| 高温磁场热处理Alnico8永磁合金组织粗化过程的稳定性分叉 |
| 褚卫国 费维栋 杨德庄 |
| 哈尔滨工业大学材料与工程学院; 哈尔滨 150001 |
|
引用本文:
褚卫国; 费维栋; 杨德庄 . 高温磁场热处理Alnico8永磁合金组织粗化过程的稳定性分叉[J]. 金属学报, 1999, 35(12): 1253-1258 .
[1] McCurrie R A In: Wohlfarth E P, ed, Ferromagnetic Met,Amsterdam: Springer-Verlag, 1982; 3: 107 [2] Hutten A, Haasen P. J Phes Colloq, 1986; (C7): 205 [3] Hetherington N G, Cerezo A, Jakubovics J P, Smith G D W.J Phes Colloq, 1984; (Cg): 429 [4] Zhu F, Alvensleben L V, Haasen P. Scr Metall, 1984; 18: 337 [5] Hutten A, Grune R. Scr Metall, 1986; 20: 551 [6] Pfeiffer J. Cobalt, 1969; 44: 115 [7] Abruzov M P, Paviyukov A A. Met Metalloved, 1965; 20:724(K O B AA. PhysMet Metallog, 1965; 20: 724) [8] Cowley S A, Hetherington M G, Jakubovics J P, Smith G DW. J Phys, 1986; C7: 211 [9] Pashkov P P, Fridman A, Granovsky E. IEEE Trans Magn,1970; 6: 211 [10] Miyazaki T, Seki K, Doi M, Kozakai T. J Mater Sci Eng,1986; 77: 125 [11] Miyazaki T, Imamura H, Kozakai T. J Mater Sci Eng, 1982;54: 9 [12] Haasen P. Liu Z G et al transl. Phase Transformation inMaterials. Beijing: Science Press, 1998: 251(Haasen P著刘治国等译 材料的相变 北京:科学出版社,1998:251) [13] Meng Z F. The Theory of Small Angle X-ray Scattering andIts Application. Changchun: Jilin Press of Sicience. 1996:14, 21(孟昭富 小角X射线散射理论及应用 长春:吉林科学出版社,1996: 14, 21)W |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|