| 镀锡钢板耐蚀性与恒电流阳极溶解电位--时间曲线的关系 |
| 王 焜 钱 钢 陆文聪 陈念贻 |
| 上海大学化学系计算机化学研究室; 上海 200436 |
|
| CORRELATION BETWEEN POTENTIAL--TIME CURVES OF CONSTANT--CURRENT ANODIC DISSOLUTION AND CORROSION RESISTANCE OF TINPLATE |
| WANG Kun; QIAN Gang; LU Wencong; CHEN Nianyi |
| Laboratory of Chemical Data Mining; Shanghai University; Shanghai 200436 |
引用本文:
王焜; 钱钢; 陆文聪; 陈念贻 . 镀锡钢板耐蚀性与恒电流阳极溶解电位--时间曲线的关系[J]. 金属学报, 2004, 40(7): 759-762 .
,
,
,
.
CORRELATION BETWEEN POTENTIAL--TIME CURVES OF CONSTANT--CURRENT ANODIC DISSOLUTION AND CORROSION RESISTANCE OF TINPLATE[J]. Acta Metall Sin, 2004, 40(7): 759-762 .
[1] Toyo Steel Plate Co., Translated by Zhou Q L. Thin Tin-plate. Beijing: Metallurgy Industry Press, 1977: 133(日本东洋钢板公司,周其良译.镀锡薄钢板.北京;冶金工业出版社,1977:133) [2] Bard A J, Faulkner L R. Electrochemical Methods. New York: John-Wiley & Sons, 2001: 4 [3] Chen N Y, Qi P, Chen R L, Lu W C. Pattern Recognition Applied to Chemistry and Chemical Industry, Beijing: Science Press, 2002: 2(陈念贻,钦佩,陈瑞亮,陆文聪.模式识别在化学化工中的应用,北京:科学出版社,2002:2) [4] Lu W C, Chen N Y, Ye C Z, Li G Z. Computers and Applied Chemisry, 2002; 19(6) : 696(陆文聪,陈念贻,叶晨洲,李国正.计算机与应用化学,2002;19(6) :697) [5] Cristinini N, Taylor J. An Introduction on Support Vector Machine and Other Kernel-based Learning Methods. Cambridge: Cambridge University Press, 2000: 42D |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|