| 热输入量对一种新型药芯焊丝熔敷金属组织及冲击韧性的影响* |
宋峰雨1,李艳梅2,王平1( ),朱伏先2 |
1 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819。 2 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819。 |
|
| EFFECTS OF HEAT INPUT ON THE MICROSTRUC-TURE AND IMPACT TOUGHNESS OF WELD METAL PROCESSED BY A NEW FLUXNOVEL FLUX CORED WIRE WELD |
Fengyu SONG1,Yanmei LI2,Ping WANG1( ),Fuxian ZHU2 |
1 Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819, China. 2 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China. |
引用本文:
宋峰雨,李艳梅,王平,朱伏先. 热输入量对一种新型药芯焊丝熔敷金属组织及冲击韧性的影响*[J]. 金属学报, 2016, 52(7): 890-896.
Fengyu SONG,
Yanmei LI,
Ping WANG,
Fuxian ZHU.
EFFECTS OF HEAT INPUT ON THE MICROSTRUC-TURE AND IMPACT TOUGHNESS OF WELD METAL PROCESSED BY A NEW FLUXNOVEL FLUX CORED WIRE WELD[J]. Acta Metall Sin, 2016, 52(7): 890-896.
| [1] | Yu S F, Yang K, Lei Y, Yang H.Trans China Weld Inst, 2008; 29(3): 17 | | [1] | (余圣甫, 杨可, 雷毅, 杨华. 焊接学报, 2008; 29(3): 17) | | [2] | Chai F, Su H, Yang C F, Luo X B.Trans China Weld Inst, 2010; 31(12): 25 | | [2] | (柴锋, 苏航, 杨才福, 罗小兵. 焊接学报, 2010; 31(12): 25) | | [3] | Lee S, Kim B C, Lee D Y.Scr Metall, 1989; 23: 995 | | [4] | Wang G D. Steel Roll, 2010; 27(2): 1(王国栋. 轧钢, 2010; 27(2): 1) | | [5] | Xia D X, Shang C J, Sun W H, Hou D H, Chen Y.Trans China Weld Inst, 2011; 32(4): 83 | | [5] | (夏佃秀, 尚成嘉, 孙卫华, 侯东华, 陈晔. 焊接学报, 2011; 32(4): 83) | | [6] | Sun Z, Huang J H, Zhang H, Zhao X K, Li Q Q.Trans China Weld Inst, 2008; 29(3): 41 | | [6] | (孙占, 黄继华, 张华, 赵兴科, 李曲全. 焊接学报, 2008; 29(3): 41) | | [7] | Lee J L.Acta Metall Mater, 1994; 42: 3291 | | [8] | Tomita Y, Saito N, Tsuzuki T, Tokunaga Y, Okamoto K.ISIJ Int, 1994; 34: 829 | | [9] | Yang J H, Wang X Y, Liu G.Iron Steel, 2012; 47(2): 87 | | [9] | (杨景红, 王小燕, 刘刚. 钢铁, 2012; 47(2): 87) | | [10] | McPherson N A.Ironmaking Steelmaking, 2009; 36(3): 93 | | [11] | Hodnik P, Furst C, Pennerstorfer P, Lengauer H.Stahl Eisen, 2008; 128(10): 35 | | [12] | Weng Y Q, Kang Y L.Iron Steel, 2010; 45(9): 1 | | [13] | Xia W Y, Yang C F, Su H, Chai F, Yong Q L.Iron Steel, 2011; 46(4): 76 | | [13] | (夏文勇, 杨才福, 苏航, 柴锋, 雍岐龙. 钢铁, 2011; 46(4): 76) | | [14] | Alogab K A, Matlock D K, Speer J G, Kleebe H J.ISIJ Int, 2007; 47: 1034 | | [15] | Lee J L, Pan Y T.Mater Sci Eng, 1991; A136: 109 | | [16] | Yamashita T, Shimamura J, Oi K, Nagoshi M, Oikawa K, Ishida K.Tetsu Hagané, 2014; 100: 397 | | [16] | (山下孝子, 嶋村純二, 大井健次, 名越正泰, 及川勝成, 石田清仁.鉄と鋼, 2014; 100: 397) | | [17] | Terada Y, Tamehiro H, Chijiiwa R.Tetsu Hagané, 2004; 90: 812 | | [17] | (寺田好男, 為広博,千々岩力男. 鉄と鋼, 2004; 90: 812) | | [18] | Omiya Y, Nako H, OkazakiY, Hatano H.J Jpn Weld Soc, 2012; 81(1): 16 | | [18] | (大宮良信, 名古秀徳, 岡崎喜臣, 畑野. 溶接学会誌, 2012; 81(1): 16) | | [19] | Zhang P Y, Gao C R, Zhu F X.Acta Metall Sin, 2012; 48: 264 | | [19] | (张朋彦, 高彩茹, 朱伏先. 金属学报, 2012; 48: 264) | | [20] | Zhang P Y, Yan J J, Gao C R, Zhu F X. Iron Steel, 2012; 47(11): 79 | | [20] | (张朋彦, 燕际军, 高彩茹, 朱伏先. 钢铁, 2012; 47(11): 79) | | [21] | Zhang P Y.PhD Dissertation, Northeastern University, Shenyang, 2011 | | [21] | (张朋彦. 东北大学博士学位论文, 沈阳, 2011) | | [22] | Song F Y, Zhang P Y, Wang P, Zhu F X. China Metall, 2015; 25(12): 7 | | [22] | (宋峰雨, 张朋彦, 王平, 朱伏先. 中国冶金, 2015; 25(12): 7) | | [23] | Horigome T, Tsunetomi E, Shinmyo K, Nagano K, Mori N, Kato T.J Jpn Weld Soc, 1978; 47(1): 18 | | [23] | (堀籠健男, 常富栄一, 新名恭三, 永野恭一, 森直道, 加藤隆司. 溶接学会誌, 1978; 47(1): 18) | | [24] | Ricks R A, Howell P R, Barritte G S.J Mater Sci, 1982; 17: 732 | | [25] | Rees G I, Bhadeshia H K D H.Mater Sci Technol, 1994; 10: 353 |
|
|