| Nb对Zr基大块非晶合金热稳定性、非晶形成能力及机械性能的影响 |
| 孙 民 王敬丰 刘 兵 柳 林 |
| (华中科技大学材料科学与工程学院 塑性成型及模具技术国家重点实验室;武汉 430074) |
|
引用本文:
孙民; 王敬丰; 刘兵; 柳林 . Nb对Zr基大块非晶合金热稳定性、非晶形成能力及机械性能的影响[J]. 金属学报, 2005, 41(5): 534-538 .
[1] Inoue A, Ohtere K, Kita K, Masumoto T. Jpn J Appl Phys, 1988; 27: L2248 [2] Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1989; 30: 965 [3] Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1990; 31: 177 [4] Peker A, Johnson W L. Appl Phys Lett, 1993; 63: 2342 [5] Inoue A, Gook J S. Mater Trans JIM, 1995; 36: 1180 [6] Inoue A, Zhang T, Itoi T. Mater Trans JIM, 1997; 38: 359 [7] Inoue A, Nishiyama N, T. Matsuda. Mater Trans JIM, 1996; 37: 181 [8] Zhang T, Inoue A. Mater Trans JIM, 1998; 39: 1001 [9] Zhang T, Inoue A. Mater Trans JIM, 1999; 40: 301 [10] Akarsuka R, Zhang T, Koshiba M. Mater Trans JIM, 1999; 40: 258 [11] Saida J, Matsushita M, Zhang T, Inoue A, Chen M W, Sakurai T. Appl Phys Lett, 1999; 75: 3497 [12] Li C, Inoue A. J Alloy Compd, 2001; 325: 230 [13] Molokanov V V, Petrzhik M I, Mikhailova T N, Sviridova T A, Djakonova N P, J Non-Cryst Solids, 1999; 250: 560 [14] Yokoyama Y, Yamano K, Fukaura, Sunada H, Inoue A. Mater Trans JIM, 1999; 40:1015 [15] Fan C, Li C, Inoue A. Appl Phys Lett, 2001; 79: 1024 [16] Fan C, Inoue A. Scr Mater, 2001; 45: 115 [17] Lu Z P, Liu C T. Acta Mater, 2002; 50: 3501 [18] Lu Z P, Liu C T. Phys Rev Lett, 2003; 91: 115505 [19] Lu Z P, Liu C T, Intermetallics, 2004; 12: 1035 [20] Nishiyama N, Inoue A. Mater Trans JIM, 1996; 31: 1531 [21] de Boer F R, Boom R, Mattens W C M, Miedema A R, Niessen A K. Cohesion in Metals. Amsterdam: North Holland, 1988: 314, 375, 390 [22] Zhang T, Inoue A. Mater Trans, 2002; 43: 1367 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|