| 梯度NiCoCrAlYSi涂层的循环氧化及热腐蚀行为* |
彭新1,2,姜肃猛3,孙旭东1( ),宫骏3,孙超3 |
1 材料各向异性与织构教育部重点实验室, 东北大学材料科学与工程学院, 沈阳 110819
2 中航工业沈阳黎明航空发动机(集团)有限责任公司, 沈阳 110043
3 中国科学院金属研究所, 沈阳 110016 |
|
| CYCLIC OXIDATION AND HOT CORROSION BEHAVIORS OF A GRADIENT NiCoCrAlYSi COATING |
Xin PENG1,2,Sumeng JIANG3,Xudong SUN1( ),Jun GONG3,Chao SUN3 |
1 Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
2 AVIC Shenyang Liming Aero-engine (Group) Corporation Ltd., Shenyang 110043, China
3 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
彭新, 姜肃猛, 孙旭东, 宫骏, 孙超. 梯度NiCoCrAlYSi涂层的循环氧化及热腐蚀行为*[J]. 金属学报, 2016, 52(5): 625-631.
Xin PENG,
Sumeng JIANG,
Xudong SUN,
Jun GONG,
Chao SUN.
CYCLIC OXIDATION AND HOT CORROSION BEHAVIORS OF A GRADIENT NiCoCrAlYSi COATING[J]. Acta Metall Sin, 2016, 52(5): 625-631.
| [1] | Li M H, Sun X F, Li J G, Zhang Z Y, Jin T, Guan H R, Hu Z Q.Oxid Met, 2003; 59: 591 | | [2] | Nicholls J R, Stephenson D J.Met Mater, 1991; 7: 156 | | [3] | Goward G W.Surf Coat Technol, 1998; 68: 73 | | [4] | Meetham G W.Mater Sci Technol, 1986; 2: 290 | | [5] | Salam S, Hou P Y, Zhang Y D, Wang H F, Zhang C, Yang Z G.Corros Sci, 2015; 95:143 | | [6] | Srinivasan V, Cheruvu N S, Carr T J, Obrien C M.Mater Manuf Process, 1995; 10: 955 | | [7] | Lee E Y, Chartier D M, Biederman R R, Sisson R D.Surf Coat Technol, 1987; 32: 19 | | [8] | Tang F, Ajdelsztajn L, Schoenung J M.Oxid Met, 2004; 61: 219 | | [9] | Padture N P, Gell M, Jordan E H.Science, 2002; 296: 280 | | [10] | Nicholls J R, Simms N J, Chan W Y, Evans H E.Surf Coat Technol, 2002; 149: 236 | | [11] | Guo M H, Wang Q M, Gong J, Sun C, Huang R F, Wen L S.Corros Sci, 2006; 48: 2750 | | [12] | Jiang S M, Peng X, Bao Z B, Liu S C, Wang Q M, Gong J, Sun C.Corros Sci, 2008; 50: 3213 | | [13] | Wang W X, Jiang S M, Wei G Z, Ma J, Gong J, Sun C.Acta Metall Sin, 2011; 47: 578 | | [13] | (王维新, 姜肃猛, 卫广智, 马军, 宫骏, 孙超. 金属学报, 2011; 47: 578) | | [14] | Yu D Q, Lu X Y, Ma J, Jiang S M, Liu S C, Gong J, Sun C.Acta Metall Sin, 2012; 48: 759 | | [14] | (于大千, 卢旭阳, 马军, 姜肃猛, 刘山川, 宫骏, 孙超. 金属学报, 2012; 48: 759) | | [15] | Xu C Z, Jiang S M, Ma J, Gong J, Sun C.Acta Metall Sin, 2009; 45: 964 | | [15] | (徐朝政, 姜肃猛, 马军, 宫骏, 孙超. 金属学报, 2009; 45: 964) | | [16] | Xu C Z, Jiang S M, Bao Z B, Gong J, Sun C.Corros Sci, 2009; 51: 1467 | | [17] | Gleeson B, Cheung W H, Dacosta W, Young D J.Oxid Met, 1992; 38: 407 | | [18] | Felix P.Deposition and Corrosion in Gas Turbines. London: Applied Science Publish, 1972: 331 | | [19] | Lindblad N R.Oxid Met, 1969; 1: 143 | | [20] | Merchant S M, Notis M R.Mater Sci Eng, 1984; A66: 47 | | [21] | Hancock P.Mater Sci Technol, 1987; 3: 536 | | [22] | Eliaz N, Shemesh G, Latanision R M.Eng Fail Anal, 2002; 9: 31 | | [23] | Rapp R A.Corros Sci, 2002; 44: 209 | | [24] | McKee D W, Shore D A, Lurthra K L.J Electrochem Soc, 1978; 125: 411 | | [25] | Gurrappa I.Oxid Met, 1999; 51: 353 | | [26] | Tsaur C C, Roch J C, Chang Y Y.Mater Chem Phys, 2005; 91: 330 | | [27] | Hossain M K, Saunders S R J.Oxid Met, 1978; 12: 1 | | [28] | Deb D, Iyer S R, Radhakrishnan V M.Mater Lett, 1996; 29: 19 |
|
|