| 0.12C-3.0Mn低碳中锰钢中残余奥氏体稳定性与低温韧性的关系 |
黄龙,邓想涛( ),刘佳,王昭东 |
| 东北大学轧制技术及连轧自动化国家重点实验室 沈阳 110819 |
|
| Relationship Between Retained Austenite Stability and Cryogenic Impact Toughness in 0.12C-3.0Mn Low Carbon Medium Manganese Steel |
Long HUANG,Xiangtao DENG( ),Jia LIU,Zhaodong WANG |
| State Key Laboratory of Rolling Technology and Automation, Northeastern University, Shenyang 110819, China |
引用本文:
黄龙,邓想涛,刘佳,王昭东. 0.12C-3.0Mn低碳中锰钢中残余奥氏体稳定性与低温韧性的关系[J]. 金属学报, 2017, 53(3): 316-324.
Long HUANG,
Xiangtao DENG,
Jia LIU,
Zhaodong WANG.
Relationship Between Retained Austenite Stability and Cryogenic Impact Toughness in 0.12C-3.0Mn Low Carbon Medium Manganese Steel[J]. Acta Metall Sin, 2017, 53(3): 316-324.
| [1] | Wang C J, Liang J X, Liu Z B, et al.Effect of metastable austenite on mechanical property and mechanism in cryogenic steel applied and oceaneering[J]. Acta Metall. Sin., 2016, 52: 385 | | [1] | (王长军, 梁剑雄, 刘振宝等. 亚稳奥氏体对低温海工用钢力学性能的影响与机理[J]. 金属学报, 2016, 52: 385) | | [2] | Zhang K, Tang D, Wu H B.Effect of heating rate before tempering on reversed austenite in Fe-9Ni-C alloy[J]. J. Iron Steel Res. Int., 2012, 19: 73 | | [3] | Gao G H, Zhang H, Gui X L, et al.Enhanced ductility and toughness in an ultrahigh-strength Mn-Si-Cr-C steel: The great potential of ultrafine filmy retained austenite[J]. Acta Mater., 2014, 76: 425 | | [4] | Chen J, Lv M Y, Tang S, et al.Correlation between mechanical properties and retained austenite characteristics in a low-carbon medium manganese alloyed steel plate[J]. Mater. Charact., 2015, 106: 108 | | [5] | Chen J, Lv M Y, Liu Z Y, et al.Combination of ductility and toughness by the design of fine ferrite/tempered martensite-austenite microstructure in a low carbon medium manganese alloyed steel plate[J]. Mater. Sci. Eng., 2015, A648: 51 | | [6] | Xie Z J, Yuan S F, Zhou W H, et al.Stabilization of retained austenite by the two-step intercritical heat treatment and its effect on the toughness of a low alloyed steel[J]. Mater. Des., 2014, 59: 193 | | [7] | Hoshino M, Saitoh N, Muraoka H, et al.Development of super-9% Ni steel plates with superior low-temperature toughness for LNG storage tanks[J]. Nippon Steel Technical Report, 2004, 90 | | [7] | (星野学, 斎藤直樹, 村岡寛英等. LNGタンク用高靭性スーパー9%Ni鋼の開発[J]. 新日鉄技報, 2004, 90) | | [8] | Niikura M, Morris J W.Thermal processing of ferritic 5Mn steel for toughness at cryogenic temperatures[J]. Metall. Trans., 1980, 11A: 1531 | | [9] | Kim J I, Syn C K, Morris J W.Microstructural sources of toughness in QLT-treated 5.5Ni cryogenic steel[J]. Metall. Trans., 1983, 14A: 93 | | [10] | Speer J G, Edmonds D V, Rizzo F C, et al.Partitioning of carbon from supersaturated plates of ferrite, with application to steel processing and fundamentals of the bainite transformation[J]. Curr. Opin. Solid St. M., 2004, 8: 219 | | [11] | Clarke A J, Speer J G, Miller M K, et al.Carbon partitioning to austenite from martensite or bainite during the quench and partition (Q&P) process: a critical assessment[J]. Acta Mater., 2008, 56: 16 | | [12] | Wu R M, Li W, Zhou S, et al.Effect of retained austenite on the fracture toughness of quenching and partitioning (Q&P)-treated sheet steels[J]. Metall. Mater. Trans., 2014, 45A: 1892 | | [13] | Xu Z Y.New processes for steel heat treatment[J]. Heat Treat., 2007, 22(1): 1 | | [13] | (徐祖耀. 钢热处理的新工艺[J]. 热处理, 2007, 22(1): 1) | | [14] | Xu Z Y.A brief introduction to quenching-partitioning-tempering (Q-P-T) process[J]. Heat Treat. Met., 2009, 34(6): 1 | | [14] | (徐祖耀. 淬火-碳分配-回火, 2009, 34(6): 1) | | [15] | Zhou W H, Guo H, Xie Z J, et al.High strength low-carbon alloyed steel with good ductility by combining the retained austenite and nano-sized precipitates[J]. Mater. Sci. Eng., 2013, A587: 365 | | [16] | Zhou W H, Wang X L, Venkatsurya P K C, et al. Structure-mechanical property relationship in a high strength low carbon alloy steel processed by two-step intercritical annealing and intercritical tempering[J]. Mater. Sci. Eng., 2014, A607: 569 | | [17] | Zhou W H, Xie Z J, Guo H, et al.Regulation of multi-phase microstructure and mechanical properties in a 700 MPa grade low carbon low alloy steel with good ductility[J]. Acta Metall. Sin., 2015, 51: 407 | | [17] | (周文浩, 谢振家, 郭晖等. 700 MPa级高塑低碳低合金钢的多相组织调控及性能[J]. 金属学报, 2015, 51: 407) | | [18] | Xie Z J, Han G, Zhou W H, et al.Study of retained austenite and nano-scale precipitation and their effects on properties of a low alloyed multi-phase steel by the two-step intercritical treatment[J]. Mater. Charact., 2016, 113: 60 | | [19] | Hu J, Du L X, Sun G S, et al.The determining role of reversed austenite in enhancing toughness of a novel ultra-low carbon medium manganese high strength steel[J]. Scr. Mater., 2015, 104: 87 | | [20] | Cai Z H, Ding H, Misra R D K, et al. Austenite stability and deformation behavior in a cold-rolled transformation-induced plasticity steel with medium manganese content[J]. Acta Mater., 2015, 84: 229 | | [21] | Zhang S, Findley K O.Quantitative assessment of the effects of microstructure on the stability of retained austenite in TRIP steels[J]. Acta Mater., 2013, 61: 1895 | | [22] | Zhou Q, Qian L H, Tan J, et al.Inconsistent effects of mechanical stability of retained austenite on ductility and toughness of transformation-induced plasticity steels[J]. Mater. Sci. Eng., 2013, A578: 370 | | [23] | Fultz B, Kim J I, Kim Y H, et al.The stability of precipitated austenite and the toughness of 9Ni steel[J]. Metall. Trans., 1985, 16A: 2237 | | [24] | Yuan L, Ponge D, Wittig J, et al.Nanoscale austenite reversion through partitioning, segregation and kinetic freezing: Example of a ductile 2 GPa Fe-Cr-C steel[J]. Acta Mater., 2012, 60: 2790 | | [25] | Tan X D, Xu Y B, Yang X L, et al.Microstructure-properties relationship in a one-step quenched and partitioned steel[J]. Mater. Sci. Eng., 2014, A589: 101 | | [26] | Santofimia M J, Nguyen-Minh T, Zhao L, et al.New low carbon Q&P steels containing film-like intercritical ferrite[J]. Mater. Sci. Eng., 2010, A527: 6429 | | [27] | Yen H W, Ooi S W, Eizadjou M, et al.Role of stress-assisted martensite in the design of strong ultrafine-grained duplex steels[J]. Acta Mater., 2015, 82: 100 |
|
|