					引用本文:
						|  |  
    					|  |  
    					| 微观组织对共析钢室温加工硬化行为的影响 |  
						| 郑成思1,李龙飞1,杨王玥2,孙祖庆1 |  
					| 1) 北京科技大学新金属材料国家重点实验室, 北京 100083 2) 北京科技大学材料科学与工程学院, 北京 100083 |  
						|  |  
    					| INFLUENCE OF MICROSTRUCTURES OF EUTECTOIDSTEEL ON ROOM TEMPERATURE WORKHARDENING BEHAVIOR |  
						| ZHENG Chengsi1, LI Longfei1, YANG Wangyue2, SUN Zuqing1 |  
						| 1) The State Key Laboratory for Advanced Metals and Materials, University of Science& Technology Beijing, Beijing,100083 2) School of Materials Science and Engineering, University of Science & Technology Beijing, Beijing 100083 |  
								郑成思,李龙飞,杨王玥,孙祖庆. 微观组织对共析钢室温加工硬化行为的影响[J]. 金属学报, 2013, 49(3): 257-264.	
																												ZHENG Chengsi1,
																								LI Longfei1,
																								YANG Wangyue2,
																												SUN Zuqing1. 
				INFLUENCE OF MICROSTRUCTURES OF EUTECTOIDSTEEL ON ROOM TEMPERATURE WORKHARDENING BEHAVIOR[J]. Acta Metall Sin, 2013, 49(3): 257-264.
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1]Howe AA.Mater SciTechnol, 2000; 16: 1264 [2]Jia D, Ramesh K T, Ma E.Acta Mater, 2003; 51: 3495 [3]Hazra S S, Pereloma E V, Gazder A A.Acta Mater, 2011; 59: 4015 [4]Gazder A A, Hazra S S, Pereloma E V.Mater SciEng, 2011; A530: 492 [5]Akio O, Shiro T, Kotobu N.ISIJ Int, 2004; 44: 1063 [6]Torizuka S, Muramatsu E, NarayanaMurty S V S, Nagai K.Scr Mater, 2006; 55: 751 [7]Zhao M C, Yin F X, Hanamura T, Nagai K, Atrens A.Scr Mater, 2007; 57: 857 [8]Maki T, Furuhara T.Mater Sci Forum, 2003; 426--432: 19 [9]Furuhara T, Mizoguchi T.ISIJ Int, 2004; 45: 392 [10]Song R, Ponge D, Raabe R.Scr Mater, 2005; 52: 1075 [11]Song R, Ponge D, Raabe R.Acta Mater, 2005; 53: 4881 [12]Tsuzaki K, Sato E, Furimoto S, Furuhara T, Maki T.Scr Mater, 1999; 40: 675 [13]Park K T, Kim Y S, Lee J G, Shi D H.Mater SciEng, 2000; A293: 165 [14]Tsuji N, Ueji R, Minamino Y, Saito Y.Scr Mater, 2002; 46: 305 [15]Ueji R, Tsuji N, Minamino Y, Koizumi Y.Acta Mater, 2002; 50: 4177 [16]Park K T, Shin D H.Metall Mater Trans, 2002; 33A: 705 [17]Song R, Ponge D, Raabe D, Kaspar R.Acta Mater, 2005; 53: 845 [18]Tsuchida N, Masuda H, Harada Y, Fukaura K, Tomota Y, Nagai K.Mater SciEng, 2008; A488: 446 [19]Song R, Ponge D, Raabe D, Speer J G, Matlock D K.Mater SciEng, 2006; A441: 1 [20]Yoda R, Shibata K, Morimitsu T, Terada D, Tsuji N.Scr Mater, 2011; 65: 175 [21]Syn C K, Lesuer D, Sherby O D.Metall Mater Trans, 1994; 25A: 1481 [22]Chen W, Li L F, Yang W Y, Sun Z Q, He J P.ActaMetall Sin, 2009; 45: 151 (陈伟, 李龙飞, 杨王玥, 孙祖庆, 何建平. 金属学报, 2009; 45: 151) [23]Huang Q S, Li L F, Yang W Y, Sun Z Q.ActaMetall Sin, 2007; 43: 724 (黄青松, 李龙飞, 杨王玥, 孙祖庆. 金属学报, 2007; 43: 724) [24]Oyama T, Sherby O D, Wadsworth J, Walser B.ScrMetall, 1984; 18: 799 [25]Dollar M, Bernstein I M, Thompson A W.ActaMetall, 1988; 36: 311 [26]Ray K K, Mondal D.ActaMetall Mater, 1991; 39: 2201 [27]Ashby M F.Philos Mag, 1970; 21: 399 [28]Kuhlmann-Wilsdorf D.Philos Mag, 1999; 79: 955 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |