| Ca对Al2O3(P)/Al-Si复合材料凝固组织的影响 |
| 吴树森 黄乃瑜 安萍 吴广忠 |
| 华中理工大学材料科学与工程学院; 武汉 430074 |
|
引用本文:
吴树森; 黄乃瑜; 安萍; 吴广忠 . Ca对Al2O3(P)/Al-Si复合材料凝固组织的影响[J]. 金属学报, 1999, 35(6): 663-667 .
[1]Rose D L, Cox B M, Skibu M D. AFS Trans, 1993; 101: 619 [2]Mortenson A,Jin I.Int Mat Rev, 1992; 37:101 [3]Tsumura Y,Sakakibara A,Toyda K.J Jpn Inst Light Met,1972; 22:369 [4]Tsumura Y, Sakakibara A, Toyoda K.J Jpn Inst Light Met,1980; 30:239 [5]Kobayashi T, Niinomi M, Yamaka M. J Jpn Inst Light Met, 1993; 43:581 [6]Lu S Z, Hellawell A.J Crys Growth; 1985; 73: 316 [7]Hogan L M, Song H. Metall Trans, 1987; A18: 707 [8]Wu S,Nakae H.J Jpn Foundry Eng Soc,1997;69:3 [9]Song K, Fujii H, Nakae H, Yamaura H.J Jpn Inst Light Met,993; 43:484 [10]Rohatgi P, Asthana R, Das S. Int Met Rev, 1986; 31: 115 [11]Wu S,Nakae H.J Jpn Foundry Eng Soc,1997;69:775 [12]Wu S, Nakae H. Acta Metall Sin, 1998; 34: 939 (吴树森,中江秀雄.金属学报,1998:34:939) [13]Petzow G, Effenberg G. Ternary Alloys. Vo1.3, Weinheim,Germany: VCH Verlagsgesellschaft, 1990: 270, 628h |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|