| 温度对N离子注入金属深度分布的影响 |
| 白彬 张鹏程 邹觉生 陈元儒 |
| 中国工程物理研究院;绵阳621900 |
|
引用本文:
白彬; 张鹏程; 邹觉生; 陈元儒 . 温度对N离子注入金属深度分布的影响[J]. 金属学报, 2001, 37(1): 82-86 .
[1] Straede C A, Mikkelseen N J. Surf Coat Technol,1998;103/104: 189 [2] Wei R, Wilbur P J, Ozturk O. Nucl Instrum Methods,1991; B59/60:731 [3] Wilbur P J W, Buchholtz B. Surf Coat Technol,1996;79:1 [4] Wei R, Dhogrin B, Wilbur P J. J Tribol, 1994;. 116: 870 [5] Wei R, Wilbur P J, Sampath W S. J Tribol, 1991; 113:166 [6] Rehn L H, Aerback R S, Okamoto P R. Mater Sci Eng,1985; 69:1 [7] Terwagne G, Piette M, Bodart F. Mater Sci Eng, 1989;A115: 25 [8] Lueas S, Chevallier J, Chechen N G. Surf Coat Technol,1994; 66: 334 [9] Ohtani S, Inoue M, Takagi T. Nucl Instrum Methods,1997; B121: 319 [10] Vglov V V P, Rusalsky O P,. Vkhodasevich V. Surf CoatTechnol, 1998; 103/104: 323 [11] Zhang T H, Wu Y G. Optimizing Pressing of Ion Implantation. Beijing: Metallurgical industry Press, 1993: 155(张通和,吴瑜光.离子注入表面优化技术.北京:冶金工业出版社,1993:155) [12] Zhang T H, Wu Y G, Ji C Z. Nucl Instrum Methods, 1992;B67: 458 [13] Wang A M, Ji C Z, Zhang T H. J Beijing Norm Univ(NatSci), 1992; 28: 482(王安明,姬成周,张通和.北京师范大学学报(自然科学版),1992;28:482) [14] Ji C Z, Wang A M, Zhang T H. J Beijing Norm Univ (NatSci), 1992; 28: 323(姬成周,王安明,张通和.北京师范大学学报(自然科学版),1992;28:323) [15] Ozturk O, Williamson D L. J Appl Phys, 1995; 77: 3839 [16] Zhang T H, Wu Y G. Material Modification Science andIts Application by Ion Beam. Beijing: Metallurgical Industry Press, 1999: 42(张通和,吴瑜光.离子束材料表面改性科学及应用.北京:冶金工业出版社,1999:42) [17] Kpcewie M, Jagielski J, Gawlik G. Nucl Instram Methods,1995; B95: 208 [18] Bai B. Master Thesis, Southwest Jiaotong University,Chengdu, 1999: 47(白 彬.西南交通大学硕士学位论文,成都,1999:47) [19] Shi D K. Dislocation and Strength of Materials. Xi'an:Xi'an Jiaotong University Press, 1988: 62(石德珂.位错与材料强度. 西安:西安交通大学出版社,1988:62)M |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|