| Fe-3%Si电工钢铸坯柱状晶织构的演变规律* |
付勇军1,2,杨平1( ),蒋奇武2,王晓达2,金文旭2 |
1 北京科技大学材料科学与工程学院, 北京 100083 2 鞍钢股份有限公司冷轧硅钢厂, 鞍山 114021 |
|
| EVOLUTION OF TEXTURES OF COLUMNAR GRAINS IN Fe-3%Si ELECTRICAL STEEL SLABS |
Yongjun FU1,2,Ping YANG1( ),Qiwu JIANG2,Xiaoda WANG2,Wenxu JIN2 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
2 Cold Rolling Silicon Plant, Anshan Steel Co., Ltd., Anshan 114021 |
引用本文:
付勇军, 杨平, 蒋奇武, 王晓达, 金文旭. Fe-3%Si电工钢铸坯柱状晶织构的演变规律*[J]. 金属学报, 2015, 51(5): 545-552.
Yongjun FU,
Ping YANG,
Qiwu JIANG,
Xiaoda WANG,
Wenxu JIN.
EVOLUTION OF TEXTURES OF COLUMNAR GRAINS IN Fe-3%Si ELECTRICAL STEEL SLABS[J]. Acta Metall Sin, 2015, 51(5): 545-552.
| [1] | Walter J L, Hibbard W R. Trans Met Soc AIME, 1958; 212: 731 | | [2] | Park J Y, Han K S, Woo J S, Chang S K, Rajmohan N, Szpunar J A. Acta Mater, 2002; 50: 1825 | | [3] | Sakai T, Shiozaki M, Takashina K. J Appl Phys, 1979; 50: 2369 | | [4] | Obara T, Takeuchi H, Takamiya T, Kan T. J Mater Eng Perform, 1993; 2: 205 | | [5] | Takashima M, Obara T, Kan T. J Mater Eng Perform, 1993; 2: 249 | | [6] | Dong H, Zhao Y, Yu X J, Lian F Z. J Iron Steel Res Int, 2009; 16: 86 | | [7] | Littmann M F. Metall Trans, 1975; 6A: 1041 | | [8] | Liu H T, Liu Z Y, Cao G M, Li C G, Wang G D. J Magn Magn Mater, 2011; 323: 2648 | | [9] | Cheng L, Yang P, Fang Y P, Mao W M. J Magn Magn Mater, 2012; 324: 4068 | | [10] | Heo N H, Chai K H, Na J G. Acta Mater, 2000; 48: 2901 | | [11] | Park H K, Kim S J, Han H N, Han C H, Hwang N M. Mater Trans, 2010; 51: 1547 | | [12] | Xiang L, Yue E B, Fan D D, Qiu S T, Zhao P. J Iron Steel Res Int, 2008; 15: 88 | | [13] | Park J T, Szpunar J A. Acta Mater, 2003; 51: 3037 | | [14] | Li C S, Yang H, Wang Y F, Yu Y M. J Iron Steel Res Int, 2010; 17: 46 | | [15] | Park S Y, Lim K M, Namkung J, Kim M C, Park C G. Scr Mater, 2006; 54: 621 | | [16] | Zhang N, Yang P, Mao W M. Acta Metall Sin, 2012; 48 : 784 (张 宁, 杨 平, 毛卫民. 金属学报, 2012; 48 : 784) | | [17] | Zhang N, Yang P, Mao W M. Acta Metall Sin, 2012; 48: 308 (张 宁, 杨 平, 毛卫民. 金属学报, 2012; 48: 308) | | [18] | Shao Y Y, Yang P, Mao W M. Acta Metall Sin, 2014; 50: 259 (邵媛媛, 杨 平, 毛卫民. 金属学报, 2014; 50: 259) | | [19] | Walter J L, Koch E F. Acta Metall, 1963; 11: 923 | | [20] | Walter J L, Koch E F. Acta Metall, 1962; 10: 1059 | | [21] | Dunn C G. Acta Met, 1954; 2: 173 |
|
|