| 脉冲电流作用下Pb-Al合金的液-固分相过程 |
李彦强1,2, 赵九洲1,2( ), 江鸿翔1,2, 张丽丽1, 何杰1,2 |
1 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 2 中国科学技术大学 材料科学与工程学院 沈阳 110016 |
|
| Liquid-Solid Phase Separation Process of Pb-Al Alloy Under the Effect of Electric Current Pulses |
LI Yanqiang1,2, ZHAO Jiuzhou1,2( ), JIANG Hongxiang1,2, ZHANG Lili1, HE Jie1,2 |
1 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
李彦强, 赵九洲, 江鸿翔, 张丽丽, 何杰. 脉冲电流作用下Pb-Al合金的液-固分相过程[J]. 金属学报, 2024, 60(12): 1710-1720.
Yanqiang LI,
Jiuzhou ZHAO,
Hongxiang JIANG,
Lili ZHANG,
Jie HE.
Liquid-Solid Phase Separation Process of Pb-Al Alloy Under the Effect of Electric Current Pulses[J]. Acta Metall Sin, 2024, 60(12): 1710-1720.
| 1 |
Cao Y D. Preparation and performance of a novel lead-based alloy anode for zinc electrowinning [D]. Kunming: Kunming University of Science and Technology, 2009
|
| 1 |
曹远栋. 锌电积用新型铅基合金阳极的制备及性能研究 [D]. 昆明: 昆明理工大学, 2009
|
| 2 |
Cole J F, Goodwin F E. The development and potential applications of a Pb-Al alloy [J]. JOM, 1990, 42(6): 41
|
| 3 |
Hu J, Sun Y, Jiang D H, et al. Development of Al-Pb system research [J]. J. Kunming Univ. Sci. Technol. (Sci. Technol.), 2003, 28(1): 23
|
| 3 |
胡 劲, 孙 勇, 姜东慧 等. Al-Pb体系研究进展 [J]. 昆明理工大学学报(理工版), 2003, 28(1): 23
|
| 4 |
Yu S K, Sommer F, Predel B. Isopiestic measurements and assessment of the Al-Pb system [J]. Int. J. Mater. Res., 1996, 87: 574
|
| 5 |
Ahmed T, Jiang H X, Li W, et al. Solidification of Pb-Al alloys under the influence of electric current pulses [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 842
|
| 6 |
Chen Z X, Ding H S, Chen R R, et al. Microstructural evolution and mechanism of solidified TiAl alloy applied electric current pulse [J]. Acta Metall. Sin., 2019, 55: 611
doi: 10.11900/0412.1961.2018.00504
|
| 6 |
陈占兴, 丁宏升, 陈瑞润 等. 脉冲电流作用下TiAl合金凝固组织演变及形成机理 [J]. 金属学报, 2019, 55: 611
doi: 10.11900/0412.1961.2018.00504
|
| 7 |
Zhang X F, Yan L G. Regulating the non-metallic inclusions by pulsed electric current in molten metal [J]. Acta Metall. Sin., 2020, 56: 257
doi: 10.11900/0412.1961.2019.00391
|
| 7 |
张新房, 闫龙格. 脉冲电流调控金属熔体中的非金属夹杂物 [J]. 金属学报, 2020, 56: 257
doi: 10.11900/0412.1961.2019.00391
|
| 8 |
Nakada M, Shiohara Y, Flemings M C. Modification of solidification structures by pulse electric discharging [J]. ISIJ Int., 1990, 30: 27
|
| 9 |
Balasubramani N, Xu Y Y, Zhang Y H, et al. Investigating the grain refinement mechanisms of pulsed electric current, ultrasonic and melt stirring solidification of pure aluminium [J]. JOM, 2021, 73: 3873
doi: 10.1007/s11837-021-04904-7
|
| 10 |
Zhang L M, Liu H N, Li N, et al. The relevance of forced melt flow to grain refinement in pure aluminum under a low-frequency alternating current pulse [J]. J. Mater. Res., 2016, 31: 396
|
| 11 |
Xu Z, Wang X, Liang D, et al. Electric current pulse induced grain refinement in pure aluminium [J]. Mater. Sci. Technol., 2015, 31: 1595
|
| 12 |
Wang W J, Yuan T C, Li R D, et al. Electrochemical corrosion behaviors of Pb-Ag anodes by electric current pulse assisted casting [J]. J. Electroanal. Chem., 2019, 847: 113250
|
| 13 |
Li N, Zhang L M, Zhang R, et al. Research on grain refinement in hypoeutectic Al-Si alloy during solidification under an alternating electric current pulse [J]. Metals, 2019, 9: 571
|
| 14 |
Zhu J, Wang T M, Cao F, et al. Real-time observation on evolution of droplets morphology affected by electric current pulse in Al-Bi immiscible alloy [J]. J. Mater. Eng. Perform., 2013, 22: 1319
|
| 15 |
Ma T, Sun X S, Ning Y N, et al. Solidification microstructure characteristics of Cu-Pb alloy by ECP treatment [J]. High Temp. Mater. Process., 2021, 40: 382
|
| 16 |
Jiang H X, Zhao J Z, Wang C P, et al. Effect of electric current pulses on solidification of immiscible alloys [J]. Mater. Lett., 2014, 132: 66
|
| 17 |
Jiang H X, He J, Zhao J Z. Influence of electric current pulses on the solidification of Cu-Bi-Sn immiscible alloys [J]. Sci. Rep., 2015, 5: 12680
doi: 10.1038/srep12680
pmid: 26228180
|
| 18 |
Lv H Y, Zhou R F, Li L, et al. Effect of electric current pulse on microstructure and corrosion resistance of hypereutectic high chromium cast Iron [J]. Materials, 2018, 11: 2220
|
| 19 |
Geng B Y, Zhou R F, Li Y K, et al. The difference in effects of electric current pulses on inoculation of austenite and M7C3 carbides [J]. Mater. Res. Express, 2020, 7: 096506
|
| 20 |
Gao B Y, Meng X R, Cao Z Q, et al. Bidirectional pulsed current effect on the precipitation behavior of Cu6Sn5: An in situ observation [J]. Mater. Today Commun., 2021, 29: 102825
|
| 21 |
Zhang J, Liu J D, Zhang X F, et al. Effect of high density current pulses on microstructure and mechanical properties of dual-phase wrought superalloy [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 1635
|
| 22 |
Zhao J Z, Ratke L, Jia J, et al. Modeling and simulation of the microstructure evolution during a cooling of immiscible alloys in the miscibility gap [J]. J. Mater. Sci. Technol., 2002, 18: 197
|
| 23 |
Shangguan D, Ahuja S, Stefanescu D M. An analytical model for the interaction between an insoluble particle and an advancing solid/liquid interface [J]. Metall. Trans., 1992, 23A: 669
|
| 24 |
Jiang H X. Study of the continuous solidification of monotectic alloys under the effect of electric current [D]. Shenyang: University of Chinese Academy of Sciences, 2014
|
| 24 |
江鸿翔. 电流作用下偏晶合金连续凝固过程研究 [D]. 沈阳: 中国科学院大学, 2014
|
| 25 |
Li H L, Zhao J Z. Convective effect on the microstructure evolution during a liquid-liquid decomposition [J]. Appl. Phys. Lett., 2008, 92: 241902
|
| 26 |
Einstein A. A new determination of molecular dimensions [J]. Ann. Phys., 1906, 19: 289
|
| 27 |
Zhao J, Ratke L. Repeated nucleation of minority phase droplets induced by drop motion [J]. Scr. Mater., 1998, 39: 181
|
| 28 |
Iida T, Guthrie R I L, translated by Xian A P, Wang L W. The Physical Properties of Liquid Metals [M]. Beijing: Science Press, 2006: 256
|
| 28 |
Iida T, Guthrie R I L著, 冼爱平, 王连文译. 液态金属的物理性能 [M]. 北京: 科学出版社, 2006: 256
|
| 29 |
Li Y Q, Zhao J Z, Jiang H X, et al. Microstructure formation in directionally solidified Pb-Al alloy [J]. Acta Metall. Sin., 2022, 58: 1072
doi: 10.11900/0412.1961.2021.00492
|
| 29 |
李彦强, 赵九洲, 江鸿翔 等. Pb-Al合金定向凝固组织形成过程 [J]. 金属学报, 2022, 58: 1072
doi: 10.11900/0412.1961.2021.00492
|
| 30 |
Gránásy L, Ratke L. Homogeneous nucleation within the liquid miscibility gap of Zn-Pb alloys [J]. Scr. Metall. Mater., 1993, 28: 1329
|
| 31 |
Qin R S, Zhou B L. Effect of electric current pulses on grain size in castings [J]. Int. J. Non-Equilib. Process., 1998, 11: 77
|
| 32 |
Deng C K, Jiang H X, Zhao J Z, et al. Study on the solidification of Ag-Ni monotectic alloy [J]. Acta Metall. Sin., 2020, 56: 212
doi: 10.11900/0412.1961.2019.00192
|
| 32 |
邓聪坤, 江鸿翔, 赵九洲 等. Ag-Ni偏晶合金凝固过程研究 [J]. 金属学报, 2020, 56: 212
doi: 10.11900/0412.1961.2019.00192
|
| 33 |
He J, Zhao J Z, Ratke L. Solidification microstructure and dynamics of metastable phase transformation in undercooled liquid Cu-Fe alloys [J]. Acta Mater., 2006, 54: 1749
|
| 34 |
Li H L, Zhao J Z, Zhang Q X, et al. Microstructure formation in a directionally solidified immiscible alloy [J]. Metall. Mater. Trans., 2008, 39A: 3308
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|