| 基于Thermo-Calc和微观偏析统一模型对Al-6.32Cu-25.13Mg合金凝固路径的预测* |
闫二虎1,2( ),孙立贤1,徐芬1,徐达鸣2 |
1 桂林电子科技大学材料科学与工程学院, 桂林 541004 2 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001 |
|
| PREDICTION OF THE SOLIDIFICATION PATH OF Al-6.32Cu-25.13Mg ALLOY BY A UNIFIED MICROSEGREGATION MODEL COUPLED WITH THERMO-CALC |
Erhu YAN1,2( ),Lixian SUN1,Fen XU1,Daming XU2 |
1 School of Materials Science and Engineering, Guilin University of Electronic Technology, Guilin 541004, China 2 School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China |
引用本文:
闫二虎,孙立贤,徐芬,徐达鸣. 基于Thermo-Calc和微观偏析统一模型对Al-6.32Cu-25.13Mg合金凝固路径的预测*[J]. 金属学报, 2016, 52(5): 632-640.
Erhu YAN,
Lixian SUN,
Fen XU,
Daming XU.
PREDICTION OF THE SOLIDIFICATION PATH OF Al-6.32Cu-25.13Mg ALLOY BY A UNIFIED MICROSEGREGATION MODEL COUPLED WITH THERMO-CALC[J]. Acta Metall Sin, 2016, 52(5): 632-640.
| [1] | Djordje M, Joachim G, Rainer S F.Acta Mater, 2008; 56: 5214 | | [2] | Dou K, Qing J S, Wang L, Zhang X F, Wang B, Liu Q, Dong H B.Acta Metall Sin, 2014; 50: 1505 | | [2] | (窦坤, 卿家胜, 王雷, 张晓峰, 王宝, 刘青, 董洪标. 金属学报, 2014; 50: 1505) | | [3] | Wang N, Li C R, Du Z M.Acta Metall Sin, 2008; 44: 1111 | | [3] | (王娜, 李长荣, 杜振民. 金属学报, 2008; 44: 1111) | | [4] | Zhang W B, Sha C S, Du Y, Wen G H, Xie W, Wang S Q.Acta Metall Sin, 2011; 47: 1307 | | [4] | (张伟彬, 沙春生, 杜勇, 温光华, 谢文, 王社权. 金属学报, 2011; 47: 1307) | | [5] | Mehrabian R, Flemings M C.Metall Trans, 1970; 1B: 455 | | [6] | Gao Q N, Wang J, Shang S L, Liu S H, Du Y, Liu Z.Calphad, 2014; 47: 196 | | [7] | Feng H, Zhang M, Chen H M, Liang J L, Tao X M, Ouyang Y H, Du Y.J Phase Equilib Diff, 2014; 35: 256 | | [8] | Chen F Y, Jie W Q.Acta Metall Sin, 2003; 39: 597 | | [8] | (陈福义, 介万奇. 金属学报, 2003; 39: 597) | | [9] | Yoo H, Kim C J.Int J Heat Mass Transfer, 1998; 30: 3268 | | [10] | Roósz A, Exner H E.Acta Matall Mater, 1990; 38: 375 | | [11] | Xie F Y, Kraft T, Zuo Y, Moon C H, Chang Y A.Acta Metall Sin (Engl Lett), 1999; 2: 489 | | [12] | Kraft T, Rettenmayr M, Exner H E.Modell Simul Mater Sci Eng, 1996; 4: 161 | | [13] | Zhao G W, Xu D M, Fu H Z.Int J Mater Res, 2008; 99: 680 | | [14] | Brooks J A, Baskes M I, Greulich F A.Metall Trans, 1991; 22A: 915 | | [15] | Flemings M C, Brody H D.Trans Metall Soc AIME, 1966; 236: 615 | | [16] | Clyne T W, Kurz W.Metall Trans, 1981; 12A: 965 | | [17] | Ohnaka I.Trans Iron Steel Inst Jpn, 1986; 26:1045 | | [18] | Kobayashi S.Trans Iron Steel Inst Jpn, 1988; 28: 728 | | [19] | Nastac L, Stefanescu D M.Metall Trans, 1993; 24A: 2107 | | [20] | Larouche D.Calphad, 2007; 31: 490 | | [21] | Du Q, Eskin D G, Katgerman L.Calphad, 2008; 32: 478 | | [22] | Hao D, Hu B, Zhang K, Zhang L J, Du Y.J Mater Sci, 2014; 49: 1157 | | [23] | Chen F Y, Jie W Q.Acta Metall Sin, 2004; 40: 664 | | [23] | (陈福义, 介万奇. 金属学报, 2004; 40: 664) | | [24] | Zhao G W, Li X Z, Xu D M, Guo J J, Du Y, He Y H.Calphad, 2012; 36: 155 | | [25] | Buhler T, Fries S G, Spencer P J, Lukas H L.J Phase Equilib, 1998; 19: 317 | | [26] | Xu D M.Metall Mater Trans, 2001; 32B: 1129 | | [27] | Yan E H, Li X Z, Rettenmayr M, Liu D M, Su Y Q, Guo J J, Xu D M, Fu H Z.Int J Hydrogen Energy, 2014; 39: 3505 | | [28] | Xu D M.Metall Mater Trans, 2002; 33B: 451 | | [29] | Xu D M, Fu H Z, Guo J J, Jia J, Li Q C.J Harbin Inst Technol, 2003; 35: 1156 | | [29] | (徐达鸣, 傅恒志, 郭景杰, 贾钧, 李庆春. 哈尔滨工业大学学报, 2003; 35:1156) | | [30] | Zhao G W, Xu D M, Song M H, Fu H Z, Du Y, He Y H.Acta Metall Sin, 2009; 45: 956 | | [30] | (赵光伟, 徐达鸣, 宋梦华, 傅恒志, 杜勇, 贺跃辉. 金属学报, 2009; 45: 956) | | [31] | Wang Z, Wang F Z, He Y H, Wang X, Ma S, Wang H M.Acta Metall Sin, 2014; 50: 1393 | | [31] | (王哲, 王发展, 何银花, 王欣, 马姗, 王辉绵. 金属学报, 2014; 50: 1393) | | [32] | Nishida Y, Aiga F, Itoh S.J Cryst Growth, 2014; 405: 110 | | [33] | Flemings M C. Solidification Processing.New York: McGraw-Hill Book Co NY, 1974: 134 | | [34] | Kurz W, Fisher D J.Fundamentals of Solidification. Lausanne, Switzerland: Trans Tech Publications, 1989: 68 | | [35] | Singh S N, Bardes B P, Flemings M C.Metall Trans, 1970; 1: 1383 |
|
|