| 基于位错密度的Fe-22Mn-0.6C型TWIP钢物理本构模型研究 |
孙朝阳( ), 黄杰, 郭宁, 杨竞 |
| 北京科技大学机械工程学院, 北京 100083 |
|
| A PHYSICAL CONSTITUTIVE MODEL FOR Fe-22Mn-0.6C TWIP STEEL BASED ON DISLOCATION DENSITY |
SUN Chaoyang( ), HUANG Jie, GUO Ning, YANG Jing |
| School of Mechanical Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
孙朝阳, 黄杰, 郭宁, 杨竞. 基于位错密度的Fe-22Mn-0.6C型TWIP钢物理本构模型研究[J]. 金属学报, 2014, 50(9): 1115-1122.
Chaoyang SUN,
Jie HUANG,
Ning GUO,
Jing YANG.
A PHYSICAL CONSTITUTIVE MODEL FOR Fe-22Mn-0.6C TWIP STEEL BASED ON DISLOCATION DENSITY[J]. Acta Metall Sin, 2014, 50(9): 1115-1122.
| [1] |
Mi Z L, Tang D, Yan L, Guo J. J Mater Sci Technol, 2005; 21: 451
|
| [2] |
Grassel O, Kruger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391
|
| [3] |
Vercammen S, Blanpain B, De Cooman B C, Wollants P. Acta Mater, 2004; 52: 2005
|
| [4] |
Frommeyer G, Brux U, Neumann P. ISIJ Int, 2003; 43: 438
|
| [5] |
Bouaziz O. Scr Mater, 2012; 66: 982
|
| [6] |
Wang S H, Liu Z Y, Zhang W N, Wang G D. Acta Metall Sin, 2009; 45: 573
|
| [6] |
(王书晗, 刘振宇, 张维娜, 王国栋. 金属学报, 2009; 45: 573)
|
| [7] |
Renard K, Jacques P J. Mater Sci Eng, 2012; A542: 8
|
| [8] |
Bouaziz O, Allain S, Scott C P, Cugy P, Barbier D. Curr Opin Solid State Mater Sci, 2011; 15: 141
|
| [9] |
Gutierrez-Urrutia I, Raabe D. Acta Mater, 2011; 59: 6449
|
| [10] |
Yang P, Lu F Y, Meng L, Cui F E. Acta Metall Sin, 2010; 46: 657
|
| [10] |
(杨 平, 鲁法云, 孟 利, 崔凤娥. 金属学报, 2010; 46: 657)
|
| [11] |
Bouaziz O, Guelton N. Mater Sci Eng, 2001; A319: 246
|
| [12] |
Allain S, Chateau J P, Bouaziz O. Mater Sci Eng, 2004; A387: 143
|
| [13] |
Kim J, Estrin Y, Beladi H, Timokhina I, Chin K, Kim S, De Cooman B C. Metall Mater Trans, 2012; 43A: 479
|
| [14] |
Johnson G R, Cook W H. Eng Fract Mech, 1985; 21: 31
|
| [15] |
Zerilli F J, Armstrong R W. J Appl Phys, 1987; 61: 1816
|
| [16] |
Salem A A, Kalidindi S R, Doherty R D, Semiatin S L. Metall Mater Trans, 2006; 37A: 259
|
| [17] |
Salem A A, Kalidindi S R, Doherty R D. Acta Mater, 2003; 51: 4225
|
| [18] |
Yu Y, Pan X X, Xie R Z, Zhang F J, Hu W J. Chin J Theory Appl Mech, 2012; 44: 334
|
| [18] |
(余 勇, 潘晓霞, 谢若泽, 张方举, 胡文军. 力学学报, 2012; 44: 334)
|
| [19] |
Wu Z Q, Tang Z Y, Li H Y, Zhang H D. Acta Metall Sin, 2012; 48: 593
|
| [19] |
(吴志强, 唐正友, 李华英, 张海东. 金属学报, 2012; 48: 593)
|
| [20] |
Koyama M, Sawaguchi T, Lee T, Lee C S, Tsuzaki K. Mater Sci Eng, 2011; A528: 7310
|
| [21] |
Remy L. Acta Metall, 1978; 26: 443
|
| [22] |
Voyiadjis G Z, Abed F H. Mech Mater, 2005; 37: 355
|
| [23] |
Estrin Y, Mecking H. Acta Metall, 1984; 32: 57
|
| [24] |
Mecking H, Kocks U F. Acta Metall, 1981; 29: 1865
|
| [25] |
Ismael A M, Ahmed H, Johannes R. Mater Sci Eng, 2009; A504: 40
|
| [26] |
Allain S, Chateau J P, Bouaziz O, Migot S, Guelton N. Mater Sci Eng, 2004; A387-389: 246
|
| [27] |
Wang W H. Master Thesis, University of Science and Technology Beijing, 2012
|
| [27] |
(王伟华. 北京科技大学硕士学位论文, 2012)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|