| 激光成形修复2Cr13不锈钢热影响区的组织研究 |
| 徐庆东,林鑫,宋梦华,杨海欧,黄卫东 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| MICROSTRUCTURE OF HEAT-AFFECTED ZONE OF LASER FORMING REPAIRED 2Cr13 STAINLESS STEEL |
| XU Qingdong, LIN Xin, SONG Menghua, YANG Haiou, HUANG Weidong |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
徐庆东,林鑫,宋梦华,杨海欧,黄卫东. 激光成形修复2Cr13不锈钢热影响区的组织研究[J]. 金属学报, 2013, 49(5): 605-613.
XU Qingdong,
LIN Xin,
SONG Menghua,
YANG Haiou,
HUANG Weidong.
MICROSTRUCTURE OF HEAT-AFFECTED ZONE OF LASER FORMING REPAIRED 2Cr13 STAINLESS STEEL[J]. Acta Metall Sin, 2013, 49(5): 605-613.
| [1] Shao T M, Hua M, Tam H Y. Wear, 2003; 255: 444 [2] Xue L, Chen J, Lin X, Wang W, Lv X W, Huang W D. Rare Met Mater Eng, 2007; 36: 989 (薛蕾, 陈静, 林鑫, 王维, 吕晓卫, 黄卫东. 稀有金属材料与工程, 2007; 36: 989) [3] Yaso M, Morito S, Ohba T, Kobota K. Mater Sci Eng, 2008; A481: 770 [4] Lin X, Yue T M, Yang H O, Huang W D. Acta Mater, 2006; 54: 1901 [5] Gaumann M, Henry S, Cleton F, Wegniere J D, Kurz W. Mater Sci Eng, 1999; A271: 232 [6] Liu F C, Lin X, Huang C P, Song M H, Yang G L, Chen J, Huang W D. J Alloys Compd, 2011; 205: 4505 [7] Lin X, Yang H O, Chen J, Huang W D. Acta Metall Sin, 2006; 42: 361 (林鑫, 杨海欧, 陈静, 黄卫东. 金属学报, 2006; 42: 361) [8] Xu X J, Lin X, Yang M C, Chen J, Huang W D. J Alloys Compd, 2009; 480: 782 [9] Wu X, Sharman R, Mei J, Voice W. Mater Des, 2004; 25: 103 [10] Lin X, Yue T M. Mater Sci Eng, 2005; A402: 294 [11] Liu Y H, Chen J, Zhang Q, Xue L, Lin X, Huang W D. Chin Opt Lett, 2011; 9: 1671 [12] Tan H, Chen J, Zhang F Y, Lin X, Huang W D. Rare Met Mater Eng, 2009; 38: 574 [13] Lin X, Cao Y Q, Wu X Y, Yang H O, Chen J, Huang W D. Mater Sci Eng, 2012; A553: 80 [14] Mahmoudia B, Torkamany M J, Sabour Rouh Aghdam A R, Sabbaghzade J. Mater Des, 2010; 31: 2553 [15] Chen J Y, Xue L, Wang S H. In: Asfahani R, Milbourn D, eds, Materials Science & Technology 2008 Conference & Exhibition, Pittsburgh: Materials Science and Technology, 2008: 1388 [16] Yang D H, Zhang X S, Xue Q J. Tribology, 1994; 14: 41 (杨德华, 张绪寿, 薛群基. 摩擦学学报, 1994; 14: 41) [17] Shao T M, Lin X C, Yuan W D. Acta Metall Sin, 2001; 37: 1040 (邵天敏, 蔺秀川, 袁伟东. 金属学报, 2001; 37: 1040) [18] Li Y M, Liu Z X, Yang H O, Lin X, Huang W D, Li J G. Acta Metall Sin, 2003; 39: 521 (李延民, 刘振侠, 杨海欧, 林鑫, 黄卫东, 李建国. 金属学报, 2003; 39: 521) [19] Wang L, Felicelli S. J Manuf Sci Eng, 2007; 129: 1028 [20] Jendrzejewski R, Kreja I, Sliwinski G. Mater Sci Eng, 2004; A379: 313 [21] Jia W P, Tang H P, He W W, Lin X, Huang W D. Acta Metall Sin, 2010; 46: 135 (贾文鹏, 汤慧萍, 贺卫卫, 林鑫, 黄卫东. 金属学报, 2010; 46: 135) [22] Ye R Q, Smugeresky J E, Zheng B L, Zhou Y Z, Lavernia E J. Mater Sci Eng, 2006; A428: 47 [23] Bassani R, Levita G, Meozzi M, Palla G. Wear, 2001; 247: 125 [24] Lippold J C, Kotecki D J, translated by Chen J H. Welding Metallurgy and Weldability of Stainless Steel. Beijing: China Maching Press, 2008: 61 (Lippold J C, Kotecki D J著, 陈剑虹译. 不锈钢焊接冶金学及焊接性. 北京: 机械工业出版社, 2008: 61) [25] Yong Q L. Second Phases in Structural Steels. Beijing: Metallurgical Industry Press, 2006: 81 (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 81) [26] Miokovic T, Schulze V, Vohringer O, Lohe D. Acta Metall, 2007; 55: 589 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|