| Ti30Ni50Hf20 高温形状记忆合金的热变形行为 |
姜沐池1,2, 宫继双3, 杨兴远2, 任德春2( ), 蔡雨升2, 李秉洋4,5, 吉海宾2( ), 雷家峰1,2 |
1 中国科学技术大学 材料科学与工程学院 沈阳 110016 2 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 3 中山大学 航空航天学院 广州 510275 4 中国航天科技创新研究院 先进材料与能源中心 北京 100163 5 北京大学 工学院 北京 100871 |
|
| Hot Deformation Behavior of Ti30Ni50Hf20 High-Temperature Shape Memory Alloy |
JIANG Muchi1,2, GONG Jishuang3, YANG Xingyuan2, REN Dechun2( ), CAI Yusheng2, LI Bingyang4,5, JI Haibin2( ), LEI Jiafeng1,2 |
1 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 2 Shi -changxu Advanced Materials Innovation Center, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 3 School of Aeronautics and Astronautics, Sun Yat-Sen University, Guangzhou 510275, China 4 Advanced Materials and Energy Center, China Academy of Aerospace Science and Innovation, Beijing 100163, China 5 College of Engineering, Peking University, Beijing 100871, China |
引用本文:
姜沐池, 宫继双, 杨兴远, 任德春, 蔡雨升, 李秉洋, 吉海宾, 雷家峰. Ti30Ni50Hf20 高温形状记忆合金的热变形行为[J]. 金属学报, 2025, 61(6): 857-865.
Muchi JIANG,
Jishuang GONG,
Xingyuan YANG,
Dechun REN,
Yusheng CAI,
Bingyang LI,
Haibin JI,
Jiafeng LEI.
Hot Deformation Behavior of Ti30Ni50Hf20 High-Temperature Shape Memory Alloy[J]. Acta Metall Sin, 2025, 61(6): 857-865.
| 1 |
Singh S, Karthick S, Palani I A. Design and development of Cu-Al-Ni shape memory alloy coated optical fiber sensor for temperature sensing applications [J]. Vacuum, 2021, 191: 110369
|
| 2 |
Chen F, Qiu P C, Liu Y, et al. Microstructure and mechanical properties of NiTi shape memory alloys by in situ laser directed energy deposition [J]. Acta Metall. Sin., 2023, 59: 180
doi: 10.11900/0412.1961.2022.00425
|
| 2 |
陈 斐, 邱鹏程, 刘 洋 等. 原位激光定向能量沉积NiTi形状记忆合金的微观结构和力学性能 [J]. 金属学报, 2023, 59: 180
|
| 3 |
Es-Souni M, Fischer-Brandies H. Assessing the biocompatibility of NiTi shape memory alloys used for medical applications [J]. Anal. Bioanal. Chem., 2005, 381: 557
pmid: 15660223
|
| 4 |
Abbas A, Hung H Y, Lin P C, et al. Atomic layer deposited TiO2 films on an Equiatomic NiTi shape memory alloy for biomedical applications [J]. J. Alloys Compd., 2021, 886: 161282
|
| 5 |
Ren D C, Zhang H B, Li S J, et al. Properties of Ti-Ni pre-alloyed powder used for electron beam melting [J]. Rare Met. Mater. Eng., 2020, 49: 3218
|
| 5 |
任德春, 张慧博, 李述军 等. 电子束增材制造技术用Ti-Ni预合金粉末性能研究 [J]. 稀有金属材料与工程, 2020, 49: 3218
|
| 6 |
Feng Z W, Cui Y, Shang Z Y, et al. Development of NiTiZr high temperature shape memory alloys [J]. Mater. Rep., 2016, 30(suppl.2) : 616
|
| 6 |
冯昭伟, 崔 跃, 尚再艳 等. 镍钛锆高温形状记忆合金的研究进展 [J]. 材料导报, 2016, 30(): 616
|
| 7 |
Li Q Q, Li Y, Ma Y H. Research progress of titanium-based high-temperature shape memory alloy [J]. Mater. Rep., 2020, 34: 148
|
| 7 |
李启泉, 李 岩, 马悦辉. 钛基高温形状记忆合金进展综述 [J]. 材料导报, 2020, 34: 148
|
| 8 |
Canadinc D, Trehern W, Ma J, et al. Ultra-high temperature multi-component shape memory alloys [J]. Scr. Mater., 2019, 158: 83
|
| 9 |
Yi X Y, Meng X L, Cai W, et al. Research progress in Ti-Ni-Hf high temperature shape memory alloys [J]. J. Mater. Eng., 2021, 49(3): 31
|
| 9 |
衣晓洋, 孟祥龙, 蔡 伟 等. Ti-Ni-Hf高温形状记忆合金的研究进展 [J]. 材料工程, 2021, 49(3): 31
doi: 10.11868/j.issn.1001-4381.2020.000531
|
| 10 |
Zuo S G, Jin X J, Jin M J. Research progress in high temperature shape memory alloys [J]. Mater. Mech. Eng., 2014, 38(1): 1
|
| 10 |
左舜贵, 金学军, 金明江. 高温形状记忆合金的研究进展 [J]. 机械工程材料, 2014, 38(1): 1
|
| 11 |
Meng X K, Zhao C W. Research progress on Ti-Ni-Hf high temperature shape memory alloy [J]. Mater. Rep., 2013, 27(3): 99
|
| 11 |
孟晓凯, 赵春旺. 钛镍铪高温形状记忆合金的研究进展 [J]. 材料导报, 2013, 27(3): 99
|
| 12 |
Liao B, Cao L F, Wu X D, et al. Hot deformation behavior and processing map of 7A55 aluminum alloy in double thermo-mechanical treatment process [J]. Nonferrous Met. Eng., 2021, 11(2): 1
|
| 12 |
廖 斌, 曹玲飞, 吴晓东 等. 双级形变热处理工艺中7A55铝合金热变形行为及热加工图 [J]. 有色金属工程, 2021, 11(2): 1
|
| 13 |
Ma X, Xu S Y, Zhou G, et al. Thermal deformation behavior of Ni60Ti40 shape memory alloy [J]. China Metall., 2022, 32(9): 26
|
| 13 |
马 昕, 许斯洋, 周 舸 等. Ni60Ti40形状记忆合金的热变形行为 [J]. 中国冶金, 2022, 32(9): 26
|
| 14 |
Zhu L Z, Lu S Q, Shu X Y, et al. Hot deformation behavior and constitutive relationships of Ni-40Ti shape memory alloy [J]. Spec. Cast. Nonferrous Alloys, 2016, 36: 425
|
| 14 |
朱乐宗, 鲁世强, 舒小勇 等. Ni-40Ti形状记忆合金热变形行为及本构关系的建立 [J]. 特种铸造及有色合金, 2016, 36: 425
|
| 15 |
Zhao Y N, Jiang S Y, Zhang Y Q, et al. Hot deformation behavior and processing map of NiTi shape memory alloy [J]. Appl. Sci. Technol., 2017, 44(1): 76
|
| 15 |
赵亚楠, 江树勇, 张艳秋 等. NiTi形状记忆合金的热变形行为及热加工图 [J]. 应用科技, 2017, 44(1): 76
|
| 16 |
Karelin R, Komarov V, Cherkasov V, et al. Production, mechanical and functional properties of long-length TiNiHf rods with high-temperature shape memory effect [J]. Materials, 2023, 16: 615
|
| 17 |
Tugrul H O, Akgul O, Kockar B. Creep behavior of 50at%Ni 25at%Ti 25at%Hf high temperature shape memory alloy under constant load [J]. Mater. Today Commun., 2022, 33: 104827
|
| 18 |
Meng X L, Cai W, Zheng Y F, et al. Phase transformation and precipitation in aged Ti-Ni-Hf high-temperature shape memory alloys [J]. Mater. Sci. Eng., 2006, A438-440: 666
|
| 19 |
Chen S H, Wang Q Y, Jiang H C, et al. Effect of δ-ferrite on hot deformation and recrystallization of 316KD austenitic stainless steel for sodium-cooled fast reactor application [J]. Acta Metall. Sin., 2024, 60: 367
|
| 19 |
陈胜虎, 王琪玉, 姜海昌 等. δ-铁素体对钠冷快堆用316KD奥氏体不锈钢热变形行为和动态再结晶的影响 [J]. 金属学报, 2024, 60: 367
doi: 10.11900/0412.1961.2022.00039
|
| 20 |
Li F L, Fu R, Bai Y R, et al. Effects of initial grain size and strengthening phase on thermal deformation and recrystallization behavior of GH4096 superalloy [J]. Acta Metall. Sin., 2023, 59: 855
doi: 10.11900/0412.1961.2021.00532
|
| 20 |
李福林, 付 锐, 白云瑞 等. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响 [J]. 金属学报, 2023, 59: 855
doi: 10.11900/0412.1961.2021.00532
|
| 21 |
Luo L S, Wang F X, Wu X M, et al. Hot deformation and processing maps of low cost Ti-Al-V-Fe-O alloy [J]. Rare Met. Mater. Eng., 2018, 47: 2049
|
| 21 |
骆良顺, 王富鑫, 吴晓明 等. 低成本Ti-Al-V-Fe-O合金热变形行为及热加工图 [J]. 稀有金属材料与工程, 2018, 47: 2049
|
| 22 |
Liu Q Q, Lu Y, Zhang Y F, et al. Thermal deformation behavior of Al19.3Co15Cr15Ni50.7 high entropy alloy [J]. Acta Metall. Sin., 2021, 57: 1299
|
| 22 |
刘庆琦, 卢 晔, 张翼飞 等. Al19.3Co15Cr15Ni50.7高熵合金的热变形行为 [J]. 金属学报, 2021, 57: 1299
doi: 10.11900/0412.1961.2020.00349
|
| 23 |
Bai X H, Zhao X C, Zhao D L, et al. Research on thermal deformation behavior of a high carbon Cr5 roll steel [J]. MW Met. Form., 2021, (12): 68
|
| 23 |
白兴红, 赵席春, 赵德利 等. 一种高碳Cr5轧辊钢的热变形行为研究 [J]. 金属加工热加工, 2021, (12): 68
|
| 24 |
Hua S M, Zhang P Z, Liu Z L, et al. Hot deformation behavior and hot working map of Cu-0.58Sn alloy [J]. Nonferrous Met. Eng., 2021, 11(10): 40
|
| 24 |
花思明, 张平则, 刘子利 等. Cu-0.58Sn合金热变形行为和热加工图 [J]. 有色金属工程, 2021, 11(10): 40
|
| 25 |
Tian L, Ji H B, Lei J F, et al. Study on constitutive relationship for hot deformation of Ti6242s Alloy [J]. Hot Work. Technol., 2013, 42(20): 97
|
| 25 |
田 录, 吉海宾, 雷家峰 等. Ti6242s合金本构关系的研究 [J]. 热加工工艺, 2013, 42(20): 97
|
| 26 |
Huang Y L, Wang J B, Ling X S, et al. Research development of hot processing map theory [J]. Mater. Rep., 2008, 22(suppl.3): 173
|
| 26 |
黄有林, 王建波, 凌学士 等. 热加工图理论的研究进展 [J]. 材料导报, 2008, 22(): 173
|
| 27 |
Semiatin S L, Seetharaman V, Weiss I. Flow behavior and globularization kinetics during hot working of Ti-6Al-4V with a colony alpha microstructure [J]. Mater. Sci. Eng., 1999, A263: 257
|
| 28 |
Bobbili R, Madhu V. Hot deformation behavior and processing maps of Ti-15Al-12Nb alloy [J]. Rare Met., 2022, 41: 2316
|
| 29 |
Lv B J, Peng J, Wang Y J, et al. Dynamic recrystallization behavior and hot workability of Mg-2.0Zn-0.3Zr-0.9Y alloy by using hot compression test [J]. Mater. Des., 2014, 53: 357
|
| 30 |
Wei L L, Pan Q L, Zhou J, et al. Processing maps and flow instability analysis of Al-Zn-Mg-Cu-Zr alloy [J]. J. Cent. South Univ. (Sci. Technol.), 2013, 44: 1798
|
| 30 |
韦莉莉, 潘清林, 周 坚 等. Al-Zn-Mg-Cu-Zr合金加工图的构建及失稳分析 [J]. 中南大学学报(自然科学版), 2013, 44: 1798
|
| 31 |
Lei W G, Han D, Zhang Y Q, et al. Hot deformation mechanism and processing map of TC4-DT titanium alloy [J]. Titanium Ind. Prog., 2015, 32(1): 20
|
| 31 |
雷文光, 韩 栋, 张永强 等. TC4-DT钛合金热变形机制及加工图 [J]. 钛工业进展, 2015, 32(1): 20
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|