金属学报  2026, Vol. 62 Issue (6): 1082-1090    DOI: 10.11900/0412.1961.2025.00339
  研究论文 本期目录 | 过刊浏览 |
TC4钛合金循环变形微观组织演化与滑移机制
吴帆, 刘华辉, 边文珊, 蔡竣宇, 金士杰, 罗忠兵()
大连理工大学 材料科学与工程学院 大连 116024
Microstructural Evolution and Slip Mechanisms in TC4 Titanium Alloy During Cyclic Deformation
WU Fan, LIU Huahui, BIAN Wenshan, CAI Junyu, JIN Shijie, LUO Zhongbing()
School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
引用本文:

吴帆, 刘华辉, 边文珊, 蔡竣宇, 金士杰, 罗忠兵. TC4钛合金循环变形微观组织演化与滑移机制[J]. 金属学报, 2026, 62(6): 1082-1090.
Fan WU, Huahui LIU, Wenshan BIAN, Junyu CAI, Shijie JIN, Zhongbing LUO. Microstructural Evolution and Slip Mechanisms in TC4 Titanium Alloy During Cyclic Deformation[J]. Acta Metall Sin, 2026, 62(6): 1082-1090.

全文: PDF(2871 KB)   HTML
摘要: 

为揭示TC4钛合金在循环变形过程中的微观组织演变、位错组态及滑移行为,以探究其变形损伤机制,本工作通过EBSD和TEM等显微分析手段对TC4钛合金展开研究。结果表明,在加载初期,材料快速硬化,微织构区域与周围晶粒的变形不协调导致应变高度集中。随后材料进入准稳态阶段,整体发生塑性累积;受材料织构和加载方向影响,锥面101¯1<c + a>滑移系以最高Schmid因子激活,主导变形并推动晶粒取向逐步向<112¯0>方向演化;循环变形过程中α/β相界面处位错增殖并在界面处平行堆积,界面作为位错源和障碍区提高了材料寿命。α/β界面处位错演化与微织构区域应变高度集中的协同作用是TC4钛合金循环变形损伤的主要机制。

关键词 : 钛合金,  循环变形,  微织构,  滑移机制,  位错    
Abstract:

The cyclic damage behavior of TC4 alloy, which is widely utilized in aerospace and other fields, is critical to the structural integrity of its components. The aim of this study is to elucidate the underlying microstructural damage mechanisms, from the aspect of microstructural evolution, slip activity, and dislocation configurations, during cyclic loading through advanced characterization techniques including EBSD and TEM. The results indicate an initial rapid hardening stage, during which strain is highly localized in microtextured regions due to deformation incompatibility with the surrounding grains. The material subsequently reaches a quasi-steady state, which is marked by accumulated plasticity. Influenced by crystallographic texture and loading direction, the pyramidal 101¯1<c + a> slip system exhibits the highest Schmid factor and is preferentially activated, dominating the deformation process and promoting a gradual grain reorientation toward the <112¯0> direction. TEM analysis indicates that dislocations multiply and align parallel to α/β phase interfaces during cyclic deformation. These interfaces function as both dislocation sources and barriers, thereby enhancing the material's fatigue life. The synergistic coupling between dislocation activity at α/β interfaces and pronounced strain localization within microtextured regions is identified as the dominant mechanism governing cyclic deformation damage in TC4 alloy.

Key words: titanium alloy    cyclic deformation    microtexture    slip mechanism    dislocation
收稿日期: 2025-10-24     
ZTFLH:  TG142.71  
基金资助:国家自然科学基金项目(52375527);国家自然科学基金项目(52275520)
通讯作者: 罗忠兵,zhbluo@dlut.edu.cn,主要从事材料损伤与无损评价研究
Corresponding author: LUO Zhongbing, professor, Tel: (0411)84706049, E-mail: zhbluo@dlut.edu.cn
作者简介: 吴 帆,男,1999年生,硕士生
图1  TC4合金循环变形试样几何示意图
图2  TC4合金初始显微组织及XRD谱
图3  TC4合金循环加载响应:应力-应变滞后环及塑性应变幅与循环加载周次曲线
图4  不同循环周次TC4合金LSCM表面形貌、EBSD晶粒取向分布反极图及局部取向差(KAM)结果
图5  TC4合金KAM分布的均值(mKAM)和方差(vKAM)随循环周次的变化情况
图6  TC4合金不同循环周次不同区域的带衬度(BC)变化
图7  TC4合金循环变形过程中X0方向反极图及晶粒取向示意图
图8  不同循环周次下循环变形TC4合金滑移系的Schmid因子演变
图9  TC4合金中α相滑移机制示意图
图10  初始态和加载5000 cyc后TC4合金样品的TEM像
[1] Banerjee D, Williams J C. Perspectives on titanium science and technology[J]. Acta Mater., 2013, 61: 844
doi: 10.1016/j.actamat.2012.10.043
[2] Chen B, Bao R, Zhang J Y, et al. Combined design and analysis of durability and damage tolerance for flight structure[J]. J. Beijing Univ. Aeronaut. Astronaut., 2004, 30: 139
[2] 陈 勃, 鲍 蕊, 张建宇 等. 飞机结构耐久性/损伤容限综合设计与分析[J]. 北京航空航天大学学报, 2004, 30: 139
[3] Guo P, Zhao Y Q, Zeng W D, et al. The effect of microstructure on the mechanical properties of TC4-DT titanium alloys[J]. Mater. Sci. Eng., 2013, A563: 106
[4] Guo P. Research on damage behaviors of TC4-DT titanium alloys[D]. Xi'an: Northwestern Polytechnical University, 2015
[4] 郭 萍. TC4-DT钛合金损伤行为研究[D]. 西安: 西北工业大学, 2015
[5] Huang S S, Ma Y J, Zhang S L, et al. Influence of alloying elements partitioning behaviors on the microstructure and mechanical properties in α + β titanium alloy[J]. Acta Metall. Sin., 2019, 55: 741
[5] 黄森森, 马英杰, 张仕林 等. α + β两相钛合金元素再分配行为及其对显微组织和力学性能的影响[J]. 金属学报, 2019, 55: 741
doi: 10.11900/0412.1961.2018.00460
[6] Wu W Y, Song C H, Zhang Z S, et al. Microstructure and properties of as-cast Co-28Cr alloy with aging treatment[J]. Chin. J. Rare Met., 2025, 49: 982
[6] 吴文源, 宋成浩, 张振山 等. 时效处理对铸态Co-28Cr合金组织和性能的影响[J]. 稀有金属, 2025, 49: 982
[7] Zhu Z S, Wang X N, Tong L, et al. Research and application of damage tolerance titanium alloys for aeronautical use[J]. Mater. China, 2010, 29(5): 14
[7] 朱知寿, 王新南, 童 路 等. 航空用损伤容限型钛合金研究与应用[J]. 中国材料进展, 2010, 29(5): 14
[8] Cheng J. Study on cold deformation, phase transformation and corrosion behavior of a new metastable β-type Ti-B12 biomedical titanium alloy[D]. Xi'an: Northwestern Polytechnical University, 2021
[8] 程 军. 新型亚稳定β型Ti-B12医用钛合金冷变形、相变与腐蚀行为研究[D]. 西安: 西北工业大学, 2021
[9] Fu Y, Peng H B, Wang H, et al. Engineering omega phase enables a wide temperature range Elinvar effect in metastable β-Ti alloys[J]. J. Mater. Sci. Technol., 2025, 225: 159
doi: 10.1016/j.jmst.2024.11.028
[10] Nalla R K, Ritchie R O, Boyce B L, et al. Influence of microstructure on high-cycle fatigue of Ti-6Al-4V: Bimodal vs. lamellar structures[J]. Metall. Mater. Trans., 2002, 33A: 899
[11] Germain L, Gey N, Humbert M, et al. Texture heterogeneities induced by subtransus processing of near α titanium alloys[J]. Acta Mater., 2008, 56: 4298
doi: 10.1016/j.actamat.2008.04.065
[12] Szczepanski C J, Jha S K, Larsen J M, et al. Microstructural influences on very-high-cycle fatigue-crack initiation in Ti-6246[J]. Metall. Mater. Trans., 2008, 39A: 2841
[13] Germain L, Gey N, Humbert M, et al. β→αs variant selection in sharp hcp textured regions of a bimodal IMI834 billet[J]. Mater. Sci. Forum, 2005, 495-497: 663
doi: 10.4028/www.scientific.net/MSF.495-497
[14] Rugg D, Dixon M, Dunne F P E. Effective structural unit size in titanium alloys[J]. J. Strain Anal. Eng. Des., 2007, 42: 269
doi: 10.1243/03093247JSA273
[15] Bache M R, Evans W J. Dwell sensitive fatigue response of titanium alloys for power plant applications[J]. J. Eng. Gas Turbines Power, 2003, 125: 241
doi: 10.1115/1.1494094
[16] Whittaker R, Fox K, Walker A. Texture variations in titanium alloys for aeroengine applications[J]. Mater. Sci. Technol., 2010, 26: 676
doi: 10.1179/026708310X12635619988186
[17] Lunt D, da Fonseca J Q, Rugg D, et al. Microscopic strain localisation in Ti-6Al-4V during uniaxial tensile loading[J]. Mater. Sci. Eng., 2017, A680: 444
[18] Lunt D, Thomas R, Atkinson M D, et al. Understanding the role of local texture variation on slip activity in a two-phase titanium alloy[J]. Acta Mater., 2021, 216: 117111
doi: 10.1016/j.actamat.2021.117111
[19] Bridier F, Villechaise P, Mendez J. Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales[J]. Acta Mater., 2008, 56: 3951
doi: 10.1016/j.actamat.2008.04.036
[20] Evans W J, Jones J P, Whittaker M T. Texture effects under tension and torsion loading conditions in titanium alloys[J]. Int. J. Fatigue, 2005, 27: 1244
doi: 10.1016/j.ijfatigue.2005.06.045
[21] Le Biavant K, Pommier S, Prioul C. Local texture and fatigue crack initiation in a Ti-6Al-4V titanium alloy[J]. Fatigue Fract. Eng. Mater. Struct., 2002, 25: 527
doi: 10.1046/j.1460-2695.2002.00480.x
[22] Imani N, Shahmir H, Huang Y, et al. The significance of crystal structure on grain refinement during severe plastic deformation[J]. J. Mater. Sci., 2025, 60: 11616
doi: 10.1007/s10853-025-11101-3
[23] Zaefferer S. A study of active deformation systems in titanium alloys: Dependence on alloy composition and correlation with deformation texture[J]. Mater. Sci. Eng., 2003, A344: 20
[24] Bridier F, Villechaise P, Mendez J. Analysis of the different slip systems activated by tension in a α/β titanium alloy in relation with local crystallographic orientation[J]. Acta Mater., 2005, 53: 555
doi: 10.1016/j.actamat.2004.09.040
[25] Jones I P, Hutchinson W B. Stress-state dependence of slip in titanium-6Al-4V and other H.C.P. metals[J]. Acta Metall., 1981, 29: 951
doi: 10.1016/0001-6160(81)90049-3
[26] Wu Z H, Kou H C, Li J S, et al. Crack initiation mechanism of a silicide-containing high-strength Ti-5Al-7.5V alloy under low-cycle fatigue loading[J]. Mater. Sci. Eng., 2023, A865: 144654
[27] Wang C L, Yu D P, Niu Z Q, et al. The role of pyramidal 〈c + a〉 dislocations in the grain refinement mechanism in Ti-6Al-4V alloy processed by severe plastic deformation[J]. Acta Mater., 2020, 200: 101
doi: 10.1016/j.actamat.2020.08.076
[28] Su R, Liu Q L, Li H Z, et al. Effect of three-stage heat treatment on the composite waveform and variable amplitude fatigue properties of TC4 titanium alloy pulsed laser-arc hybrid welded joints[J]. Int. J. Fatigue, 2025, 191: 108673
doi: 10.1016/j.ijfatigue.2024.108673
[29] Zhu X L. Fatigue damage evaluation of coarse-grained austenitic stainless steel based on EBSD and ultrasound methods[D]. Dalian: Dalian University of Technology, 2017
[29] 朱效磊. 基于EBSD和超声的粗晶奥氏体不锈钢疲劳损伤评价[D]. 大连: 大连理工大学, 2017
[30] Che F, Zhang P, Meng Y Y, et al. Mesoscale damage behavior and meso-macroscale correlation of low-cycle fatigue in Z2CND18.12N austenitic stainless steel[J]. Mater. Sci. Eng., 2022, A854: 143894
[31] Guo Y Y, Zhang B W, Zhou L L, et al. Creep strain and stress state-dependent creep asymmetry during early-stage room-temperature creep in a titanium alloy[J]. J. Mater. Sci. Technol., 2026, 243: 1
doi: 10.1016/j.jmst.2025.03.092
[32] Littlewood P D, Wilkinson A J. Local deformation patterns in Ti-6Al-4V under tensile, fatigue and dwell fatigue loading[J]. Int. J. Fatigue, 2012, 43: 111
doi: 10.1016/j.ijfatigue.2012.03.001
[1] 秦志伟, 王彬, 赵强, 李家辰, 孙毓涛, 洪小龙, 李鹏, 董红刚. 热处理对GH4065A/IN718异质高温合金惯性摩擦焊接头界面微观组织的影响[J]. 金属学报, 2026, 62(6): 1032-1042.
[2] 王建峰, 许珍木, 刘战, 高转妮, 占小红. 超声振动对TC4钛合金窄间隙激光焊接组织及强化机理的影响[J]. 金属学报, 2026, 62(3): 406-420.
[3] 张哲峰, 侯嘉鹏, 刘睿, 李孝滔, 张振军, 张鹏. 金属材料强度-塑性及强度-电导率定量关系[J]. 金属学报, 2026, 62(2): 253-262.
[4] 赵子博, 谭海兵, 张博华, 刘玉敬, 刘建荣, 郭会明, 曾卫东, 田伟, 王清江. 综述:近 α 型和 α + β 两相钛合金的微织构[J]. 金属学报, 2026, 62(2): 275-288.
[5] 谭若涵, 宋永锋, 陈超, 李丹, 成庶, 李雄兵. 增材制造钛合金等效弹性张量的细观力学建模与实验研究[J]. 金属学报, 2025, 61(9): 1438-1448.
[6] 张洺川, 徐勤思, 刘意, 蔡雨升, 牟义强, 任德春, 吉海宾, 雷家峰. 热压温度对TC4合金扩散连接区组织与性能的影响[J]. 金属学报, 2025, 61(8): 1183-1192.
[7] 范荣磊, 陈明和, 吴迪鹏, 武永. 基于晶体塑性模型预测TA32钛合金损伤及高温成形极限[J]. 金属学报, 2025, 61(8): 1293-1304.
[8] 徐小严, 方超, 邱建科, 张蒙蒙, 史栋刚, 马英杰, 雷家峰, 杨锐. 峰值应力对Ti6242压气机盘锻件室温保载效应的影响[J]. 金属学报, 2025, 61(8): 1141-1152.
[9] 李夫顺, 刘志鹏, 丁灿灿, 胡斌, 罗海文. 一种新型高强奥氏体低密度钢的强塑性机理[J]. 金属学报, 2025, 61(6): 909-916.
[10] 赵焯雅, 孟令健, 林鹏, 曹晓卿. TC4钛合金跨相区连续热压缩 α 相组织演变规律及织构形成机理[J]. 金属学报, 2025, 61(5): 717-730.
[11] 曾小勤, 于铭迪, 王静雅. 镁合金的多系滑移与塑性调控[J]. 金属学报, 2025, 61(3): 361-371.
[12] 周生玉, 胡明昊, 李冲, 丁海民, 郭乾应, 刘永长. 一种 γ'/γ'' 相强化镍基高温合金的蠕变行为[J]. 金属学报, 2025, 61(2): 226-234.
[13] 戴进财, 闵小华, 辛社伟, 刘凤金. 间隙元素O对 β 型Ti-15Mo合金超低温力学性能的影响[J]. 金属学报, 2025, 61(2): 243-252.
[14] 齐敏, 王倩, 马英杰, 曹贺萌, 黄森森, 雷家峰, 杨锐. Ti6246钛合金 β → α 相变中晶界 α 相生长行为及其对微织构的影响[J]. 金属学报, 2025, 61(2): 265-277.
[15] 李丹, 宫得伦, 郝玉琳. O含量对Ti2448合金时效析出行为及力学性能的影响[J]. 金属学报, 2025, 61(12): 1790-1802.