金属轧制复合过程微观变形行为的分子动力学建模及研究 |
张清东,李硕,张勃洋( ),谢璐,李瑞 |
北京科技大学机械工程学院 北京 100083 |
|
Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process |
Qingdong ZHANG,Shuo LI,Boyang ZHANG( ),Lu XIE,Rui LI |
School of Mechanical Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
张清东,李硕,张勃洋,谢璐,李瑞. 金属轧制复合过程微观变形行为的分子动力学建模及研究[J]. 金属学报, 2019, 55(7): 919-927.
Qingdong ZHANG,
Shuo LI,
Boyang ZHANG,
Lu XIE,
Rui LI.
Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process. Acta Metall Sin, 2019, 55(7): 919-927.
链接本文:
https://www.ams.org.cn/CN/10.11900/0412.1961.2018.00524
或
https://www.ams.org.cn/CN/Y2019/V55/I7/919
|
[1] | Luo Z A, Wang G L, Xie G M, et al. Interfacial microstructure and properties of a vacuum hot roll-bonded titanium-stainless steel clad plate with a niobium interlayer [J]. Acta Metall. Sin. (Eng. Lett.), 2013, 26: 754 | [2] | Rong J H, Hong X, Xiang G Y, et al. Research on finishing rolling force model for hot rolling wide and heavy stainless steel clad sheets [J]. Appl. Mech. Mater., 2014, 488-489: 213 | [3] | Zhang Q D, Li S, Liu J Y, et al. Study of a bimetallic interfacial bonding process based on ultrasonic quantitative evaluation [J]. Metals, 2018, 8: 329 | [4] | Tzou G Y, Tieu A K, Huang M N, et al. Analytical approach to the cold-and-hot bond rolling of sandwich sheet with outer hard and inner soft layers [J]. J. Mater. Process. Technol., 2002, 125-126: 664 | [5] | Peng Z H, She X F. Effect of thickness ratio on the properties of stainless steel clad aluminum sheet [J]. Acta Metall. Sin., 2000, 36: 1067 | [5] | (彭志辉, 佘旭凡. 厚度比对不锈钢复合铝板性能的影响 [J]. 金属学报, 2000, 36: 1067) | [6] | Zepeda-Ruiz L A, Stukowski A, Oppelstrup T, et al. Probing the limits of metal plasticity with molecular dynamics simulations [J]. Nature, 2017, 550: 492 | [7] | Song J, Srolovitz D J. Molecular dynamics investigation of patterning via cold welding [J]. J. Mech. Phys. Solids, 2009, 57: 776 | [8] | Yuan L, Jing P, Liu Y H, et al. Molecular dynamics simulation of polycrystal silver nanowires under tensile deformation [J]. Acta Phys. Sin., 2014, 63: 016201 | [8] | (袁 林, 敬 鹏, 刘艳华等. 多晶银纳米线拉伸变形的分子动力学模拟研究 [J]. 物理学报, 2014, 63: 016201) | [9] | He A M, Shao J L, Wang P, et al. Plastic deformation of single-crystalline copper films with surface orientation [001]: Molecular dynamics simulations [J]. Acta Phys. Sin., 2010, 59: 8836 | [9] | (何安民, 邵建立, 王 裴等. 单晶Cu(001)薄膜塑性变形的分子动力学模拟 [J]. 物理学报, 2010, 59: 8836) | [10] | Zhang H W, Fu Y F, Zheng Y G, et al. Molecular dynamics investigation of plastic deformation mechanism in bulk nanotwinned copper with embedded cracks [J]. Phys. Lett., 2014, 378A: 736 | [11] | Mendelev M I, Srolovitz D J, Ackland G J, et al. Effect of Fe segregation on the migration of a non-symmetric Σ5 tilt grain boundary in Al [J]. J. Mater. Res., 2005, 20: 208 | [12] | Bonny G, Pasianot R C, Castin N, et al. Ternary Fe-Cu-Ni many-body potential to model reactor pressure vessel steels: First validation by simulated thermal annealing [J]. Philos. Mag., 2009, 89: 3531 | [13] | Stukowski A, Sadigh B, Erhart P, et al. Efficient implementation of the concentration-dependent embedded atom method for molecular-dynamics and Monte-Carlo simulations [J]. Modell. Simul. Mater. Sci. Eng., 2009, 17: 075005 | [14] | Zheng D L, Chen S D, Soh A K, et al. Molecular dynamics simulations of glide dislocations induced by misfit dislocations at the Ni/Al interface [J]. Comput. Mater. Sci., 2010, 48: 551 | [15] | Hoagland R G, Hirth J P, Misra A. On the role of weak interfaces in blocking slip in nanoscale layered composites [J]. Philos. Mag., 2006, 86: 3537 | [16] | Wang J, Misra A. An overview of interface-dominated deformation mechanisms in metallic multilayers [J]. Curr. Opin. Solid State Mater. Sci., 2011, 15: 20 | [17] | Shao S, Medyanik S N. Interaction of dislocations with incoherent interfaces in nanoscale FCC-BCC metallic bi-layers [J]. Modell. Simul. Mater. Sci. Eng., 2010, 18: 055010 | [18] | Wang J, Hoagland R G, Hirth J P, et al. Atomistic simulations of the shear strength and sliding mechanisms of copper-niobium interfaces [J]. Acta Mater., 2008, 56: 3109 | [19] | Misra A, Hirth J P, Hoagland R G. Length-scale-dependent deformation mechanisms in incoherent metallic multilayered composites [J]. Acta Mater., 2005, 53: 4817 | [20] | Weng S Y, Ning H M, Hu N, et al. Strengthening effects of twin interface in Cu/Ni multilayer thin films—A molecular dynamics study [J]. Mater. Des., 2016, 111: 1 | [21] | Luo X, Qian G F, Wang Y M. Computer simulation of metal interfaces [J]. Acta Phys. Sin., 1994, 43: 1957 | [21] | (罗 旋, 钱革非, 王煜明. Ag/Ni和Cu/Ni界面的分子动力学模拟 [J]. 物理学报, 1994, 43: 1957) | [22] | Cheng D, Yan Z J, Yan L. Molecular dynamics simulation of strengthening mechanism of Cu/Ni multilayers [J]. Acta Metall. Sin., 2008, 44: 1461 | [22] | (程 东, 严志军, 严 立. Cu/Ni多层膜强化机理的分子动力学模拟 [J]. 金属学报, 2008, 44: 1461) | [23] | Cheng C, Chen S D, Wu Y Z, et al. Molecular dynamics simulations of deformation behaviors for nanocrystalline Cu/Ni films under different strain rates [J]. J. Mater. Eng., 2015, 43(3): 60 | [23] | (成 聪, 陈尚达, 吴勇芝, 等. 不同应变率下纳米多晶Cu/Ni薄膜变形行为的分子动力学模拟 [J]. 材料工程, 2015, 43(3): 60) | [24] | Bonny G, Castin N, Terentyev D. Interatomic potential for studying ageing under irradiation in stainless steels: The FeNiCr model alloy [J]. Modell. Simul. Mater. Sci. Eng., 2013, 21: 085004 | [25] | Eich S M, Beinke D, Schmitz G. Embedded-atom potential for an accurate thermodynamic description of the iron-chromium system [J]. Comput. Mater. Sci., 2015, 104: 185 | [26] | Kelchner C L, Plimpton S J, Hamilton J C. Dislocation nucleation and defect structure during surface indentation [J]. Phys. Rev., 1998, 58B: 11085 | [27] | Yu J, Xin L, Wang J J, et al. First-principles study of the relaxation and energy of bcc-Fe, fcc-Fe and AISI-304 stainless steel surfaces [J]. Appl. Surf. Sci., 2009, 255: 9032 | [28] | Stukowski A, Albe K. Extracting dislocations and non-dislocation crystal defects from atomistic simulation data [J]. Modell. Simul. Mater. Sci. Eng., 2010, 18: 085001 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|