| 800H合金热变形行为及热加工性能研究 |
| 曹宇1),邸洪双1),张敬奇1),马天军2),张洁岑1) |
1) 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳110819
2) 宝山钢铁股份有限公司特钢事业部, 上海200940 |
|
| RESEARCH ON HOT DEFORMATION BEHAVIOR AND HOT WORKABILITY OF ALLOY 800H |
| CAO Yu 1), DI Hongshuang1), ZHANG Jingqi1), MA Tianjun2), ZHANG Jiecen1) |
| 1) State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
2) Special Steel Business Unit, Baoshan Iron & Steel Co., Ltd., Shanghai 200940 |
引用本文:
曹宇,邸洪双,张敬奇,马天军,张洁岑. 800H合金热变形行为及热加工性能研究[J]. 金属学报, 2013, 49(7): 811-821.
CAO Yu,
DI Hongshuang,
ZHANG Jingqi,
MA Tianjun,
ZHANG Jiecen.
RESEARCH ON HOT DEFORMATION BEHAVIOR AND HOT WORKABILITY OF ALLOY 800H[J]. Acta Metall Sin, 2013, 49(7): 811-821.
| [1] Liu Q, Hansen N. Scr Metall Mater, 1995; 32: 1289
[2] Hansen N, Huang X, Winther G. Mater Sci Eng, 2008; A494: 61
[3] Meyers M A, Andrade U R, Chokshi A H. Metall Mater Trans, 1995; 26A: 2881
[4] Nemat-Nasser S, Isaacs J B, Liu M Q. Acta Mater, 1998; 46: 1307
[5] Meyer M A, Xu Y B, Xue Q, Perez-Prado M T, McNelley T R. Acta Mater, 2003; 51: 1307
[6] Xue Q, Bingert J F, Henrie B L, Gray III G T. Mater Sci Eng, 2008; A473: 279
[7] Xu Y B, Yang H J, Meyer M A. Scr Mater, 2008; 58: 691
[8] Derby B. Acta Metall, 1991; 39: 955
[9] Meyers M A, Nesterenko V F, Lasalvia J C, Xu Y B, Xue Q J. Phys IV, 2000; 9: 51
[10] Hines J A, Vecchio K S, Ahzi S. Metall Mater Trans, 1998; 29A: 191
[11] Momeni A, Dehghani K, Keshmiri H, Ebrahimi G R. Mater Sci Eng, 2010; A527: 1605
[12] Ju Q, Li D G, Liu G Q. Acta Metall Sin, 2006; 42: 219
(鞠泉, 李殿国, 刘国权. 金属学报, 2006; 42: 219)
[13] Zhang J Q, Di H S, Wang H T, Mao K, Ma T J, Cao Y. J Mater Sci, 2012; 47: 4000
[14] Sivaprasad P V, Mannan S L, Prasad Y V R K, Chaturvedi R C. Mater Sci Technol, 2001; 17: 545
[15] Tang W N, Chen R S, Han E H. Acta Metall Sin, 2006; 42: 1096
(唐伟能, 陈荣石, 韩恩厚. 金属学报, 2006; 42: 1096)
[16] Meng G, Li B L, Li H M, Nie Z R. Mater Sci Eng, 2009; A517: 132
[17] Cavaliere P, Cerri E, Evangelista E. Mater Sci Eng, 2004; A387--389: 857
[18] Lin Y C, Chen M S, Zhong J. Mech Res Commun, 2008; 35: 142
[19] Mandal S, Bhaduri A K, Subramaya Sarma V. Metall Mater Trans, 2012; 43A: 2056
[20] Roberts W, Ahlblom B. Acta Metall, 1978; 26: 801
[21] Meyers M A, Nesterenko V F, Lasalvia J C, Xue Q. Mater Sci Eng, 2001; A317: 204
[22] Monajati H, Jahazi M, Yue S, Taheri A K. Metall Mater Trans, 2005; 36A: 895
[23] Goetz R L, Semiatin S L. J Mater Eng Perform, 2001; 10: 710
[24] Mataya M C, Sackschewsky V E. Metall Mater Trans, 1994; 41A: 2737
[25] Liu Y, Hu R, Li J S, Kou H C, Li H W, Chang H, Fu H Z. Mater Sci Eng, 2008; A497: 283
[26] Akben M G, Weiss I, Jonas J J. Acta Metall, 1981; 29: 114
[27] Lee K J. Scr Mater, 1999; 40: 840
[28] Vega M I, Medina S F, Chapa M, Quispe A. ISIJ Int, 1999; 39: 1304
[29] Guo J T, Ranucci D, Picco E, Strocchi M. Metall Mater Trans, 1983; 14A: 2329
[30] Cao Y, Di H S, Zhang J C, Ma T J, Zhang J Q. Acta Metall Sin, 2012; 48: 1179
(曹宇, 邸洪双, 张洁岑, 马天军, 张敬奇. 金属学报, 2012; 48: 1179)
[31] Zurob H S, Berchet Y, Purdy G. Acta Mater, 2001; 49: 4183
[32] Prasad Y V R K, Gegel H L, Doraivelu S M, Malas J C, Morgan J T, Lark K A, Barker D R. Metall Mater Trans, 1984; 15A: 1883
[33] Kalyan Kumar A K S. PhD Dissertation, Indian Institute of Science, Bangalore, India, 1987
[34] Ziegler H. Progress in Solid Mechanics. New York: Wiley, 1963: 93
[35] Prasad Y V R K, Seshacharyulu T. Int Mater Rev, 1998; 43: 243 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|