Please wait a minute...
金属学报  2013, Vol. 49 Issue (11): 1325-1332    DOI: 10.3724/SP.J.1037.2013.00452
  论文 本期目录 | 过刊浏览 |
NiAl-2.5Ta-7.5Cr-1B合金的微观组织、力学性能与摩擦磨损特性
王振生1,2),张孟恩1),杨双双1),郭建亭3),周兰章3),陈志钢1)
1) 湖南科技大学先进矿山装备教育部工程研究中心, 湘潭 411201
2) 湖南科技大学高温耐磨材料及制备技术湖南省国防科技重点实验室, 湘潭 411201
3) 中国科学院金属研究所, 沈阳 110016
MICROSTRUCTURE, MECHANICAL, FRICTION AND WEAR PROPERTIES OF NiAl-2.5Ta-7.5Cr-1B ALLOY
WANG Zhensheng 1,2), ZHANG Meng'en 1), YANG Shuangshuang 1), GUO Jianting3), ZHOU Lanzhang3), CHEN Zhigang1)
1) Engineering Research Center of Advanced Mining Equipment, Ministry of Education,Hunan University of Science and Technology, Xiangtan 411201
2) High Temperature Wear Resistance Materials and Preparation Technology of Hunan Province,the National Defense Science and Technology Key Laboratory, Hunan University of Science and Technology, Xiangtan 411201
3) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
引用本文:

王振生,张孟恩,杨双双,郭建亭,周兰章,陈志钢. NiAl-2.5Ta-7.5Cr-1B合金的微观组织、力学性能与摩擦磨损特性[J]. 金属学报, 2013, 49(11): 1325-1332.
WANG Zhensheng, ZHANG Meng'en, YANG Shuangshuang, GUO Jianting, ZHOU Lanzhang, CHEN Zhigang. MICROSTRUCTURE, MECHANICAL, FRICTION AND WEAR PROPERTIES OF NiAl-2.5Ta-7.5Cr-1B ALLOY[J]. Acta Metall Sin, 2013, 49(11): 1325-1332.

全文: PDF(4108 KB)  
摘要: 

采用SEM和XRD分析了NiAl-2.5Ta-7.5Cr-1B合金的微观组织,采用万能力学试验机测试了合金的力学性能,采用高温摩擦磨损机研究了合金室温--600℃的摩擦磨损特性. 研究表明,NiAl-2.5Ta-7.5Cr-1B合金由NiAl相、NiAl-Cr共晶、Cr2Ta相、(Ta, Cr)3B2相和TaB相组成.B元素的添加使NiAl-2.5Ta-7.5Cr合金的塑性提高了50%. 从室温-600℃时,NiAl-2.5Ta-7.5Cr-1B合金表现出良好的自润滑耐磨损特性,其自润滑耐磨损特性来源于合金磨损表面存在固体Al4B2O9颗粒和液态B2O3,液态B2O3使摩擦磨损符合流体动压润滑机制,Al4B2O9颗粒起到支撑作用.

关键词 : NiAl-2.5Ta-7.5Cr-1B合金,  微观组织,  力学性能,  摩擦磨损特性    
Abstract:

  The microstructure and properties of NiAl-2.5Ta-7.5Cr-1B alloy are investigated in this work. The microstructure is analyzed by SEM and XRD, the mechanical properties are conducted by a universal mechanical testing machine and the friction and wear features from room temperature to 600℃ are mainly studied using an elevated temperature friction and wear machine. The experimental results show that the NiAl-2.5Ta-7.5Cr-1B alloy consists of NiAl, eutectic (NiAl-Cr), Cr2Ta, (Ta, Cr)3B2 and TaB. The addition of B into the NiAl-2.5Ta-7.5Cr alloy improves the plasticity by 50%. The NiAl-2.5Ta-7.5Cr-1B alloy exhibits excellent self-lubricating and wear-resistant properties from room temperature to 600℃ which could be mainly attributed to the co-existence of B2O3 liquid phase and Al4B2O9 solid particles on the worn surface. The B2O3 liquid phase makes the friction and wear process conform to the mechanism of hydrodynamic lubrication and the Al4B2O9 solid particles have a load-bearing function.

Key words: NiAl-2.5Ta-7.5Cr-1B alloy    microstructure    mechanical property    friction and wear property
收稿日期: 2013-07-27     
基金资助:

国家自然科学基金项目51101055和湖南省自然科学基金项目13JJ8015资助

作者简介: 王振生, 男, 1978年生, 副教授, 博士

[1] Guo J T. Ordered Intermetallic Compound NiAl Alloy. Beijing: Science Press, 2003: 58

(郭建亭. 有序金属间化合物镍铝合金. 北京: 科学出版社, 2003: 58)
[2] Noebe R D, Bowman R R, Nathal M V. Int Mater Rev, 1993; 38(4): 193
[3] Miracle D B. Acta Metall Mater, 1993; 41: 649
[4] Ball A, Smallman R E. Acta Metall Mater, 1966; 14: 1349
[5] Ball A, Smallman R E. Acta Metall Mater, 1966; 14: 1517
[6] Veyssiere P, Noebe R D. Philos Mag, 1992; 65: 1
[7] Bowman R R, Noebe R D, Raj S V, Locci I E. Metall Trans, 1992; 23A: 1493
[8] Nagpal P, Baker I. J Mater Lett, 1992; 11: 1209
[9] Cotton J D, Noebe R D, Kaufman M J. Intermetallics, 1993; 1: 117
[10] Liu Z G, Guo J T, Shi N L, Hu Z Q. J Mater Sci Technol, 1996; 12: 7
[11] Zhou J, Guo J T . Mater Sci Eng, 2003; A339: 167
[12] Hawk J A, Alman D E. J Mater Sci Technol, 1997; (spec issue): 239
[13] Hawk J A, Alman D E. Wear, 1999; (spec issue): 225
[14] Wang Z S, Guo J T, Zhou L Z, Xie Y, Sheng L Y, Hu Z Q. Chin J Mater Res, 2009; 23: 225
(王振生, 郭建亭, 周兰章, 谢 \ \ 亿, 盛立远, 胡壮麒. 材料研究学报, 2009; 23: 225)
[15] Wang Z S, Guo J T, Zhou L Z, Sheng L Y, Hu Z Q. Acta Metall Sin, 2009; 45: 297
(王振生, 郭建亭, 周兰章, 盛立远, 胡壮麒. 金属学报, 2009; 45: 297)
[16] Wang Z S, Zhou L Z, Guo J T, Sheng L Y, Hu Z Q. Tribology, 2008; 28: 497
(王振生, 周兰章, 郭建亭, 胡壮麒. 摩擦学学报, 2008; 28: 497)
[17] Guo J T, Wang Z S, Sheng L Y, Zhou L Z. Prog Nat Sci: Mater Int, 2012; 22: 414
[18] Wang Z S, Zhou L Z, Guo J T, Zhang G Y, Li H Q, Hu Z Q. Tribology, 2010; 30: 589
(王振生, 周兰章, 郭建亭, 张光业, 李会强, 胡壮麒. 摩擦学学报, 2010; 30: 589)
[19] Palma M, Preuhsb J, Sauthoff G. J Mater Process Technol, 2003; 136: 105
[20] Zeumer B, Sauthoff G. Intermetallic$s$, 1998: 6: 451
[21] Katsubiro N, Shingo S, Taku K, Soukich U. J Jpn Soc Powder Metall,1993; 40(1): 49
[22] Senda T, Yamamoto Y, Ochi Y J. Ceram Soc Jpn, 1993; 101: 461
[23] Archard J F. Wear, 1958/1959; 2: 438
[24] Bowden F P, Tabor D, translated by Chen S L, Yuan H C, Ding X J. The Friction and Lubrication of Solids.Beijing: China Machine Press, 1982: 74
(Bowden F P, Tabor D著, 陈绍澧, 袁汉昌, 丁雪加~译. 固体的摩擦与润滑. 北京: 机械工业出版社, 1982: 74)
[25] Shi M S. Solid Lubrication Technology. Beijing: China Petrochemical Press, 1998: 156

(石淼森. 固体润滑技术. 北京: 中国石化出版社, 1998: 156)

[1] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[5] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[6] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] 刘兴军, 魏振帮, 卢勇, 韩佳甲, 施荣沛, 王翠萍. 新型钴基与Nb-Si基高温合金扩散动力学研究进展[J]. 金属学报, 2023, 59(8): 969-985.
[9] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[10] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[11] 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
[12] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[13] 王长胜, 付华栋, 张洪涛, 谢建新. 冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响[J]. 金属学报, 2023, 59(5): 585-598.
[14] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[15] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.