Mn含量对Fe-Mn-Si-Cr-Ni合金记忆效应的影响机制* |
张成燕1, 宋帆1, 王珊玲2, 彭华备1, 文玉华1( ) |
1 四川大学制造科学与工程学院, 成都 610065 2 四川大学分析测试中心, 成都 610065 |
|
EFFECT MECHANISM OF Mn CONTENTS ON SHAPE MEMORY OF Fe-Mn-Si-Cr-Ni ALLOYS |
ZHANG Chengyan1, SONG Fan1, WANG Shanling2, PENG Huabei1, WEN Yuhua1( ) |
1 College of Manufacturing Science and Engineering, Sichuan University, Chengdu 610065 2 Analytical and Testing Center, Sichuan University, Chengdu 610065 |
引用本文:
张成燕, 宋帆, 王珊玲, 彭华备, 文玉华. Mn含量对Fe-Mn-Si-Cr-Ni合金记忆效应的影响机制*[J]. 金属学报, 2015, 51(2): 201-208.
Chengyan ZHANG,
Fan SONG,
Shanling WANG,
Huabei PENG,
Yuhua WEN.
EFFECT MECHANISM OF Mn CONTENTS ON SHAPE MEMORY OF Fe-Mn-Si-Cr-Ni ALLOYS[J]. Acta Metall Sin, 2015, 51(2): 201-208.
[1] |
Sato A, Suaga Y, Tori T. Acta Metall, 1977; 25: 627
|
[2] |
Sato A, Chishima E, Soma K, Mori T. Acta Metall, 1982; 30: 1177
|
[3] |
Nishimura F, Watanabe N, Tanaka K. Mater Sci Eng, 1998; A247:275
|
[4] |
Andrade M S, Osthues R M, Arruda G J. Mater Sci Eng, 1999; A273: 512
|
[5] |
Bliznuk V V, Gavriljuk V G, Kopitsa G P, Grigoriev S V, Runov V V. Acta Mater, 2004; 52: 4791
|
[6] |
Stanford N, Dune D P. Mater Sci Eng, 2007; A454: 407
|
[7] |
Jiang B H, Qu X, Zhou W M, Xi Z L, Hsu T Y. Scr Mater Metall, 1996; 34: 1437
|
[8] |
Gavriljuk V G, BliznukV V, Shanina B D, Kolesnik S P. Mater Sci Eng, 2005; A406: 1
|
[9] |
Wang D F, Chen Y R, Gong F Y, Liu D Z, Liu W X. J Phys IV, 1995; 05: 527
|
[10] |
Stanford N, Dunne D P. Mater Sci Eng, 2006; A422: 352
|
[11] |
Baruj A, Kikuchi T, Kajiwara S, Shinya N. Mater Sci Eng, 2004; A378: 333
|
[12] |
Koyama M, Sawaguchi T, Tsuzaki K. Mater Sci Eng, 2011; A528: 2882
|
[13] |
Koyama M, Sawaguchi T, Ogawa K, Kikuchi T, Murakami M. Mater Sci Eng, 2008; A497: 353
|
[14] |
Rong L J, Li Y Y, Shi C X. Acta Metall Sin,1995; 31: 125
|
[14] |
(戎利建, 李依依, 师昌绪. 金属学报, 1995; 31: 125)
|
[15] |
Stanford N, Dunne D P. Mater Sci Eng, 2007; A454-455: 407
|
[16] |
Wen Y H, Peng H B, Wang C P, Yu Q X. Li N. Adv Eng Mater, 2011; 13: 1
|
[17] |
Otsuka H, Yamada H, Maruyama T, Tanahahi H, Matsua S, Murakam M. ISIJ Int, 1990; 30: 674
|
[18] |
Inagaki H, Inoue K. Z Metall, 1994; 85: 790
|
[19] |
Federzoni L, Guénin G. Scr Mater Metall, 1994; 31: 25
|
[20] |
Stanford N, Chen K, Dunne D P, Jin X J. ISIJ Int, 2007; 47: 883
|
[21] |
Stanford N, Dunne D P. J Mater Sci, 2006; 41: 4883
|
[22] |
Lee T H, Ha H Y, Kang J Y, Moon J, Lee C H, Park S J. Acta Mater, 2013; 61: 7399
|
[23] |
Olson G B, Cohen M. J Less-Common Met, 1972; 28: 107
|
[24] |
Caenegem N V, Duprez L, Verbeken K, Cooman B C, Houbaert Y, Segers D. ISIJ Int, 2007; 47: 723
|
[25] |
Stanford N, Dunne D P. Acta Mater, 2010; 58: 6752
|
[26] |
Tomota Y, Nakagawara W, Tsuzaki K, Maki T. Scr Mater Metall, 1992; 26: 1571
|
[27] |
Kajiwara S. Mater Sci Eng, 1999; A273-275: 67
|
[28] |
Bergeon N, Guenin G, Esnouf C. Mater Sci Eng, 1998; A242: 87
|
[29] |
Matsumoto S, Sato A, Mori T. Acta Metall Mater, 1994; 42: 1207
|
[30] |
Yang J H, Wayman C M. Metall Trans, 1992; 23A: 1445
|
[31] |
Caenegem N V, Duprez L, Verbken K, Cooman B C D, Houbaert Y, Segrs D. ISIJ Int, 2007; 47: 723
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|