| 高锰TRIP钢冷轧以及α'-M逆转变过程的相变和织构演变 |
王丽娜1,2, 杨平1( ), 李凯1, 崔凤娥1, 毛卫民1 |
1 北京科技大学材料科学与工程学院 北京 100083 2 北京科技大学天津学院材料系 天津 301830 |
|
| Phase Transformation and Texture Evolution During Cold Rolling and α'-M Reversion in High Manganese TRIP Steel |
Lina WANG1,2, Ping YANG1( ), Kai LI1, Feng'e CUI1, Weimin MAO1 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 2 Department of Materials, School of Tianjin, University of Science and Technology Beijing, Tianjin 301830, China |
引用本文:
王丽娜, 杨平, 李凯, 崔凤娥, 毛卫民. 高锰TRIP钢冷轧以及α'-M逆转变过程的相变和织构演变[J]. 金属学报, 2018, 54(12): 1756-1766.
Lina WANG,
Ping YANG,
Kai LI,
Feng'e CUI,
Weimin MAO.
Phase Transformation and Texture Evolution During Cold Rolling and α'-M Reversion in High Manganese TRIP Steel[J]. Acta Metall Sin, 2018, 54(12): 1756-1766.
| [1] | Frommeyer G, Brüx U, Neumann P.Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes[J]. ISIJ Int., 2003, 43: 438 | | [2] | Gr?ssel O, Krüger L, Frommeyer G, et al.High strength Fe-Mn-(Al, Si) TRIP/TWIP steels development-properties-application[J]. Int. J. Plast., 2000, 16: 1391 | | [3] | Bouaziz O, Allain S, Scott C P, et al.High manganese austenitic twinning induced plasticity steels: A review of the microstructure properties relationships[J]. Curr. Opin. Solid State Mater. Sci., 2011, 15: 141 | | [4] | Allain S, Chateau J P, Bouaziz O, et al. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe-Mn-C alloys [J]. Mater. Sci. Eng., 2004, A387-389: 158 | | [5] | Vercammen S, Blanpain B, De Cooman B C, et al. Cold rolling behaviour of an austenitic Fe-30Mn-3Si-3Al TWIP-steel: The importance of deformation twinning[J]. Acta Mater., 2004, 52: 2005 | | [6] | Gr?ssel O, Frommeyer G.Effect of martensitic phase transformation and deformation twinning on mechanical properties of Fe-Mn-Si-Al steels[J]. Mater. Sci. Technol., 1998, 14: 1213 | | [7] | Sato K, Ichinose M, Hirotsu Y, et al.Effects of deformation induced phase transformation and twinning on the mechanical properties of austenitic Fe-Mn-Al alloys[J]. ISIJ Int., 1989, 29: 868 | | [8] | Sun X R, Wang H Z, Yang P, et al.Mechanical behaviors and micro-shear structures of metals with different structures by high-speed compression[J]. Acta Metall. Sin., 2014, 50: 387(孙秀荣, 王会珍, 杨平等. 不同结构金属高速压缩力学行为及微观剪切结构差异[J]. 金属学报, 2014, 50: 387) | | [9] | Li J, Yang H Y, Yang P.Prolonged work hardening range in high manganese TRIP steel during adiabatic shear band formation[J]. Mater. Lett., 2014, 134: 180 | | [10] | Murata Y, Ohashi S, Uematsu Y.Recent trends in the production and use of high strength stainless steels[J]. ISIJ Int., 1993, 33: 711 | | [11] | Tomimura K, Takaki S, Tanimoto S, et al.Optimal chemical composition in Fe-Cr-Ni alloys for ultra grain refining by reversion from deformation induced martensite[J]. ISIJ Int., 1991, 31: 721 | | [12] | Cayron C, Barcelo F, de Carlan Y. The mechanisms of the fcc-bcc martensitic transformation revealed by pole figures[J]. Acta Mater., 2010, 58: 1395 | | [13] | Dash J, Otte H M.The martensite transformation in stainless steel[J]. Acta Metall., 1963, 11: 1169 | | [14] | Nagy E, Mertinger V, Tranta F, et al.Deformation induced martensitic transformation in stainless steels[J]. Mater. Sci. Eng., 2004, A378: 308 | | [15] | Ray R K, Jonas J J.Transformation textures in steels[J]. Int. Mater. Rev., 1990, 35: 1 | | [16] | Tomota Y, Gong W, Harjo S, et al.Reverse austenite transformation behavior in a tempered martensite low-alloy steel studied using in situ neutron diffraction[J]. Scr. Mater., 2017, 133: 79 | | [17] | Takaki S, Tomimur K, Ueda S.Effect of pre-cold-working on diffusional reversion of deformation induced martensite in metastable austenitic stainless steel[J]. ISIJ Int., 1994, 34: 522 | | [18] | Ma Y Q, Jin J E, Lee Y K.A repetitive thermomechanical process to produce nano-crystalline in a metastable austenitic steel[J]. Scr. Mater., 2005, 52: 1311 | | [19] | Hu B, Luo H W, Yang F, et al.Recent progress in medium-Mn steels made with new designing strategies, a review[J]. J. Mater. Sci. Technol., 2017, 33: 1457 | | [20] | Zhang Y, Jing X T, Lou B Z, et al.Mechanism and reversible behavior of the α′→γ transformation in 1Cr18Ni9Ti stainless steel[J]. J. Mater. Sci., 1999, 34: 3291 | | [21] | Tomimura K, Takaki S, Tokunaga Y.Reversion mechanism from deformation induced martensite to austenite in metastable austenitic stainless steels[J]. ISIJ Int., 1991, 31: 1431 | | [22] | Johannsen D L, Kyr?l?inen A, Ferreira P J.Influence of annealing treatment on the formation of nano/submicron grain size AISI 301 austenitic stainless steels[J]. Metall. Mater. Trans., 2006, 37A: 2325 | | [23] | Tomida T, Wakita M, Yasuyama M, et al.Memory effects of transformation textures in steel and its prediction by the double Kurdjumov-Sachs relation[J]. Acta Mater., 2013, 61: 2828 | | [24] | Watanabe S, Kunitake T.The influence of reduction-ratio in the hot-rolling on the strength and toughness of quenched and tempered steel[J]. Tetsu Hagané, 1975, 61: 828(渡辺征一, 邦武立郎. 調質鋼の強度と靱性におよぼす熱間圧延時の圧下比の影響[J]. 鉄と鋼, 1975, 61: 828) | | [25] | Kimmins S T, Gooch D J.Austenite memory effect in 1Cr-1Mo-0.75V(Ti, B) steel[J]. Met. Sci., 1983, 17: 519 | | [26] | Matsuda S, Okamura Y.Reverse transformation of low-carbon low alloy steels[J]. Tetsu Hagané, 1974, 60: 226(松田昭一, 岡村義弘. 低炭素低合金鋼の逆変態[J]. 鉄と鋼, 1974, 60: 226) | | [27] | Hara T, Maruyama N, Shinohara Y, et al.Abnormal α to γ transformation behavior of steels with a martensite and bainite microstructure at a slow reheating rate[J]. ISIJ Int., 2009, 49: 1792 | | [28] | Zhang L W, Yang P, Wang J H, et al.Transformation of {100} texture induced by surface effect in ultra-low carbon electrical steel[J]. J. Mater. Sci., 2016, 51: 8087 | | [29] | Zhang L W, Yang P, Mao W M.Opposite relationship between orientation selection and texture memory in the deformed electrical steel sheets during α→γ→α transformation[J]. J. Mater. Sci. Technol., 2017, 33: 1522 | | [30] | Lu F Y, Yang P, Meng L, et al.Behavior of martensite reverse transformation in 18Mn TRIP steel during warm deformation[J]. Acta Metall. Sin., 2010, 46: 1153(鲁法云, 杨平, 孟利等. 18Mn TRIP钢温变形过程中马氏体逆相变行为[J]. 金属学报, 2010, 46: 1153) | | [31] | Lü Y P, Hutchinson B, Molodov D A, et al.Effect of deformation and annealing on the formation and reversion of ε-martensite in an Fe-Mn-C alloy[J]. Acta Mater., 2010, 58: 3079 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|