| 脉冲电流对AZ91镁合金温挤压过程中动态析出和微观组织的影响 |
王彬杉1,2, 徐光1,2, 任睿1,2, 张强1,2,3, 单召辉4, 樊建锋1,2,3( ) |
1 太原理工大学 新材料界面科学与工程教育部重点实验室 太原 030024 2 太原理工大学 材料科学与工程学院 太原 030024 3 太原理工大学 镁基材料山西省重点实验室 太原 030024 4 太原理工大学 物理与光电学院 太原 030024 |
|
| Effect of Electropulse on Dynamic Precipitation and Microstructure of AZ91 Magnesium Alloy During Warm Extrusion |
WANG Binshan1,2, XU Guang1,2, REN Rui1,2, ZHANG Qiang1,2,3, SHAN Zhaohui4, FAN Jianfeng1,2,3( ) |
1 Key Laboratory of Interface Science and Engineering in Advanced Materials, Ministry of Education, Taiyuan University of Technology, Taiyuan 030024, China 2 College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024, China 3 Shanxi Key Laboratory of Advanced Magnesium Based Materials, Taiyuan University of Technology, Taiyuan 030024, China 4 College of Physics and Optoelectronics, Taiyuan University of Technology, Taiyuan 030024, China |
引用本文:
王彬杉, 徐光, 任睿, 张强, 单召辉, 樊建锋. 脉冲电流对AZ91镁合金温挤压过程中动态析出和微观组织的影响[J]. 金属学报, 2025, 61(1): 129-142.
Binshan WANG,
Guang XU,
Rui REN,
Qiang ZHANG,
Zhaohui SHAN,
Jianfeng FAN.
Effect of Electropulse on Dynamic Precipitation and Microstructure of AZ91 Magnesium Alloy During Warm Extrusion[J]. Acta Metall Sin, 2025, 61(1): 129-142.
| 1 |
Aghion E, Bronfin B. Magnesium alloys development towards the 21st century[J]. Mater. Sci. Forum, 2000, 350-351: 19
|
| 2 |
Mordike B L, Ebert T. Magnesium: Properties-applications-potential[J]. Mater. Sci. Eng., 2001, A302: 37
|
| 3 |
Chen X H, Pan F S, Mao J J, et al. Effect of heat treatment on strain hardening of ZK60 Mg alloy[J]. Mater. Des., 2011, 32: 1526
|
| 4 |
Xu Q, Tang G Y, Jiang Y B. Thermal and electromigration effects of electropulsing on dynamic recrystallization in Mg-3Al-1Zn alloy[J]. Mater. Sci. Eng., 2011, A528: 4431
|
| 5 |
Wang S N. Effect of electric pulses on drawability and corrosion property of AZ31 magnesium alloy[D]. Beijing: Tsinghua University, 2009
|
| 5 |
王少楠. 电脉冲对AZ31镁合金冲压性能和腐蚀性能的影响[D]. 北京: 清华大学, 2009
|
| 6 |
Shan Z H, Yang J, Fan J F, et al. Extraordinary mechanical properties of AZ61 alloy processed by ECAP with 160° channel angle and EPT[J]. J. Magnes. Alloy., 2021, 9: 548
|
| 7 |
Jiang L Y, Zhang D F, Fan X W, et al. Microstructure and mechanical properties of as-extruded AZ80-xSn magnesium alloys[J]. Mater. Sci. Technol., 2016, 32: 1838
|
| 8 |
Stanford N, Atwell D. The effect of Mn-rich precipitates on the strength of AZ31 extrudates[J]. Metall. Mater. Trans., 2013, 44A: 4830
|
| 9 |
Moreau G, Cornet J A, Calais D. Acceleration de la diffusion chimique sous irradiation dans le systeme aluminium-magnesium[J]. J. Nucl. Mater., 1971, 38: 197
|
| 10 |
Zhu T P, Chen Z W, Gao W. Dissolution of eutectic β-Mg17Al12 phase in magnesium AZ91 cast alloy at temperatures close to eutectic temperature[J]. J. Mater. Eng. Perform., 2010, 19: 860
|
| 11 |
Shan Z H, Yang J, Fan J F, et al. Microstructure evolution and mechanical properties of an AZ61 alloy processed with TS-ECAP and EPT[J]. Mater. Sci. Eng., 2020, A780: 139195
|
| 12 |
Godfrey A, Cao W Q, Liu Q, et al. Stored energy, microstructure, and flow stress of deformed metals[J]. Metall. Mater. Trans., 2005, 36A: 2371
|
| 13 |
Lin B Y, Zhang H, Meng Y P, et al. Deformation behavior, microstructure evolution, and dynamic recrystallization mechanism of an AZ31 Mg alloy under high-throughput gradient thermal compression[J]. Mater. Sci. Eng., 2022, A847: 143338
|
| 14 |
Xu H, Liu M, Wang Y P, et al. Refined microstructure and dispersed precipitates in a gradient rolled AZ91 alloy under pulsed current[J]. Materialia, 2021, 20: 101245
|
| 15 |
Jeong H J, Kim M J, Park J W, et al. Effect of pulsed electric current on dissolution of Mg17Al12 phases in as-extruded AZ91 magnesium alloy[J]. Mater. Sci. Eng., 2017, A684: 668
|
| 16 |
Shan Z H, Zhang Y X, Wang B S, et al. Microstructural evolution and precipitate behavior of an AZ61 alloy plate processed with ECAP and electropulsing treatment[J]. J. Mater. Res. Technol., 2022, 19: 382
|
| 17 |
Qin R S, Samuel E I, Bhowmik A. Electropulse-induced cementite nanoparticle formation in deformed pearlitic steels[J]. J. Mater. Sci., 2011, 46: 2838
|
| 18 |
Conrad H. Influence of an electric or magnetic field on the liquid-solid transformation in materials and on the microstructure of the solid[J]. Mater. Sci. Eng., 2000, A287: 205
|
| 19 |
Qin R S, Zhou B L. Effect of electric current pulses on grain size in castings[J]. Int. J. Non-Equilib. Process., 1998, 11: 77
|
| 20 |
Wang X L, Guo J D, Wang Y M, et al. Segregation of lead in Cu-Zn alloy under electric current pulses[J]. Appl. Phys. Lett., 2006, 89: 061910
|
| 21 |
Jiang Y B, Tang G Y, Shek C, et al. Effect of electropulsing treatment on microstructure and tensile fracture behavior of aged Mg-9Al-1Zn alloy strip[J]. Appl. Phys., 2009, 97A: 607
|
| 22 |
Onodera Y, Hirano K. The effect of a.c. frequency on precipitation in Al-5.6 at % Zn[J]. J. Mater. Sci., 1984, 19: 3935
|
| 23 |
Sprecher A F, Mannan S L, Conrad H. On the temperature rise associated with the electroplastic effect in titanium[J]. Scr. Metall., 1983, 17: 769
|
| 24 |
Porter D A, Easterling K E, Sherif M Y. Phase Transformations in Metals and Alloys (Revised Reprint)[M]. 3rd Ed., Boca Raton: CRC Press, 2009: 312
|
| 25 |
Nabarro F R N. Dislocations in Solids[M]. Amsterdam: Elsevier, 1989: 499
|
| 26 |
Sprecher A F, Mannan S L, Conrad H. Overview no. 49: On the mechanisms for the electroplastic effect in metals[J]. Acta Metall., 1986, 34: 1145
|
| 27 |
Kim S H, You B S, Park S H. Effect of billet diameter on hot extrusion behavior of Mg-Al-Zn alloys and its influence on microstructure and mechanical properties[J]. J. Alloys Compd., 2017, 690: 417
|
| 28 |
Braszczyńska-Malik K N. Spherical shape of γ-Mg17Al12 precipitates in AZ91 magnesium alloy processed by equal-channel angular pressing[J]. J. Alloys Compd., 2009, 487: 263
|
| 29 |
Lee S W, Han G, Jun T S, et al. Effects of initial texture on deformation behavior during cold rolling and static recrystallization during subsequent annealing of AZ31 alloy[J]. J. Mater. Sci. Technol., 2021, 66: 139
doi: 10.1016/j.jmst.2020.04.074
|
| 30 |
Di H S, Zhang X M, Wang G D, et al. Spheroidizing kinetics of eutectic carbide in the twin roll-casting of M2 high-speed steel[J]. J. Mater. Process. Technol., 2005, 166: 359
|
| 31 |
Huang K, Marthinsen K, Zhao Q L, et al. The double-edge effect of second-phase particles on the recrystallization behaviour and associated mechanical properties of metallic materials[J]. Prog. Mater. Sci., 2018, 92: 284
|
| 32 |
Shi D K. Fundamentals of Materials Science[M]. 2nd Ed., Beijing: China Machine Press, 2003: 363
|
| 32 |
石德珂. 材料科学基础[M]. 第2版, 北京: 机械工业出版社, 2003: 363
|
| 33 |
Guo F, Zhang D F, Yang X S, et al. Strain-induced dynamic precipitation of Mg17Al12 phases in Mg-8Al alloys sheets rolled at 748 K[J]. Mater. Sci. Eng., 2015, A636: 516
|
| 34 |
Yan T L, Pei D, Cheng M H, et al. Development of Mg-6Al-4Sn-1Zn alloy sheets with ultra-high strength by combining extrusion and high-speed rolling[J]. J. Mater. Res. Technol., 2024, 29: 1487
|
| 35 |
Zhang Q, Li Q A, Chen X Y, et al. Dynamic precipitation and recrystallization mechanism during hot compression of Mg-Gd-Y-Zr alloy[J]. J. Mater. Res. Technol., 2021, 15: 37
doi: 10.1016/j.jmrt.2021.08.013
|
| 36 |
Okazaki K, Kagawa M, Conrad H. A study of the electroplastic effect in metals[J]. Scr. Metall., 1978, 12: 1063
|
| 37 |
Okazaki K, Kagawa M, Conrad H. Additional results on the electroplastic effect in metals[J]. Scr. Metall., 1979, 13: 277
|
| 38 |
Xiang S Q, Zhang X F. Dislocation structure evolution under electroplastic effect[J]. Mater. Sci. Eng., 2019, A761: 138026
|
| 39 |
Bhattacharyya J J, Agnew S R, Muralidharan G. Texture enhancement during grain growth of magnesium alloy AZ31B[J]. Acta Mater., 2015, 86: 80
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|