| Al70Bi11Sn19合金颗粒的核壳组织 |
| 张俊芳1),王予津2),卢温泉1),张曙光1),李建国1) |
1) 上海交通大学材料科学与工程学院, 上海 200240
2) 上海交通大学机械与动力工程学院, 上海 200240 |
|
| THE CORE-SHELL STRUCTURE OF Al70Bi11Sn19 IMMISCIBLE ALLOY PARTICLES |
| ZHANG Junfang1), WANG Yujin 2), LU Wenquan 1), ZHANG Shuguang 1), LI Jianguo 1) |
1) School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240
2) School of Mechanical Engineering, Shanghai Jiao Tong University, Shanghai 200240
|
引用本文:
张俊芳,王予津,卢温泉,张曙光,李建国. Al70Bi11Sn19合金颗粒的核壳组织[J]. 金属学报, 2013, 29(4): 457-463.
ZHANG Junfang,
WANG Yujin,
LU Wenquan,
ZHANG Shuguang,
LI Jianguo.
THE CORE-SHELL STRUCTURE OF Al70Bi11Sn19 IMMISCIBLE ALLOY PARTICLES[J]. Acta Metall Sin, 2013, 29(4): 457-463.
| [1] Ratke L, Diefenbach S. Mater Sci Eng, 1995; R15: 263 [2] Xie H, Yang G C, La P Q, Hao W X, Fan J F, Liu W M, Xu L J. Mater Charact, 2004; 52: 153 [3] Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K. Science, 2002; 297: 990 [4] Ohnuma I, Saegusa T, Takaku Y, Wang C P, Liu X J, Kainuma R, Ishida K. J Electron Mater, 2009; 38: 2 [5] Jia J, Zhao J Z, Guo J J, Liu Y. Immiscible Alloy and Preparation Technology.Harbin: Harbin Institute of Technology Press, 2002: 1 (贾均, 赵九洲, 郭景杰, 刘源. 难混溶合金及其制备技术. 哈尔滨: 哈尔滨工业大学出版社, 2002: 1) [6] Wang C P, Liu X J, Takaku Y, Ohnuma I, Kainuma R, Ishida K. Metall Mater Trans, 2004; 35A: 1243 [7] Wang C P, Liu X J, Shi R P, Shen C, Wang Y, Ohnuma I, Kainuma R, Ishida K. Appl Phys Lett, 2007; 91: 141904 [8] Dai R R, Zhang S G, Guo X, Li J G. Mater Lett, 2011; 65: 322 [9] Dai R R, Zhang S G, Guo X, Li J G. J Electron Mater, 2011; 40: 2458 [10] Dai R R, Zhang S G, Guo X, Li J G. J Alloys Compd, 2011; 509: 2289 [11] Wilde G, Perepezko J H. Acta Mater, 1999; 47: 3009 [12] Li H L, Zhao J Z, He J. Acta Metall Sin, 2007; 43: 659 (李海丽, 赵九洲, 何杰. 金属学报, 2007; 43: 659) [13] Li Y S. PhD Dissertation, Hunan University, Changsha, 2007 (李元山. 湖南大学博士学位论文, 长沙, 2007) [14] Grobner J, Schmid-Fetzer R. J Met, 2005; 57: 19 [15] Grobner J, Mirkovic D, Schmid-Fetzer R. Acta Mater, 2005; 53: 3271 [16] Kaban I, Hoyer W. Phys Rev, 2008; 77B: 125426 [17] Young N O, Goldstein J S, Block M J. J Fluid Mech, 1959; 6: 350 [18] Ratke L, Voorhees P W. Growth and Coarsening. New York: Springer-Verlag, 2002: 1 [20] Wakitani S. J Phys: Conf Ser, 2007; 64: 012006 [21] Davis R H. Int J Thermophys, 1986; 7: 609 [22] Zhang H W, Xian A P. Acta Metall Sin, 2000; 36: 347 (张宏闻, 冼爱平. 金属学报, 2000; 36: 347) [23] Qin T, Wang H P, Wei B B. Sci China, 2007; 37G: 409 (秦涛, 王海鹏, 魏炳波. 中国科学, 2007; 37G: 409) [24] Xu Z, Yao S S. Theories of Materials Processing. Beijing: Science Press, 2003: 40 (徐洲, 姚寿山. 材料加工原理. 北京: 科学出版社, 2003: 40) [25] Martin J W, Doherty R D, translated by Li X L. Stability of Microstructure in Metallic Systems.Beijing: Science Press. 1984: 194 (Martin J W, Doherty R D著, 李新立 译. 金属系中显微结构的稳定性. 北京:科学出版社, 1984: 194) [26] Shi R P, Wang C P, Wheeler D, Liu X J, Wang Y. Acta Mater, 2013; 61: 1229 |
|