| 连续冷却过程中低碳钢奥氏体→铁素体相变的元胞自动机模拟 |
| 张 林;张彩碚;王元明 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室 |
|
| Cellular Automaton Modelling Of The Transformation From Austenite to Ferrite In Low Carbon Steels During Continuous Cooling |
| ZHANG Lin; ZHANG Caibei; WANG Yuanming;WANG Shaoqing |
| Shenyang National Laboratory for Materials Science;Institute of Metal Research; The Chinese Academic of Sciences |
引用本文:
张林; 张彩碚; 王元明 . 连续冷却过程中低碳钢奥氏体→铁素体相变的元胞自动机模拟[J]. 金属学报, 2004, 40(1): 8-13 .
,
,
,
.
Cellular Automaton Modelling Of The Transformation From Austenite to Ferrite In Low Carbon Steels During Continuous Cooling[J]. Acta Metall Sin, 2004, 40(1): 8-13 .
[1] Wolfram S. Rev Modell Phys, 1983; 55:601 [2] Lepinoux J, Kubin L P. Scr Metall, 1987; 21:833 [3] Rappaz M, Gandin C A. Acta Metall.Mater, 1993; 41; 345 [4] Goetz R L, Seetharman V. Metall Mater Trans, 1998; 22A: 2307 [5] Zhang L, Wang Y M, Zhang C B. Acta Metall Sin, 2001; 37:882(张林,王元明,张彩碚.金属学报,2001;37:882) [6] Zhang L, Zhang C B, Liu X H, Wang G D, Wang Y M. J Mater Sci Technol, 2002; 18:163 [7] Umemoto M, Ohtsuka H, Tamura I. J Mater Sci Technol, 1987; 3:249 [8] Hawbolt E B, Chau B, Brimacombe J K. Metall Trans,1983; 14A: 1803 [9] Enomoto M, Aaronson H I. Metall Trans, 1986; 17A: 1381 [10] Militzer M, Pandi R, Hawbolt E B. Metall Mater Trans, 1996; 27A: 1547 [11] Jacot A, Rappaz M. Acta Mater, 1997; 45:575 [12] Zhang L, Zhang C B, Wang Y M, Liu X H, Wang G D. Mater Res, 2002; 17:2251 [13] Zhang L, Wang Y M, Zhang C B, Wang S Q, Ye H Q. Modelling Simu Mater Sci Technol, 2003; 11:791 [14] Zhang L, Zhang C B, Wang Y M, Wang S Q, Ye H Q. Acta Mater, 2003; 51:55193 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|