| 冲击疲劳循环形变阶段的晶界行为 |
| 张萌 杨平生 刘炎 谈育煦 |
| 西安交通大学材料科学与工程系; 西安 710049 |
|
引用本文:
张萌; 杨平生; 刘炎; 谈育煦 . 冲击疲劳循环形变阶段的晶界行为[J]. 金属学报, 1999, 35(7): 703-706 .
[1] Lim L C, Raj R. Acta Matall, 1984 32: 1183 [2] Liu W, Bayerlein M, Mughrabi H, Day A and Quested P N Acta Metall Matet 1992; 40: 1763 [3] Kim W H, Laird C Acta Metall, 1978 26: 777 [4]Tanaka T,Nakayama H,Kimura K.Fatigue Fract Eng Mater Struct, 1985; 8: 13 [5] Yang P S, Zhang M, Xu F, Gong S P Mater Sci Eng, 1997; A234—236:127 [6] Yang P S, Zhou H J Fatigue, 1994 16: 567 [7]Yang P S,Zhang Q F J Nanchang Univ Nat Sci,1994 18(1): 41 (杨平生,张奇凤南昌大学学报(理科版),19942 18(1):41) [8] Song Y J. Grain Boundary and Strength of Metals. Xi’an: Xi’an Jiaotong University Press, 1988: 93 (宋余九金属的晶界与强度西安:西安交通大学出版社,1988: 93)y |
|