| 电子束功率对TC4合金刚性拘束热自压连接、接头组织和力学性能的影响 |
邓云华1,2,关桥1,2( ),陶军2,吴冰2,王西昌2 |
| 2 北京航空制造工程研究所, 北京 100024 |
|
| EFFECT OF ELECTRON BEAM POWER ON TC4 ALLOY RIGID RESTRAINT THERMAL SELF-COMPRESSING BONDING, MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF JOINTS |
Yunhua DENG1,2,Qiao GUAN1,2( ),Jun TAO2,Bing WU2,Xichang WANG2 |
1 School of Mechanical Engineering and Automation, Beihang University, Beijing 100191 2 Beijing Aeronautical Manufacturing Technology Research Institute, Beijing 100024 |
引用本文:
邓云华,关桥,陶军,吴冰,王西昌. 电子束功率对TC4合金刚性拘束热自压连接、接头组织和力学性能的影响[J]. 金属学报, 2015, 51(9): 1111-1120.
Yunhua DENG,
Qiao GUAN,
Jun TAO,
Bing WU,
Xichang WANG.
EFFECT OF ELECTRON BEAM POWER ON TC4 ALLOY RIGID RESTRAINT THERMAL SELF-COMPRESSING BONDING, MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF JOINTS[J]. Acta Metall Sin, 2015, 51(9): 1111-1120.
| [1] | Kou S. Welding Metallurgy. 2nd Ed., New Jersey: John Wiley & Sons, 2003: 170 | | [2] | Kou S. JOM, 2003; 55(6): 37 | | [3] | Liu J, Gao X L, Zhang L J, Zhang J X. J Mater Eng Perform, 2014; 20: 319 | | [4] | Milella P P. Fatigue and Corrosion in Metals. Milan: Springer-Verlag, 2013: 625 | | [5] | Deng Y H, Guan Q, Wu B, Wang X C, Tao J. Mater Lett, 2014; 129: 43 | | [6] | Deng Y H, Guan Q. Mater Lett, 2015; 146: 1 | | [7] | China Aeronautical Materials Handbook Edit Committee. China Aeronautical Materials Handbook. Vol.4, Beijing: China Standard Publishing Company, 2002: 9 (中国航空材料手册编委会. 航空材料手册. 第四卷, 北京: 中国标准出版社, 2002: 9) | | [8] | Каракоэов Э С,translated by Zhai S F. Diffusion Bonding of Titanium Alloy. Beijing: National Defense Industry Press, 1986: 36 (Каракоэов Э С著,翟书汾译. 钛合金的扩散焊接. 北京: 国防工业出版社, 1986: 36) | | [9] | Wu G Q, Li Z F, Luo G X, Li H Y, Huang Z. Mater Sci Eng, 2007; A452-453: 529 | | [10] | Liu H, Nakata K, Zhang J X, Yamamoto N, Liao J. Mater Charact, 2012; 65: 1 | | [11] | Mills K C. Recommended Values of Thermophysical Properties for Selected Commercial Alloys. London: Woodhead Publishing Ltd, 2002: 217 | | [12] | Lacki P, Adamus K. Comput Struct, 2011; 89: 977 | | [13] | Luo Y, Liu J H, Ye H. Vacuum, 2010; 84: 857 | | [14] | Rouquette S, Guo J, Le P. Int J Therm Sci, 2007; 46: 128 | | [15] | Liu C, Wu B, Zhang J X. Metall Mater Trans, 2010; 41B: 1129 | | [16] | Lacki P, Adamus K, Wieczorek P. Comput Mater Sci, 2014; 94: 17 | | [17] | Cai Y. Master Thesis, Nanjing University of Aeronautics and Astronautics, 2009 (蔡 云. 南京航空航天大学硕士学位论文, 2009) | | [18] | Guan Q, Cao Y. Weld World, 1999; 43(1): 14 | | [19] | Li J. PhD Dissertation, Beijing University of Technology, 2004 (李 菊. 北京工业大学博士学位论文, 2004) | | [20] | Ma R F, Li M Q, Li H. Sci China Technol Sci, 2012; 55: 2420 | | [21] | Shen J J. Master Thesis, Harbin Institute of Technology, 2007 (沈俊军. 哈尔滨工业大学硕士学位论文, 2007) | | [22] | Hill A, Wallach E R. Acta Meter, 1989; 19: 2425 | | [23] | Orhan N, Aksoy M, Eroglu M. Mater Sci Eng, 1999; A271: 458 | | [24] | Mehrer H.Diffusion in Solids: Fundamentals, Methods, Materials, Diffusion-Controlled Process. Berlin: Springer and Verlag, 2007: 310 | | [25] | Zhang Z,Wang Q J,Mo W. Metallurgy and Heat Treatment of Titanium. Beijing: Metallurgical Industry Press, 2009: 87 (张 翥,王群骄,莫 畏. 钛的金属学和热处理. 北京: 冶金工业出版社, 2009: 87) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|