| r射线吸收法测量液态金属In的密度 |
| 王连文 冼爱平 邵涵如 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
| Density Measurement of Liquid Indium Using r--Ray Attenuation Method |
| WANG Lianwen; XIAN Aiping;SHAO Hanru |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
王连文; 冼爱平; 邵涵如 . r射线吸收法测量液态金属In的密度[J]. 金属学报, 2004, 40(6): 643-.
,
,
.
Density Measurement of Liquid Indium Using r--Ray Attenuation Method[J]. Acta Metall Sin, 2004, 40(6): 643-.
[1] Iida T, Guthrie R I L. The Physical Properties of Liquid Metals. New York: Clarendon Press, 1988: 47 [2] Bian S M, Ma L M, Wang J T. Acta Metall Sin, 1986;22(2) : B90(边茂恕,马禄铭,王景唐.金属学报,1986;22(2) :B90) [3] Zhou G Z, Cai W J, Hu J H. J Univ Sci Technol Beijing,1991; 13(4. I): 380(周国治,蔡文娟,胡建虹、北京科技大学学报,1991;13(4. I):380) [4] Chen X M, Wang Q, Lu K Q. J Phys: Cond Matt, 1999;11: 10335 [5] Han X J, Wang N, Wei B. Philos Mag Lett, 2002; 82(8) :451 [6] Wang W M, Bian X F, Wang H R, Wang Z, Zhang L, Liu Z G. J Mater Res, 2001; 16: 3592 [7] Doge G. Z Naturforschg, 1966; 21a: 266 [8] Dillon I G, Levert F E, Loretan P A, Menon G U, Siddiqi F M, Tarng H J. Nucl Technol, 1973; 12: 307 [9] Basin A S, Kolotov Y L, Stankus S V. High Temp High Press, 1979; 11: 465 [10] Peggs I A. Thermal Expansion 6. New York: Plenum Press, 1978: 83 [11] Drotning W D. High Temp High Press, 1981; 13: 441 [12] Nasch P M, Steinemann S G. Phys Chem Liq, 1995; 29:43 [13] Smith P M, Elmer J W, Gallegos G F. Scr Mater, 1999;40(8) : 937 [14] Fudan University Tsinghua University Peking Universityed. Experimental Technique in Nuclear Physics (2nd ed).Beijing: Nuclear Energy Press, 1985: 81(复旦大学,清华大学,北京大学合编.原子核物理实验方法(第二版).北京:原子能出版社,1985:81) [15] Lide D R. CRC Handbook of Chemistry and Physics (78th ed). Chemical Rubber Company Press, 1998 [16] Williams D D, Miller R R. J Am Chem Soc, 1950; 72:3821 [17] Schneider A, Heymer G. Z Anorg Allg Chem, 1956; 286:97 [18] McGonigal P J, Cahill J A, Kirshenbaum A D. J Inorg Nucl Chem, 1962; 24: 1012 [19] Berthou P E, Tougas R. Metall Trans, 1970; 1: 2978 [20] Crawley A F. Trans AIME, 1968; 242: 2237 [21] McClelland M A, Sze J S. Surf Sci, 1995; 330(3) : 313 [22] Wang L W, Wang Q, Xian A P, Lu K Q. J Phys Cond Matt, 2003; 15: 777 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|