| 对流条件下定向凝固包晶合金的相和微观组织选择 |
| 王灵水,沈军,商昭,王雷,傅恒志 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| PHASE AND MICROSTRUCTURE SELECTION IN DIRECTIONALLY SOLIDIFIED PERITECTIC ALLOYS UNDER CONVECTION CONDITION |
| WANG Lingshui, SHEN Jun, SHANG Zhao, WANG Lei, FU Hengzhi |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
王灵水,沈军,商昭,王雷,傅恒志. 对流条件下定向凝固包晶合金的相和微观组织选择[J]. 金属学报, 2013, 49(7): 822-830.
WANG Lingshui,
SHEN Jun,
SHANG Zhao,
WANG Lei,
FU Hengzhi.
PHASE AND MICROSTRUCTURE SELECTION IN DIRECTIONALLY SOLIDIFIED PERITECTIC ALLOYS UNDER CONVECTION CONDITION[J]. Acta Metall Sin, 2013, 49(7): 822-830.
| [1] Kerr H W, Kurz W. Int Mater Rev, 1996; 41: 129
[2] Asta M, Beckermann C, Karma A, Kurz W, Napolitano R, Plapp M, Purdy G,Rappaz M, Trivedi R. Acta Mater, 2009; 57: 941
[3] Boettinger W J, Coriell S R, Greer A L, Karma A, Kurz W, Rappaz M,Trivedi R. Acta Mater, 2000; 48: 43
[4] Boettinger W J. Metall Mater Trans, 1974; 5B: 2023
[5] Park J S, Trivedi R. J Cryst Growth, 1998; 187: 511
[6] Liu D M, Li X Z, Su Y Q, Luo L S, Zhang B, Guo J J, Fu H Z. Mater Lett, 2011; 65: 1628
[7] Luo L S, Su Y Q, Guo J J, Li X Z, Fu H Z. Sci China, 2007; 50G: 442
[8] Lo T S, Dobler S, Plapp M, Karma A, Kurz W. Acta Mater, 2003; 51: 599
[9] Trivedi R. Metall Mater Trans, 1995; 26A: 1583
[10] Hunziker O, Vandyoussefi M, Kurz W. Acta Mater, 1998; 46: 6325
[11] Li S M, Liu L, Li X L, Fu H Z. Acta Metall Sin, 2004; 40: 20
(李双明, 刘林, 李晓历, 傅恒志. 金属学报, 2004; 40: 20)
[12] Li X Z, Guo J J, Su Y Q, Wu S P, Fu H Z. Acta Metall Sin, 2005; 41: 593
(李新中, 郭景杰, 苏彦庆, 吴士平, 傅恒志. 金属学报, 2005; 41: 593)
[13] Guo J J, Li X Z, Su Y Q, Wu S P, Fu H Z. Acta Metall Sin, 2005; 41: 599
(郭景杰, 李新中, 苏彦庆, 吴士平, 傅恒志. 金属学报, 2005; 41: 599)
[14] Karma A, Rappel W J, Fuh B C, Trivedi R. Metall Mater Trans, 1998; 29A: 1457
[15] Mazumder P, Trivedi R. Phys Rev Lett, 2002; 88: 235507
[16] Luo L S, Zhang Y M, Su Y Q, Wang X, Guo J J, Fu H Z. Acta Metall Sin, 2011; 47: 275
(骆良顺, 张宇民, 苏彦庆, 王新, 郭景杰, 傅恒志. 金属学报, 2011; 47: 275)
[17] Luo L S, Fu H Z, Zhang Y M, Li X Z, Su Y Q, Guo J J. Acta Metall Sin, 2011; 47: 284
(骆良顺, 傅恒志, 张宇民, 李新中, 苏彦庆, 郭景杰. 金属学报, 2011; 47: 284)
[18] Nernst W. Z Phys Chem, 1904; 47: 52
[19] Burton J A, Prim R C, Schlichter W P. J Chem Phys, 1953; 21: 1987
[20] Bower T F, Brody H D, Flemings M C. Trans Metall Soc AIME, 1966; 236: 624
[21] Wang L, Shen J, Qin L, Feng Z, Wang L, Fu H. J Cryst Growth, 2012; 356: 26
[22] Yasuda H, Notake N, Tokieda K, Ohnaka I. J Cryst Growth, 2000; 210: 637
[23] Dutkiewicz J, Zabdyr L, Moser Z, Salawa J. J Phase Equil, 1989; 10: 223
[24] Ma D, Li Y, Ng S C. J Cryst Growth, 2000; 219: 300
[25] Trivedi R, Park J S. J Cryst Growth, 2002; 235: 572
[26] Liu S, Trivedi R. Metall Mater Trans, 2006; 37A: 3293 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|