| Zr-0.4Fe-1.0Cr-x Mo合金在500℃和10.3 MPa水蒸汽中的腐蚀行为 |
| 韦天国1),龙冲生1),苗志1),刘云明1),栾佰峰2) |
1)中国核动力研究设计院反应堆燃料及材料重点实验室, 成都 610041
2)重庆大学材料科学与工程学院, 重庆 400044 |
|
| CORROSION BEHAVIOR OF Zr-0.4Fe-1.0Cr-x Mo ALLOYS IN 500℃ and 10.3 MPa STEAM |
| WEI Tianguo1), LONG Chongsheng1), MIAO Zhi1), LIU Yunming1) |
1)Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610041
2)Institute of Material Science and Technology, Chongqing University, Chongqing 400044 |
引用本文:
韦天国,龙冲生,苗志,刘云明,栾佰峰. Zr-0.4Fe-1.0Cr-x Mo合金在500℃和10.3 MPa水蒸汽中的腐蚀行为[J]. 金属学报, 2013, 49(6): 717-724.
WEI Tianguo,
LONG Chongsheng,
MIAO Zhi,
LIU Yunming,
LUAN Baifeng.
CORROSION BEHAVIOR OF Zr-0.4Fe-1.0Cr-x Mo ALLOYS IN 500℃ and 10.3 MPa STEAM[J]. Acta Metall Sin, 2013, 49(6): 717-724.
| [1] Mardon J P, Charquet D, Senevat J. In: Sabol G P, Moan G D eds.,Zirconium in the Nuclear Industry: 12th International Symposium, ASTM STP 1354,West Conshonocken: ASTM International, 2000: 505
[2] Comstock R J, Schoenberger G, Sabol G P. In: Bradley E R, Sabol G P eds.,Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295,West Conshonocken: ASTM International, 1996: 710
[3] Garde A. In: Limbak M, Bareris P eds., Zirconium in the Nuclear Industry,16th International Symposium, ASTM STP 1529, West Conshonocken: ASTM International, 2010: 9
[4] Pahutova M, Kucharova K, Cadek J. Mater Sci Eng, 1977; 27: 239
[5] Pahutova M, Cadek J. Mater Sci Eng, 2004; 33: 1362
[6] Chun Y B, Hwang S K, Kim M H, Kwun S I, Kim Y S. J Nucl Mater, 1999; 265: 28
[7] Isobe T, Matsuo Y. In: Eucken C M, Garde A M eds.,Zirconium in the Nuclear Industry, 9th International Symposium, ASTM STP 1132,West Conshonocken: ASTM International, 1991: 346
[8] Chun Y B, Hwang S K, Kwun S I, Kim M H. Scr Mater, 1999; 40: 1165
[9] Lee J H, Hwang S K, Yasuda K, Kinoshita C. J Nucl Mater, 2001; 289: 334
[10] Moon J R, Lees D G. Corros Sci, 1970; 10: 85
[11] Moon J R, Evans E W. Corros Sci, 1969; 9: 323
[12] Lee J H, Hwang S K. J Nucl Mater, 2003; 321: 238
[13] George P S, Robert J C, Umesh P N. In: Sabol G P, Moan G D eds.,Zirconium in the Nuclear Industry: 12th International Syposium, ASTM STP 1354,West Conshonocken: ASTM International, 2000: 525
[14] Motta A T, Aylin Y, Marcelo J G, Comstock R J, Was G S, Busby J T,Gartner E, Peng Q J, Jeong Y H, Park J Y. J Nulc Mater, 2007; 371: 61
[15] Wang J, Long C S, Xiong J, Miao Z, Fang H Y, Huang Z H, Ying S H. Nucl Power Eng,2009; 30: 58
(王均, 龙冲生, 熊计, 苗志, 范洪远, 黄照华, 应诗浩. 核动力工程, 2009; 30: 58)
[16] Yao M Y, Wang J H, Peng J C, Zhou B X, Li Q. In: Limbak M, Bareris P eds.,Zirconium in the Nuclear Industry, 16th International Symposium, ASTM STP 1529, West Conshonocken:ASTM International, 2011: 466
[17] Li S L, Yao M Y, Zhang X, Geng J Q, Peng J C, Zhou B X. Acta Metall Sin, 2011; 47: 163
(李士炉, 姚美意, 张欣, 耿建桥, 彭建超, 周邦新. 金属学报, 2011; 47: 163)
[18] Yao M Y, Li S L, Zhang X, Peng J C, Zhou B X, Zhao X S, Shen J Y. Acta Metall Sin, 2011; 47: 865
(姚美意, 李士炉, 张欣, 彭建超, 周邦新, 赵旭山, 沈剑韵. 金属学报, 2011; 47: 865)
[19] Barberis P, Merle-Mejean T, Quintard P. J Nulc Mater, 1997; 246: 232
[20] Barberis P, Corroleur T G, Guinbretiere R, Merle M T, Mirgorodsky A,Quintard P. J Nulc Mater, 2001; 288: 241
[21] Godlewski J, Gross J P, Lambertin M, Wadier J F, Weidinger H. In:Eucken C M, Garde A M eds., Zirconium in the Nuclear Industry, 9th International Symposium,ASTM STP 1132, West Conshonocken: ASTM International, 1991: 416
[22] Liu J Z ed. Nuclear Structural Materials. Beijing: Chemical Industry Press, 2007: 27
(刘建章~ 主编. 核结构材料. 北京: 化学工业出版社, 2007: 27)
[23] Li Q, Zhou B X, Yao M Y, Liu W Q, Chu Y L. Rare Met Mater Eng, 2007; 36: 1358
(李强, 周邦新, 姚美意, 刘文庆, 褚于良. 稀有金属材料与工程, 2007; 36: 1358)
[24] IAEA-TECDOC-996. Waterside Corrosion of Zirconium Alloys in Nuclear Power Plants. Vienna, IAEA, 1998: 9
[25] Jong H B, Yong H J. J Nulc Mater, 2000; 280: 235
[26] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. In: Kamenzind B, Limback M eds.,Zirconium in the Nuclear Industry: 15th International Symposium, ASTM STP 1505,West Conshonocken: ASTM International, 2009: 360
[27] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009
(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|