| 电爆炸一步法制备Cu-Zn合金超细微粉 |
| 王群 鲍海飞 杨海滨 郭伟力 邹广田 |
| 吉林大学超硬材料国家重点实验室;长春 130023 |
|
引用本文:
王群; 鲍海飞; 杨海滨; 郭伟力; 邹广田 . 电爆炸一步法制备Cu-Zn合金超细微粉[J]. 金属学报, 1999, 35(12): 1271-1273 .
[1] William G C. Phys Today, 1964; (8): 19 [2] Antonios E V. J Appl Phys, 1967; 38: 3081 [3] Ivanenkov G V, Mingaleev A R, Novikova T A, Pikuz S A,Romanova V M, Shelkovenko T A. Zh Tekh Fiz, 1995; 65:40 [4] Il'in A P, Nazarenko O B, Ushakov V Ya, Krasnyatov Yu A,Fedushchak T A. Technol Phys, 1996; 41: 1269 [5] Yavarovsky N A. Communication Russian Collages, Phys,1996; 4: 114 [6] Antonios E V. J Appl Phys, 1973; 44: 3593 [7] Vorob'ev V S, Rakhel'A D. High Temp, 1990; 28: 17 [8] Gleiter H. Prog Mater Sci, 1989; 33: 223 [9] Wagner M. Phys Rev, 1992; 845: 635 [10] Suryanarayana C. Bull Mater Sci, 1994; 17: 307 [11] Siegel R W, Fougere G E. Nanostruct Mater 1995; 6: 1 [12] Pabi S K, Murty B S. Mater Sci Eng, 1996; A214: 146 [13] Massalski T B. Binary Alloy Phase Diagrams, VOl.1, MetalsPark, Ohio: ASM, 1986: 980 [14] Pabi S K, Joardar J, Murty B S. J Mater Sci, 1996; 31: 3207 [15] Umakoshi M, Yoshitomi T, Kato A. J Mater Sci, 1995; 30:1240} |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|