核电站控制棒驱动机构驱动杆用1Cr13厚壁管材成分选择与工艺优化 |
都祥元, 苏国跃 |
中国科学院金属研究所, 沈阳 110016 |
|
COMPONENT SELECTION AND TECHNOLOGICAL OPTIMIZATION OF THICK WALL 1Cr13 TUBE USED AS CONTROL POLES IN NUCLEAR POWER STATION DRIVING MACHINES |
DU Xiangyuan, SU Guoyue |
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
都祥元 苏国跃. 核电站控制棒驱动机构驱动杆用1Cr13厚壁管材成分选择与工艺优化[J]. 金属学报, 2011, 47(9): 1155-1158.
,
.
COMPONENT SELECTION AND TECHNOLOGICAL OPTIMIZATION OF THICK WALL 1Cr13 TUBE USED AS CONTROL POLES IN NUCLEAR POWER STATION DRIVING MACHINES[J]. Acta Metall Sin, 2011, 47(9): 1155-1158.
[1] Lu S Y, Zhang T K, Kang X F, Yang C Q, Wang X. Stainless Steel, Beijing: Atomic Energy Press, 1995: 23
(陆世英, 张廷凯, 康喜范, 杨长强, 王熙. 不锈钢. 北京: 原子能出版社, 1995: 23)
[2] Cui Z Q. Metal and Heat Treatment. Beijing: Mechanical Industry Press, 1988: 285
(崔忠圻. 金属学与热处理. 北京: 机械工业出版社, 1988: 285)
[3] Barid J D. Met Mater, 1971; 4: 1
[4] Bao J. Spec Steel Technol, 2006; 11(2): 20
(鲍进. 特钢技术, 2006; 11(2): 20)
[5] Li H S. Spec Steel Technol, 2006; 12(4): 25
(李海生. 特钢技术, 2006; 12(4): 25)
[6] Zhang Y T. Manual for Heat Treatment Technician. Beijing: Mechanical Industry Press, 2005: 89
(张玉庭. 热处理技师手册. 北京: 机械工业出版社, 2005: 89)
[7] Woodfine B C. J Iron Steel Inst, 1953; 173: 229 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|