| 高压下Mg65Cu25Y10合金凝固过程中Cu2(Y, Mg)纳米相的形成及其热稳定性 |
| 张 甲;张海峰;董 盼;全明秀;胡壮麒 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
| Formation and Thermal Stability of Nanoscale Cu2(Y, Mg) During the Solidification of Mg65Cu25Y10 Alloy Under High Pressure Condition |
| ZHANG Jia; ZHANG Haifeng; DONG Pan; QUAN Mingxiu; HU Zhuangqi |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
张甲; 张海峰; 董盼; 全明秀; 胡壮麒 . 高压下Mg65Cu25Y10合金凝固过程中Cu2(Y, Mg)纳米相的形成及其热稳定性[J]. 金属学报, 2004, 40(2): 211-214 .
,
,
,
,
.
Formation and Thermal Stability of Nanoscale Cu2(Y, Mg) During the Solidification of Mg65Cu25Y10 Alloy Under High Pressure Condition[J]. Acta Metall Sin, 2004, 40(2): 211-214 .
[1] Savage S J, Froes F H. In: Kear B H, Giessen B C eds., Rapidly Solidified Metastable Materials, New York: North-Holland, 1984: 329 [2] Uhlmamm D R, Hays J F, Turnbull D. Phys Chem Glasses, 1966; 7: 159 [3] He D, He M, Kiminami C S, Zhang F X, Xu Y F, Wang W K, Kuo K H. J Mater Res. 2000; 16: 910 [4] Shen Z Y, Shen D J, Zhang Y, Yin X J, Wu H Q. Acta Metall Mater, 1992; 40: 2185 [5] Sun L L, Wu Q, Wang L M, Yao Y S, Dai D Y, Zhang J, Wang W K. Mater Trans, JIM, 2001; 42: 579 [6] Zhang J, Qiu K Q, Wang A M, Zhang H F, Quan M X, Hu Z Q. J Mater Res, 2002; 17: 2935 [7] Parker L J, Atou T, Badding J V. Science, 1996; 273: 95 [8] Inoue A, Kato A, Zhang T, Kim S G, Masumoto, T. Mater Trans, JIM, 1991; 32: 609 [9] Wang W K, Iwasaki H, Suryanarayana C, Masumoto T. J Mater Sci, 1983; 18: 3765 [10] Turnbull D. Prog Solid State Phys, 1956; 3: 225 |
|