| 结晶器材料对低频电磁铸造超高强铝合金铸态组织的影响 |
| 董 杰;刘晓涛;赵志浩;包卫平;崔建忠 |
| 东北大学材料电磁过程研究教育部重点实验室; 沈阳 110004 |
|
| Effect of Mould Materials on the As-Cast Microstructures of a Super-High Strength Al Alloy Cast by Low Frequency Electromagnetic Casting |
| DONG Jie; LIU Xiaotao; ZHAO Zhihao; BAO Weiping; CUI Jianzhong |
| The Key Laboratory of Electromagnetic Processing of Materials; Ministry of Education; Northeastern University; Shenyang 110004 |
引用本文:
董杰; 刘晓涛; 赵志浩; 包卫平; 崔建忠 . 结晶器材料对低频电磁铸造超高强铝合金铸态组织的影响[J]. 金属学报, 2004, 40(2): 215-219 .
,
,
,
,
.
Effect of Mould Materials on the As-Cast Microstructures of a Super-High Strength Al Alloy Cast by Low Frequency Electromagnetic Casting[J]. Acta Metall Sin, 2004, 40(2): 215-219 .
[1] Li C G, Wu S J, Dai S L, Yang S J. J Nonfer Met, 2002; 12(Suppl): 14(李成功,巫世杰,戴圣龙,杨守杰.中国有色金属学报,2002;12(增刊):14) [2] Chen C Q. J Nonfer Met, 2002; 12(Suppl): 22(陈昌麒.中国有色金属学报,2002;12(增刊):22) [3] Osman T M, Singh P M, Lewandowski J J. Scr Metall Mater, 1994; 31: 607 [4] Pandey A B, Majumdar B S, Miracle D B. Metall Mater Trans, 1998; 29A: 1237 [5] Adachi H, Osamura K, Ochiai S, Kusui J, Yokoe K. Scr Mater, 2001; 44: 1489 [6] Wu Y L, Froes F H, Alvarez A, Li C G, Liu J. Mater Design, 1997; 18: 211 [7] Kusui J, Fujii K, Yokoe K, Yokote T, Osamura K, Kubota O, Okuda H. Mater Sci Forum, 1996: 217 [8] Wei Q, Xiong B Q, Zhang Y A, Zhu B H, Shi L K. Trans Nonfer Met Soc Chin (Engl Ed), 2001; 11: 258 [9] Zhang B J, Cui J Z, Lu G M, Zhang Q, Ban C Y. Acta Metall Sin, 2002; 38: 215(张北江,崔建忠,路贵民,张勤,班春燕.金属学报,2002;38:215) [10] Zhang B J, Cui J Z, Lu G M, Xu G M. Chin J Nonfer Met, 2002; 12(Suppl): 112(张北江,崔建忠,路贵民,许光明.中国有色金属学报,2002;12(增刊):112) [11] Rodger D, Eastham J F. IEEE Trans Magn, 1983; 19: 2443 [12] Oszkr B, Preis K. IEEE Trans Magn, 1989; 25: 3145c |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|