| 一个共面双滑移取向Cu单晶体疲劳位错结构的热稳定性研究 |
| 郭巍巍1,齐成军1,李小武1,2 |
| 1. 东北大学理学院材料物理与化学研究所, 沈阳 110819
2. 东北大学材料各向异性与织构教育部重点实验室, 沈阳 110819 |
|
| INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN A DOUBLE-SLIPORIENTED Cu SINGLE CRYSTAL |
| GUO Weiwei1, QI Chengjun1, LI Xiaowu1,2 |
| 1. Institute of Materials Physics and Chemistry, College of Sciences, Northeastern University, Shenyang 110819
2. Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819 |
引用本文:
郭巍巍,齐成军,李小武. 一个共面双滑移取向Cu单晶体疲劳位错结构的热稳定性研究[J]. 金属学报, 2013, 49(1): 107-114.
GUO Weiwei,
QI Chengjun,
LI Xiaowu.
INVESTIGATIONS ON THERMAL STABILITY OF FATIGUE DISLOCATION STRUCTURES IN A DOUBLE-SLIPORIENTED Cu SINGLE CRYSTAL[J]. Acta Metall Sin, 2013, 49(1): 107-114.
| [1] Mughrabi H. Mater Sci Eng, 1978; 33: 207 [2] Jin N Y, Winter A T. Acta Metall, 1984; 32: 989 [3] Basinski Z S, Basinski S J. Prog Mater Sci, 1992; 36: 89 [4] Suresh S. Fatigue of Materials. 2nd Ed., London: Cambridge University Press, 1998: 28 [5] Li X W. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1998 (李小武. 中国科学院金属研究所博士学位论文, 沈阳, 1998) [6] Li X W, Wang Z G, Li S X. Philos Mag Lett, 1999; 79: 715 [7] Zhang J X, Jiang Y Y. Int J Plast, 2005; 21: 2191 [8] Zhang J X, Jiang Y Y. Acta Mater, 2007; 55: 1831 [9] Li P, Li S X, Wang Z G, Zhang Z F. Prog Mater Sci, 2011; 56: 328 [10] Steckmeyer A, Sauzay M, Weidner A, Hieckmann E. Int J Fatigue, 2012; 40: 154 [11] Ackermann F, Kubin L P, Lepinous J, Mughrabi H. Acta Metall, 1984; 32: 715 [12] Li X W, Hu Y M, Wang Z G. Mater Sci Eng, 1998; A248: 299 [13] Li X W, Zhang Z F, Wang Z G, Li S X, Umakoshi Y. Defect Diffusion Forum, 2001; 188-199: 153 [14] Li X W, Umakoshi Y, Gong B, Li S X, Wang Z G. Mater Sci Eng, 2002; A333: 51 [15] Li P, Zhang Z F, Li X W, Li S X, Wang Z G. Acta Mater, 2009; 57: 4845 [16] Zhou Y, Li X W, Zhang G P, Zhang Z F. Mater Sci Technol, 2009; 17: 649 (周杨, 李小武, 张广平, 张哲峰. 材料科学与工艺, 2009; 17: 649) [17] Li X W, Zhou Y, Guo W W, Zhang G P. Cryst Res Technol, 2009; 44: 315 [18] Guo W W, Wang X M, Li X W. Mater Trans, 2010; 51: 887 [19] Li P, Li S X, Wang Z G, Zhang Z F. Acta Mater, 2010; 58: 3281 [20] Tabata T, Fujita H, Hiraoka M, Onishi I C. Philos Mag, 1983; 47A: 841 [21] Wang Z R. Scr Mater, 1998; 39: 493 [22] Chen S, Gottstein S. Mater Sci Eng, 1989; 110: 9 [23] Kuhlman-Wilsdorf D. Trans Met Soc AIME, 1962; 224: 1047 [24] Glazov M, Llanes L M, Laird C. Phys Stat Sol, 1995; 149A: 297 [25] Li X W, Wang Z G, Li S X. Mater Sci Eng, 1999; A260: 132 [26] Li X W, Wang Z G, Zhang Y W, Li S X, Umakoshi Y. Phys Stat Sol, 2002; 191A: 97 [27] Zhou Y, Li X W, Yang R Q. Int J Mater Res, 2008; 99: 958 [28] Kopzky C V, Novikov V Y, Fionova L K. Acta Metall, 1985; 33: 873 [29] Yang G, Sun L J, Zhang L N, Wang L M, Wang C. Chin J Iron Steel Res, 2009; 21: 39 (杨钢, 孙利军, 张丽娜, 王立民, 王昌. 钢铁研究学报, 2009; 21: 39) [30] Zhu R, Li S X, Li Y, Li M Y, Chao Y S. Acta Metall Sin, 2004; 40: 467 (朱荣, 李守新, 李勇, 李明扬, 晁月盛. 金属学报, 2004; 40: 467) [31] Guo W W, Ren H, Qi C J, Wang X M, Li X W. Acta Phys Sin, 2012; 61: 156201-1 (郭巍巍, 任焕, 齐成军, 王小蒙, 李小武. 物理学报, 2012; 61: 156201-1) [32] Xiao S H, Guo J D, Wu S D, He G H, Li S X. Acta Metall Sin, 2002; 38: 161 (肖素红, 郭敬东, 吴世丁, 何冠虎, 李守新. 金属学报, 2002; 38: 161) [33] Pande C S, Imam M A, Rath B B. Metall Trans, 1990; 21A: 2891 [34] Mahajan S, Pande C S, Imam M A, Rath B B. Acta Mater, 1997; 45: 2633 [35] Xia S, Li H, Zhou B X, Chen W J. Chin J Nature, 2010; 32: 94 (夏爽, 李慧, 周邦新, 陈文觉. 自然杂志, 2010; 32: 94) |
|