| 钢包静置过程夹杂物去除的工业试验与数值模拟 |
段豪剑1, 谢忠研1, 李占魁1, 徐学军1, 黄财德2, 温瀚2, 张立峰3( ) |
1 北京科技大学 冶金与生态工程学院 北京 100083 2 首钢京唐钢铁联合有限责任公司 炼钢部 唐山 063200 3 北方工业大学 机械与材料工程学院 北京 100144 |
|
| Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period |
DUAN Haojian1, XIE Zhongyan1, LI Zhankui1, XU Xuejun1, HUANG Caide2, WEN Han2, ZHANG Lifeng3( ) |
1 School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China 2 Steelmaking Department, Shougang Jingtang United Iron and Steel Co. Ltd., Tangshan 063200, China 3 School of Mechanical and Materials Engineering, North China University of Technology, Beijing 100144, China |
引用本文:
段豪剑, 谢忠研, 李占魁, 徐学军, 黄财德, 温瀚, 张立峰. 钢包静置过程夹杂物去除的工业试验与数值模拟[J]. 金属学报, 2026, 62(7): 1288-1296.
Haojian DUAN,
Zhongyan XIE,
Zhankui LI,
Xuejun XU,
Caide HUANG,
Han WEN,
Lifeng ZHANG.
Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period[J]. Acta Metall Sin, 2026, 62(7): 1288-1296.
| [1] |
Zhang L F, Thomas B G. State of the art in evaluation and control of steel cleanliness [J]. ISIJ Int., 2003, 43: 271
doi: 10.2355/isijinternational.43.271
|
| [2] |
Zhang L F. Nucleation, growth, transport, and entrapment of inclusions during steel casting [J]. JOM, 2013, 65: 1138
doi: 10.1007/s11837-013-0688-y
|
| [3] |
Zhang L F, Ren Q, Duan H J, et al. Modelling of non-metallic inclusions in steel [J]. Min. Proc. Ext. Metall., 2020, 129: 184
|
| [4] |
Zhang L F. Non-Metallic Inclusions in Steel: Fundmentals [M]. Beijing: Metallurgical Industry Press, 2019: 1
|
| [4] |
张立峰. 钢中非金属夹杂物 [M]. 北京: 冶金工业出版社, 2019: 1
|
| [5] |
Zhang L F. Non-Metallic Inclusions in Steel: Industrial Practice [M]. Beijing: Metallurgical Industry Press, 2019: 1
|
| [5] |
张立峰. 钢中非金属夹杂物: 工业实践 [M]. 北京: 冶金工业出版社, 2019: 1
|
| [6] |
Ilegbusi O J, Szekely J. Melt stratification in ladles [J]. ISIJ Int., 1987, 27: 563
doi: 10.2355/isijinternational1966.27.563
|
| [7] |
Austin P R, Camplin J M, Herbertson J, et al. Mathematical modelling of thermal stratification and drainage of steel ladles [J]. ISIJ Int., 1992, 32: 196
doi: 10.2355/isijinternational.32.196
|
| [8] |
Chakraborty S, Sahai Y. Effect of holding time and surface cover in ladles on liquid steel flow in continuous casting tundishes [J]. Metall. Trans., 1992, 23B: 153
|
| [9] |
Chakraborty S, Sahai Y. Effect of slag cover on heat loss and liquid steel flow in ladles before and during teeming to a continuous casting tundish [J]. Metall. Trans., 1992, 23B: 135
|
| [10] |
Olika B, Pan Y H, Björkman B, et al. Numerical simulation and industrial investigation on the melt stratification phenomena in ladles holding molten steel [J]. Scand. J. of Metall., 1996, 25(1): 18
|
| [11] |
Grip C E, Jonsson L, Jönsson P, et al. Numerical prediction and experimental verification of thermal stratification during holding in pilot plant and production ladles [J]. ISIJ Int., 1999, 39: 715
doi: 10.2355/isijinternational.39.715
|
| [12] |
Xia J L, Ahokainen T. Transient flow and heat transfer in a steelmaking ladle during the holding period [J]. Metall. Mater. Trans., 2001, 32B: 733
|
| [13] |
Xia J L, Ahokainen T. Thermal stratification in a steel ladle [J]. Can. Metall. Quart., 2001, 40: 479
doi: 10.1179/cmq.2001.40.4.479
|
| [14] |
Pan Y H, Björkman B. Numerical analysis on the similarity between steel ladles and hot-water models regarding natural convection phenomena [J]. ISIJ Int., 2002, 42: 53
doi: 10.2355/isijinternational.42.53
|
| [15] |
Pan Y H, Björkman B. Physical and mathematical modelling of thermal stratification phenomena in steel ladles [J]. ISIJ Int., 2002, 42: 614
doi: 10.2355/isijinternational.42.614
|
| [16] |
Pan Y H, Grip C E, Björkman B. Numerical studies on the parameters influencing steel ladle heat loss rate, thermal stratification during holding and steel stream temperature during teeming [J]. Scand. J. Metall., 2003, 32: 71
doi: 10.1034/j.1600-0692.2003.10608.x
|
| [17] |
Zhang C J, Wang A, Li Q X, et al. Analysis of temperture drop during 80 t ladle standing [J]. Henan Metall., 2013, 21: 20
|
| [17] |
张彩军, 王 昂, 李庆效 等. 80 t钢包静置过程温降分析 [J]. 河南冶金, 2013, 21: 20
|
| [18] |
Lu B Y, Meng X N, Zhu M Y. Numerical analysis for the heat transfer behavior of steel ladle as the thermoelectric waste-heat source [J]. Catal. Today, 2018, 318: 180
doi: 10.1016/j.cattod.2017.10.038
|
| [19] |
Duan H J, Ren Y, Zhang L F. Fluid flow, thermal stratification, and inclusion motion during holding period in steel ladles [J]. Metall. Mater. Trans., 2019, 50B: 1476
|
| [20] |
Gopala Krishna E D, Shamshoddin S, Ande R. Numerical simulation of fluid flow and heat transfer in a ductile iron ladle during holding and teeming [J]. J. Thermal. Sci. Eng. Appl., 2019, 11: 011007
|
| [21] |
Yan H, Conejo A N, Zhang H, et al. Numerical simulation of heat transfer during ladle holding period [J]. Cont. Cast., 2022, (1): 31
|
| [21] |
颜 晗, Conejo A N, 张 晗 等. 钢包静置过程中传热现象的数值模拟 [J]. 连铸, 2022, (1): 31
|
| [22] |
Huang C D, Duan H J, Zhang L F. Modeling of motion of inclusions in argon-stirred steel ladles [J]. Steel Res. Int., 2024, 95: 2300537
doi: 10.1002/srin.v95.11
|
| [23] |
Morsi S A, Alexander A J. An investigation of particle trajectories in two-phase flow systems [J]. J. Fluid Mech., 1972, 55: 193
doi: 10.1017/S0022112072001806
|
| [24] |
Pearson K. The problem of the random walk [J]. Nature, 1905, 72: 294
|
| [25] |
Duan H J, Huang C D, Zhang L F. Numerical simulation of transient flow and heat transfer in a steel ladle during holding period [J]. Metall. Mater. Trans., 2024, 55B: 2273
|
| [26] |
Duan H J, Ren Y, Zhang L F. Effects of interphase forces on fluid flow in gas-stirred steel ladles using the Eulerian-Lagrangian multiphase approach [J]. JOM, 2018, 70: 2128
doi: 10.1007/s11837-018-3045-3
|
| [27] |
Duan H J, Zhang L F, Thomas B G, et al. Fluid flow, dissolution, and mixing phenomena in argon-stirred steel ladles [J]. Metall. Mater. Trans., 2018, 49B: 2722
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|