| Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟 |
石腾龙1,2, 陈娟2, 赵彬3, 史俊勤1( ) |
1 西北工业大学 材料学院 先进润滑与密封材料研究中心 西安 710072 2 太原科技大学 材料科学与工程学院 太原 030024 3 西安赛福斯材料防护有限责任公司 西安 710200 |
|
| Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation |
SHI Tenglong1,2, CHEN Juan2, ZHAO Bin3, SHI Junqin1( ) |
1 Center of Advanced Lubrication and Seal Materials, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China 2 School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China 3 Xi'an Surface Material Protection Co. Ltd., Xi'an 710200, China |
引用本文:
石腾龙, 陈娟, 赵彬, 史俊勤. Cu/Ta纳米双层膜拉伸变形及Al、W原子掺杂对其变形影响的分子动力学模拟[J]. 金属学报, 2026, 62(7): 1297-1309.
Tenglong SHI,
Juan CHEN,
Bin ZHAO,
Junqin SHI.
Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation[J]. Acta Metall Sin, 2026, 62(7): 1297-1309.
| [1] |
Chen H B. Fabrication and property of Ta-based diffusion barrier for Cu interconnection in new generation IC [D]. Changsha: Central South University, 2007
|
| [1] |
陈海波. 新一代集成电路Cu互连用Ta基扩散阻挡层的制备及特性研究 [D]. 长沙: 中南大学, 2007
|
| [2] |
Holloway K, Fryer P M, Cabral Jr C, et al. Tantalum as a diffusion barrier between copper and silicon: Failure mechanism and effect of nitrogen additions [J]. J. Appl. Phys., 1992, 71: 5433
doi: 10.1063/1.350566
|
| [3] |
Fullwood D T, Niezgoda S R, Adams B L, et al. Microstructure sensitive design for performance optimization [J]. Prog. Mater. Sci., 2010, 55: 477
doi: 10.1016/j.pmatsci.2009.08.002
|
| [4] |
Mondal S, Polley D, Pattabi A, et al. Single-shot switching in Tb/Co-multilayer based nanoscale magnetic tunnel junctions [J]. J. Magn. Magn. Mater., 2023, 581: 170960
doi: 10.1016/j.jmmm.2023.170960
|
| [5] |
Sakhonenkov S S, Filatova E O. Nanoscale W/Be multilayers: Intermixing during magnetron sputtering deposition and effect of heat treatment [J]. Appl. Surf. Sci., 2022, 571: 151265
doi: 10.1016/j.apsusc.2021.151265
|
| [6] |
Tran A S, Fang T H. Dislocation interaction and fracture of Cu/Ta bilayer interfaces [J]. Phys. Scr., 2019, 94: 095402
|
| [7] |
Feng X T, Lin Z J, Xin K, et al. The deformation mechanisms and mechanical properties of Cu/Fe multilayer during compression process [J]. J. Mater. Res., 2021, 36: 3203
doi: 10.1557/s43578-021-00333-z
|
| [8] |
Zhang R F, Wang J, Beyerlein I J, et al. Dislocation nucleation mechanisms from fcc/bcc incoherent interfaces [J]. Scr. Mater., 2011, 65: 1022
doi: 10.1016/j.scriptamat.2011.09.008
|
| [9] |
Chen Y, Li N, Hoagland R G, et al. Effects of three-dimensional Cu/Nb interfaces on strengthening and shear banding in nanoscale metallic multilayers [J]. Acta Mater., 2020, 199: 593
doi: 10.1016/j.actamat.2020.08.019
|
| [10] |
Wang Y, Zhu X Y, Liu G M, et al. Strain rate sensitivity of Cu/Ni and Cu/Nb nanoscale multilayers [J]. Acta Metall. Sin., 2017, 53: 183
|
| [10] |
王 尧, 朱晓莹, 刘贵民 等. Cu/Ni和Cu/Nb纳米多层膜的应变率敏感性 [J]. 金属学报, 2017, 53: 183
|
| [11] |
Zhang R F, Wang J, Beyerlein I J, et al. Atomic-scale study of nucleation of dislocations from fcc-bcc interfaces [J]. Acta Mater., 2012, 60: 2855
doi: 10.1016/j.actamat.2012.01.050
|
| [12] |
Lu L, Huang C, Pi W L, et al. Molecular dynamics simulation of effects of interface imperfections and modulation periods on Cu/Ta multilayers [J]. Comp. Mater. Sci., 2018, 143: 63
doi: 10.1016/j.commatsci.2017.10.034
|
| [13] |
Shi T L, Xu L L, Chen J, et al. Influence of grain boundary and twin boundary on the stretching deformation behaviors of Cu/Ta interface material [J]. Mater. Today Commun., 2024, 39: 108633
|
| [14] |
Tu A D, Teng C Y, Wang H, et al. Molecular dynamics simulation of the structure and deformation behavior of γ/α2 interface in TiAl alloys [J]. Acta Metall. Sin., 2019, 55: 291
|
| [14] |
涂爱东, 滕春禹, 王 皞 等. Ti-Al合金γ/α2界面结构及拉伸变形行为的分子动力学模拟 [J]. 金属学报, 2019, 55: 291
doi: 10.11900/0412.1961.2018.00182
|
| [15] |
Karimzadeh A, Rouhaghdam A S, Aliofkhazraei M, et al. Sliding wear behavior of Ni-Co-P multilayer coatings electrodeposited by pulse reverse method [J]. Tribol. Int., 2020, 141: 105914
doi: 10.1016/j.triboint.2019.105914
|
| [16] |
Major L, Lackner J M, Kot M, et al. Nanostructural aspects of the wear process of multilayer tribological coatings [J]. Tribol. Int., 2020, 151: 106411
doi: 10.1016/j.triboint.2020.106411
|
| [17] |
Shi J Q, Li L L, Wang J Y, et al. Alloy strengthening toward improving mechanical and tribological performances of Cu x Ni100 - x /Ta nano multilayer materials [J]. Tribol. Int., 2023, 190: 109039
doi: 10.1016/j.triboint.2023.109039
|
| [18] |
Bai Z W, Ding Z G, Zhou A L, et al. Molecular dynamics simulation of thermo-kinetics of tensile deformation of α-Fe single crystal [J]. Acta Metall. Sin., 2024, 60: 848
|
| [18] |
柏智文, 丁志刚, 周爱龙 等. α-Fe单晶拉伸变形热-动力学的分子动力学模拟 [J]. 金属学报, 2024, 60: 848
doi: 10.11900/0412.1961.2022.00606
|
| [19] |
Zhang J Y, Qu Q M, Wang Y Q, et al. Research progress on irradiation effects and mechanical properties of metal/high-entropy alloy nanostructured multilayers [J]. Acta Metall. Sin., 2022, 58: 1371
doi: 10.11900/0412.1961.2022.00113
|
| [19] |
张金钰, 屈启蒙, 王亚强 等. 金属/高熵合金纳米多层膜的力学性能及其辐照效应研究进展 [J]. 金属学报, 2022, 58: 1371
doi: 10.11900/0412.1961.2022.00113
|
| [20] |
Abraham F F. Computational statistical mechanics methodology, applications and supercomputing [J]. Adv. Phys., 1986, 35: 1
doi: 10.1080/00018738600101851
|
| [21] |
Stukowski A. Structure identification methods for atomistic simulations of crystalline materials [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 045021
|
| [22] |
Choudhuri D, Srinivasan S G, Mishra R S. Deformation of lamellar FCC-B2 nanostructures containing Kurdjumov-Sachs interfaces: Relation between interfacial structure and plasticity [J]. Int. J. Plast., 2020, 125: 191
doi: 10.1016/j.ijplas.2019.09.014
|
| [23] |
Zhou Q, Ren Y, Du Y, et al. Cracking and toughening mechanisms in nanoscale metallic multilayer films: A brief review [J]. Appl. Sci., 2018, 8: 1821
doi: 10.3390/app8101821
|
| [24] |
Mendelev M I, Han S, Srolovitz D J, et al. Development of new interatomic potentials appropriate for crystalline and liquid iron [J]. Philos. Mag., 2003, 83: 3977
doi: 10.1080/14786430310001613264
|
| [25] |
Wei M Z, Cao Z H, Shi J, et al. Anomalous plastic deformation in nanoscale Cu/Ta multilayers [J]. Mater. Sci. Eng., 2014, A598: 355
|
| [26] |
Zhao X, Lu C, Tieu A K, et al. Deformation mechanisms and slip-twin interactions in nanotwinned body-centered cubic iron by molecular dynamics simulations [J]. Comput. Mater. Sci., 2018, 147: 34
|
| [27] |
An M R, Song H Y, Deng Q, et al. Influence of interface with mismatch dislocations on mechanical properties of Ti/Al nanolaminate [J]. J. Appl. Phys., 2019, 125: 165307
doi: 10.1063/1.5085455
|
| [28] |
Liu Y, Yang K M, Hay J, et al. The effect of coherent interface on strain-rate sensitivity of highly textured Cu/Ni and Cu/V multilayers [J]. Scr. Mater., 2019, 162: 33
doi: 10.1016/j.scriptamat.2018.10.021
|
| [29] |
Yin F X, Zhao Y Z, Yu S Y, et al. Molecular dynamics studies on the interface evolution characteristics and deformation mechanisms of Cu/Al multilayers during compression process [J]. J. Appl. Phys., 2019, 125: 025112
|
| [30] |
Eder S J, Rodríguez Ripoll M, Cihak-Bayr U, et al. Unraveling and mapping the mechanisms for near-surface microstructure evolution in CuNi alloys under sliding [J]. ACS Appl. Mater. Interfaces, 2020, 12: 32197
doi: 10.1021/acsami.0c09302
|
| [31] |
Wang J Y, Shi J Q, Lu Y, et al. Deformation evolution of Cu/Ta nanoscale multilayer during nanoindentation by a molecular dynamics study [J]. Surf. Coat. Technol., 2022, 441: 128562
doi: 10.1016/j.surfcoat.2022.128562
|
| [32] |
Shi J Q, Wang J Y, Yi X B, et al. Nanoscratching-induced plastic deformation mechanism and tribology behavior of Cu/Ta bilayer and multilayer by a molecular dynamics study [J]. Appl. Surf. Sci., 2022, 586: 152775
doi: 10.1016/j.apsusc.2022.152775
|
| [33] |
Wang T, Jin L, Shi T L, et al. Effect of Al and W atom doping on the deformation mechanism and tribological properties of Cu95 X5/Ta nanobilayer by molecular dynamics simulation [J]. Tribol. Int., 2025, 210: 110818
doi: 10.1016/j.triboint.2025.110818
|
| [34] |
Faken D, Jónsson H. Systematic analysis of local atomic structure combined with 3D computer graphics [J]. Comput. Mater. Sci., 1994, 2: 279
doi: 10.1016/0927-0256(94)90109-0
|
| [35] |
Stukowski A, Bulatov V V, Arsenlis A. Automated identification and indexing of dislocations in crystal interfaces [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 085007
|
| [36] |
Fu E G, Li N, Misra A, et al. Mechanical properties of sputtered Cu/V and Al/Nb multilayer films [J]. Mater. Sci. Eng., 2008, A493: 283
|
| [37] |
Bain E C. Factors affecting the inherent hardenability of steel [J]. J. Heat Treat., 1979, 1: 57
|
| [38] |
Burgers W G. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium [J]. Physica, 1934, 1: 561
doi: 10.1016/S0031-8914(34)80244-3
|
| [39] |
Bertin N, Carson R, Bulatov V V, et al. Crystal plasticity model of BCC metals from large-scale MD simulations [J]. Acta Mater., 2023, 260: 119336
doi: 10.1016/j.actamat.2023.119336
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|