| 0.1 mol/L NaCl溶液中不同剥蚀程度LY12CZ合金的EIS特征 |
| 张 正 宋诗哲 墨淑芬 |
| 天津大学材料科学与工程学院; 天津 300072 |
|
| EIS CHARACTERISTIC OF LY12CZ ALLOY WITH DIFFERENT EXFOLIATION CORROSION GRADES IN 0.1 mol/L NaCl SOLUTION |
| ZHANG Zheng; SONG Shizhe; MO Shufen |
| School of Material; Tianjin University; Tianjin 300072 |
引用本文:
张正; 宋诗哲; 墨淑芬 . 0.1 mol/L NaCl溶液中不同剥蚀程度LY12CZ合金的EIS特征[J]. 金属学报, 2004, 40(7): 754-758 .
,
,
.
EIS CHARACTERISTIC OF LY12CZ ALLOY WITH DIFFERENT EXFOLIATION CORROSION GRADES IN 0.1 mol/L NaCl SOLUTION[J]. Acta Metall Sin, 2004, 40(7): 754-758 .
[1] Lee S, Lifka B W. ASTM Special Technical Publication.Philadelphia,PA, USA: ASTM, 1991: 1 [2] Keddam M, Kuntz C, Takenouti H, Schuster D, Zuili D.Electrochimica Acta, 1997; 42(1) : 87 [3] Conde A, de Damborenea J. Corros Sci, 2000; 42: 1363 [4] McNaughtan D, Worsfold M, Robinson M J. Corros Sci,2003; 45: 2377 |
|