G B,Cohen M.Metall Trans,1975;6A:791 [12]Lin G Y,Han F,Yu J W,Peng X M,Ye L Y,Peng D S.Heat Treat Met,2004;29(3):8 (林高用,韩飞,余均武,彭小敏,叶凌英,彭大暑.金属热处理,2004;29(3):8) [13]Shewmon P G.Transformation in Metals.New York:McGraw-Hill Book Co.,1969:116 [14]Klement U,Erb U,El Sherik A M,Aust K T.Mater Sci Eng,1995;A203:177 [15]Surganaragana C,Froes F H.Nanostruct Mater,1992;11:196 [16]Lian J S,Valiev R Z,Baudelet B.Acta Metall Mater,1995;43:4165 [17]Inami T,Okuda S,Maeta H,Ohtsuka H.Mater Trans JIM,1998;39:1029 [18]Lu K,Wang J T,Wei W D.J Phys,1992;25D:808 [19]Lu K,Dong Z F,Bakonyi I,Cziraki A.Acta Metall Mater,1995;43:2641 [20]Eckert J,Holzen J C,Johnson W L.J Appl Phys,1993;73:131 |
|