| 铝基非晶纳米晶复合涂层显微组织与腐蚀性能研究 |
梁秀兵1,2( ), 范建文1, 张志彬1, 陈永雄1,2 |
1 陆军装甲兵学院机械产品再制造国家工程研究中心 北京 100072 2 军事科学院国防科技创新研究院 北京 100071 |
|
| Microstructure and Corrosion Properties of Aluminum Base Amorphous and Nanocrystalline Composite Coating |
Xiubing LIANG1,2( ), Jianwen FAN1, Zhibin ZHANG1, Yongxiong CHEN1,2 |
1 National Engineering Research Center for Mechanical Product Remanufacturing, Academy of Armored Army Forces, Beijing 100072, China 2 Innovation Research Institute of National Defense Science and Technology, Academy of Military Sciences, Beijing 100071, China |
引用本文:
梁秀兵, 范建文, 张志彬, 陈永雄. 铝基非晶纳米晶复合涂层显微组织与腐蚀性能研究[J]. 金属学报, 2018, 54(8): 1193-1203.
Xiubing LIANG,
Jianwen FAN,
Zhibin ZHANG,
Yongxiong CHEN.
Microstructure and Corrosion Properties of Aluminum Base Amorphous and Nanocrystalline Composite Coating[J]. Acta Metall Sin, 2018, 54(8): 1193-1203.
| [1] | IABSE, translated by Shi G. Use and Application of High-Performance Steels for Steel Structures [M]. Beijing: China Architecture & Building Press, 2010: 1(国际桥梁与结构工程协会编著, 施刚译. 高性能钢材在钢结构中的应用 [M]. 北京: 中国建筑工业出版社, 2010: 1) | | [2] | Hou B R, Zhang D, Wang P.Marine corrosion and protection: Current status and prospect[J]. Bull. Chin. Acad. Sci., 2016, 31: 1326(侯保荣, 张盾, 王鹏. 海洋腐蚀防护的现状与未来[J]. 中国科学院院刊, 2016, 31: 1326) | | [3] | Cao H T, Li X T.Corrosion protection requirements and technical measures of fasteners based on the marine environment[J]. Surf. Technol., 2013, 42(1): 105(曹宏涛, 李雪亭. 基于海洋环境的紧固件腐蚀防护要求及技术措施[J]. 表面技术, 2013, 42(1): 105) | | [4] | Zhang Q X, Xu M, Wang X T, et al.Research progress of heavy-duty anticorrosive coating applied on marine steel structure[J]. Equip. Environ. Eng., 2015, 12(4): 60(张巧霞, 许沫, 王秀通等. 重防腐涂料在海洋工程钢结构中的研究进展[J]. 装备环境工程, 2015, 12(4): 60) | | [5] | Tachibana K, Morinaga Y, Mayuzumi M.Hot dip fine Zn and Zn-Al alloy double coating for corrosion resistance at coastal area[J]. Corros. Sci., 2007, 49: 149 | | [6] | Azaroual M A, Ei Harrak E F, Touir R, et al. Synergistic corrosion protection for galvanized steel in 3.0% NaCl solution by sodium gluconate and cationic surfactant[J]. J. Mol. Liq., 2016, 220: 549 | | [7] | Yaro A S, Khadom K W, Khadom A A.Study for prevention of steel corrosion by sacrificial anode cathodic protection[J]. Theor. Found. Chem. Eng., 2013, 47: 266 | | [8] | Lee H S, Singh J K, Park J H.Pore blocking characteristics of corrosion products formed on aluminum coating produced by arc thermal metal spray process in 3.5wt.% NaCl solution[J]. Construc. Build. Mater., 2016, 113: 905 | | [9] | Lou M, Hu Y L, Qiang W J, et al.Application of high velocity arc sprayed coatings in preventing steel structures from corrosion[J]. Mater. Prot., 2011, 44(3): 54(楼淼, 胡永乐, 强文江等. 高速电弧喷涂层在钢结构防腐蚀中的作用及应用现状[J]. 材料保护, 2011, 44(3): 54) | | [10] | Liang X B, Liu Y, Chen Y X, et al.Integrated technology of materials preparation and formation based on high velocity arc spraying[J]. J. Acad. Armored Force Eng., 2008, 22(6): 79(梁秀兵, 刘燕, 陈永雄等. 基于高速电弧喷涂的材料制备与成型一体化技术[J]. 装甲兵工程学院院报, 2008, 22(6): 79) | | [11] | Liang X B, Bai J Y, Cheng J B, et al.Study on amorphous and nanocrystalline composite coatings prepared by arc spraying process[J]. Thermal Spray Technol., 2009, 1(2): 23(梁秀兵, 白金元, 程江波等. 电弧喷涂非晶纳米晶复合涂层材料研究[J]. 热喷涂技术, 2009, 1(2): 23) | | [12] | Liu Q, Xiao H Q, Ma S N.Progress of arc spraying on anticorrosion coating[J]. Surf. Technol., 2004, 33(5): 15(刘谦, 肖宏清, 马世宁. 电弧喷涂防腐蚀涂层研究[J]. 表面技术, 2004, 33(5): 15) | | [13] | Li G H, Pan S P, Qin J Y, et al.Insight into thermodynamics and corrosion behavior of Al-Ni-Gd glassy alloys from atomic structure[J]. Corros. Sci., 2013, 66: 360 | | [14] | Jinal R, Raja V S, Gibson M A, et al.Effect of annealing below the crystallization temperature on the corrosion behavior of Al-Ni-Y metallic glasses[J]. Corros. Sci., 2014, 84: 54 | | [15] | Lahiri D K. Gill P, Scudino S, et al.Cold sprayed aluminum based glassy coating: Synthesis, wear and corrosion properties[J]. Surf. Coat. Technol., 2013, 232: 33 | | [16] | Tan C L, Zhu H M, Kuang T C, et al.Laser cladding Al-based amorphous-nanocrystalline composite coatings on AZ80 magnesium alloy under water cooling condition[J]. J. Alloys Compd., 2017, 690: 108 | | [17] | Henao J, Concustel A L, Cano I G, et al.Novel Al-based metallic glass coatings by cold gas spray[J]. Mater. Des., 2016, 94: 253 | | [18] | Liang X B, Zhang Z B, Chen Y X, et al.Study of Al-based amorphous and nanocrystalline composite coating[J]. Acta Metall. Sin., 2012, 48: 289(梁秀兵, 张志彬, 陈永雄等. 铝基非晶纳米晶复合涂层研究[J]. 金属学报, 2012, 48: 289) | | [19] | Liang X B, Chen Y X, Cheng J B, et al.The Arc Spraying Metastable Composite Coating Technology [M]. Beijing: Science Press, 2014: 151(梁秀兵, 陈永雄, 程江波等. 电弧喷涂亚稳态复合涂层技术 [M]. 北京: 科学出版社, 2014: 151) | | [20] | Luo D W, Li C B, Chen W W.Recent progress for metallic glass coatings[J]. Mater. Rev., 2015, 29(3): 88(罗大为, 李聪勃, 陈为为. 非晶态合金涂层的研究进展[J]. 材料导报, 2015, 29(3): 88) | | [21] | Verdon C, Karimi A, Martin J L.A study of high velocity oxy-fuel thermally sprayed tungsten carbide based coatings. Part 1: Microstructures[J]. Mater. Sci. Eng., 1998, A246: 11 | | [22] | Liu C, Zhao W M, Ai H, et al.Electrochemical corrosion behaviors of arc-sprayed aluminum coating[J]. J. Chin. Soc. Corros. Prot., 2011, 31: 62(刘存, 赵卫民, 艾华等. 电弧喷涂铝涂层的腐蚀电化学行为[J]. 中国腐蚀与防护学报, 2011, 31: 62) | | [23] | Cao C N.Principles of Electrochemistry of Corrosion [M]. 3rd Ed., Beijing: Chemical Industry Press, 2008: 255(曹楚南. 腐蚀电化学原理 [M]. 第3版. 北京: 化学工业出版社, 2008: 255) | | [24] | Wang X F, Wu X Q, Lin J G, et al.The influence of heat treatment on the corrosion behaviour of as-spun amorphous Al88Ni6La6 alloy in 0.01M NaCl solution[J]. Mater. Lett., 2007, 61: 1715 | | [25] | Wu X Q, Ma M, Chan C G, et al.Comparative study on thermodynamical and electrochemical behavior of Al88Ni6La6 and Al86Ni6La6Cu2 amorphous alloys[J]. J. Rare Earths, 2007, 25: 381 | | [26] | Roy A, Mandhyan A K, Sahoo K L, et al.Electrochemical response of amorphous and devitrified Al-Ni-La-X (X=Ag, Cu) alloys[J]. Mater. Corros., 2015, 60: 431 | | [27] | Gupta R K, Das H, Pal T K.Influence of processing parameters on induced energy, mechanical and corrosion properties of FSW butt joint of 7475 AA[J]. J. Mater. Eng. Perform., 2012, 21: 1645 | | [28] | Huang L C, Gu A, Liu H C, et al.Corrosion failure of aluminum alloy parts on airplane used in marine environment[J]. J. Beijing Univ. Aeron. Astron., 2008, 34: 1217(黄领才, 谷岸, 刘慧丛等. 海洋环境下服役飞机铝合金零件腐蚀失效分析[J]. 北京航空航天大学学报, 2008, 34: 1217) | | [29] | Dong C F, Sheng H, An Y H, et al.Local electrochemical behavior of 2A12 aluminium alloy in the initial stage of atmospheric corrosion under Cl- conditions[J]. J. Univ. Sci. Technol. Beijing, 2009, 31: 878(董超芳, 生海, 安英辉等. Cl-作用下2A12铝合金在大气环境中腐蚀初期的微区电化学行为[J]. 北京科技大学学报, 2009, 31: 878) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|