| <111>取向小角偏离对一种镍基单晶高温合金蠕变性能的影响 |
胡斌,李树索,裴延玲,宫声凯( ),徐惠彬 |
| 北京航空航天大学材料科学与工程学院 北京 100191 |
|
| Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy |
HU Bin,LI Shusuo,PEI Yanling,GONG Shengkai( ),XU Huibin |
| School of Materials Science and Engineering, Beihang University, Beijing 100191, China |
引用本文:
胡斌,李树索,裴延玲,宫声凯,徐惠彬. <111>取向小角偏离对一种镍基单晶高温合金蠕变性能的影响[J]. 金属学报, 2019, 55(9): 1204-1210.
Bin HU,
Shusuo LI,
Yanling PEI,
Shengkai GONG,
Huibin XU.
Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy[J]. Acta Metall Sin, 2019, 55(9): 1204-1210.
| [1] | ReedR C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 121 | | [2] | MatanN, CoxD C, CarterP, , et al. Creep of CMSX-4 superalloy single crystals: Effects of misorientation and temperature [J]. Acta Mater., 1999, 47: 1549 | | [3] | WuX, ZhangJ H, LiuJ L, , et al. Plastic deformation inhomogeneity in a single crystal nickel-base superalloy [J]. Mater. Sci. Eng., 2002, A325: 478 | | [4] | WangL N, LiuY, YuJ J, , et al. Orientation and temperature dependence of yielding and deformation behavior of a nickel-base single crystal superalloy [J]. Mater. Sci. Eng., 2009, A505: 144 | | [5] | HanG M, YuJ J, SunX F, , et al. Effect of threshold stress on anisotropic creep properties of single crystal nickel-base superalloy SRR99 [J]. J. Mater. Sci. Technol., 2012, 28: 439 | | [6] | MacKayR A, MaierR D. The influence of orientation on the stress rupture properties of nickel-base superalloy single crystals [J]. Metall. Trans., 1982, 13A: 1747 | | [7] | LeverantG R, KearB H. The mechanism of creep in gamma prime precipitation-hardened nickel-base alloys at intermediate temperatures [J]. Metall. Mater. Trans., 1970, 1B: 491 | | [8] | SassV, GlatzelU, Feller-KniepmeierM. Anisotropic creep properties of the nickel-base superalloy CMSX-4 [J]. Acta Mater., 1996, 44: 1967 | | [9] | SassV, Feller-KniepmeierM. Orientation dependence of dislocation structures and deformation mechanisms in creep deformed CMSX-4 single crystals [J]. Mater. Sci. Eng., 1998, A245: 19 | | [10] | RaeC M F, ReedR C. Primary creep in single crystal superalloys: Origins, mechanisms and effects [J]. Acta Mater., 2007, 55: 1067 | | [11] | RaeC M F, RistM A, CoxD C, , et al. On the primary creep of CMSX-4 superalloy single crystals [J]. Metall. Mater. Trans., 2000, 31A: 2219 | | [12] | KnowlesD M, ChenQ Z. Superlattice stacking fault formation and twinning during creep in γ/γ' single crystal superalloy CMSX-4 [J]. Mater. Sci. Eng., 2003, A340: 88 | | [13] | JiaY X, JinT, LiuJ L, , et al. Anisotropic creep in a Ni-based single crystal superalloy [J]. Acta Metall. Sin., 2009, 45: 1364 | | [13] | 贾玉贤, 金 涛, 刘金来等. 一种镍基单晶高温合金的蠕变各向异性 [J]. 金属学报, 2009, 45: 1364 | | [14] | LiuJ L, JinT, SunX F, , et al. Anisotropy of stress rupture properties of a Ni base single crystal superalloy at two temperatures [J]. Mater. Sci. Eng., 2008, A479: 277 | | [15] | HanG M, YuJ J, SunY L, , et al. Anisotropic stress rupture properties of the nickel-base single crystal superalloy SRR99 [J]. Mater. Sci. Eng., 2010, A527: 5383 | | [16] | HopgoodA A, MartinJ W. The creep behaviour of a nickel-based single-crystal superalloy [J]. Mater. Sci. Eng., 1986, 82: 27 | | [17] | KakehiK. Influence of secondary precipitates and crystallographic orientation on the strength of single crystals of a Ni-based superalloy [J]. Metall. Mater. Trans., 1999, 30A: 1249 | | [18] | LinkT, Feller-KniepmeierM. Shear mechanisms of the γ' phase in single-crystal superalloys and their relation to creep [J]. Metall. Trans., 1992, 23A: 99 | | [19] | DiologentF, CaronP. On the creep behavior at 1033 K of new generation single-crystal superalloys [J]. Mater. Sci. Eng., 2004, A385: 245 | | [20] | HuisA J. Boom G, Bronsveld P M,, et al. Superlattice intrinsic stacking faults in γ' precipitates [J]. Scr. Metall., 1985, 19: 1123 | | [21] | CondatM, DécampsB. Shearing of γ′ precipitates by single a/2<110>matrix dislocations in a γ/γ′ Ni-based superalloy [J]. Scr. Metall., 1987, 21: 607 | | [22] | CourbonJ, LouchetF, IgnatM, , et al. Analysis of in situ shearing mechanisms of γ' precipitates in a nickel-based superalloy at 1120 K [J]. Phil. Mag. Lett., 1991, 63: 73 | | [23] | PollockT M, FieldR D. Dislocations in Solids [M]. Chapter 63, Amsterdam: Elsevier Science & Technology Press, 2002: 549 | | [24] | GunturiS S K, MacLachlanD W, KnowlesD M. Anisotropic creep in CMSX-4 in orientations distant from <001> [J]. Mater. Sci. Eng., 2000,A289: 289 | | [25] | ZhangS H, WangD, ZhangJ, , et al. Orientation dependence of stress rupture properties of a Ni-based single crystal superalloy at 760 ℃ [J]. J. Mater. Sci. Technol., 2012, 28: 229 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|