| 中间层金属对Al2O3/1Cr18Ni9Ti钎焊接头组织及剪切强度的影响* |
刘毅1,2( ), 江国锋2, 许昆1, 罗锡明1, 陈登权1, 李伟1 |
1 贵研铂业股份有限公司, 昆明 650106 2 昆明贵金属研究所, 昆明 650106 |
|
| EFFECT OF INTERLAYERS ON THE MICROSTRUC-TURE AND SHEAR STRENGTH OF ALUMINA CERAMIC AND 1Cr18Ni9Ti STAINLESS STEEL BRAZED BONDING |
LIU Yi1,2( ), JIANG Guofeng2, XU Kun1, LUO Ximing1, CHEN Dengquan1, LI Wei1 |
1 Sino-Platinum Metals Co. Ltd, Kunming 650106 2 Kunming Institute of Precious Metals, Kunming 650106 |
引用本文:
刘毅, 江国锋, 许昆, 罗锡明, 陈登权, 李伟. 中间层金属对Al2O3/1Cr18Ni9Ti钎焊接头组织及剪切强度的影响*[J]. 金属学报, 2015, 51(2): 209-215.
Yi LIU,
Guofeng JIANG,
Kun XU,
Ximing LUO,
Dengquan CHEN,
Wei LI.
EFFECT OF INTERLAYERS ON THE MICROSTRUC-TURE AND SHEAR STRENGTH OF ALUMINA CERAMIC AND 1Cr18Ni9Ti STAINLESS STEEL BRAZED BONDING[J]. Acta Metall Sin, 2015, 51(2): 209-215.
| [1] |
Nicholas M G. Joining of Ceramics. London: Chapman and Hall Ltd, 1990: 1
|
| [2] |
Schwartz M M. Ceramic Joining. Material park, Ohio: ASM International, 1990: 1
|
| [3] |
Park J W, Mendez P F, Eagar T W. Acta Mater, 2002; 50: 883
|
| [4] |
Zhang J X, Chandel R S, Chen Y Z, Seow H P. J Mater Process Technol, 2002; 122: 220
|
| [5] |
Li Z R, Fan J X, Feng J C. Aerosp Mater Technol, 2008; (4): 6
|
| [5] |
(李卓然, 樊建新, 冯吉才. 宇航材料工艺, 2008; (4): 6)
|
| [6] |
Xian A P, Si C Y. J Mater Sci, 1992; 27: 1560
|
| [7] |
Huang X L, Lin S, Xiao J M. Trans China Weld Inst, 1998; 19: 216
|
| [7] |
(黄小丽, 林 实, 肖纪美. 焊接学报, 1998; 19: 216)
|
| [8] |
Huang X L, Lin S, Xiao J M, Chu J X. Mater Sci Eng, 1996; 14(3): 58
|
| [8] |
(黄小丽, 林 实, 肖纪美, 楚建新. 材料科学与工程, 1996; 14(3): 58)
|
| [9] |
Zou G S, Ren J L, Wu A P, Peng Z S, Zeng W J. Mater Rev, 1999; 13(2): 16
|
| [9] |
(邹贵生, 任家烈, 吴爱萍, 彭真山, 曾文军. 材料导报, 1999; 13(2): 16)
|
| [10] |
Xian A P, Si C Y. Acta Metall Sin, 1991; 27: 421
|
| [10] |
(冼爱平, 斯重遥. 金属学报, 1991; 27: 421)
|
| [11] |
Zhou Y, Bao F H, Ren J L, North T H. Mater Sci Technol, 1991; 7: 863
|
| [12] |
Wang Y, He P, Feng J C, Zhang L X, Gu X L, Wang D Y. Trans Chin Weld Inst, 2007; 28(4): 13
|
| [12] |
(王 颖, 何 鹏, 冯吉才, 张丽霞, 顾小龙, 王大勇. 焊接学报, 2007; 28(4): 13)
|
| [13] |
Suganuma K, Okamoto T, Koizumi M, Kamachi K. J Mater Sci,1987; 22: 3561
|
| [14] |
Suganuma K. J Mater Sci, 1991; 26: 6144
|
| [15] |
Zhu M U, Chung D D L. J Mater Sci, 1997; 32: 5321
|
| [16] |
Shirzadi A A, Zhu Y, Bhadeshia H K D H. Mater Sci Eng, 2008; A496: 501
|
| [17] |
Tang Q, Chu J X, Zhang X Y. Electros Proc Technol, 2001; 22: 166
|
| [17] |
(唐 群, 楚建新, 张晓勇. 电子工艺技术, 2001; 22: 166)
|
| [18] |
Hao H Q, Wang Y L, Jin Z H, Wang X T. J Mater Sci, 1995; 30: 4107
|
| [19] |
Zou X. Brazing. Beijing: China Machine Press, 1997: 392
|
| [19] |
(邹 僖. 钎焊. 北京: 机械工业出版社, 1997: 392)
|
| [20] |
Valette C, Devismes M F, Voytovych R, Eustathopoulos N. Scr Mater, 2005; 52: 1
|
| [21] |
Arróyave R, Eagar T W. Acta Mater, 2003; 51: 4871
|
| [22] |
Jocelyn L W. Master Thesis, Massachusetts Institute of Technology, Cambridge, USA, 2001
|
| [23] |
Torvund T, Grong Ø, Akselsen O M, UlvensØen J H. J Mater Sci, 1997; 32: 4437
|
| [24] |
Zhu D Y, Wang Y L, Jin Z H. Ordnance Mater Sci Eng, 1998; 21(20): 22
|
| [24] |
(朱定一, 王永兰, 金志浩. 兵器材料科学与工程, 1998; 21(20): 22)
|
| [25] |
Wang X Y, Li Y, Wei S Z, Xu L J, Ma X D. New Technol New Proc, 2010; (5): 85
|
| [25] |
(王新阳, 李 炎, 魏世忠, 徐流杰, 马向东. 新技术新工艺, 2010; (5): 85)
|
| [26] |
Li Z R, Fan J X, Feng J C. J Mater Eng, 2008; (9): 1
|
| [26] |
(李卓然, 樊建新, 冯吉才. 材料工程, 2008; (9): 1)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|