Please wait a minute...
金属学报  2012, Vol. 48 Issue (8): 1005-1010    DOI: 10.3724/SP.J.1037.2012.00116
  论文 本期目录 | 过刊浏览 |
FGH4096粉末高温合金的再结晶形核机制
宁永权, 姚泽坤
西北工业大学材料学院, 西安 710072
RECRYSTALLIZATION NUCLEATION MECHANISM OF FGH4096 POWDER METALLURGY SUPERALLOY
NING Yongquan, YAO Zekun
School of Material Science and Engineering, Northwestern Polytechnical University, Xi’an 710072
引用本文:

宁永权 姚泽坤. FGH4096粉末高温合金的再结晶形核机制[J]. 金属学报, 2012, 48(8): 1005-1010.
. RECRYSTALLIZATION NUCLEATION MECHANISM OF FGH4096 POWDER METALLURGY SUPERALLOY[J]. Acta Metall Sin, 2012, 48(8): 1005-1010.

全文: PDF(6413 KB)  
摘要: 利用OM和TEM对FGH4096粉末高温合金的再结晶组织进行了系统的观察和分析,证实有3种再结晶形核机制存在, 即原始颗粒边界形核、应变诱导蝶状γ'相形核和孪晶叠加形核. 通过研究微观偏析, 弯曲褶皱边界的形成和孪晶叠加效应, 原子扩散和位错运动建立了形核模型.
关键词 : 粉末高温合金,  再结晶,  形核机制    
Abstract:FGH4096 is regarded as a promising powder metallurgy superalloy for high–temperature/pressure turbine disc in aerospace industries due to its high resistance/defect tolerance and high working temperature up to 750 ℃. In the present work, OM and TEM have been employed to study the recrystallization nucleation and microstructure evolution in FGH4096 powder metallurgy superalloy. It is proved that there exist three types of recrystallization mechanisms: nucleation from previous particle boundary (PPB), strain–induced nucleation from butterfly γ' phase (SIP) and twins superposition (TS) nucleation. The physical explanation for this is given from the view of point of micro–segregation, formation of the bend fold boundary and twins superposition, atomic diffusion and dislocation movement.
Key words: powder metallurgy superalloy    recrystallization    nucleation mechanism
收稿日期: 2012-03-05     
ZTFLH: 

TG 113

 
基金资助:

国家自然科学基金项目51101119和中国博士后基金项目20110491686资助

作者简介: 宁永权, 男, 1982年生, 博士
[1] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. 2nd Ed., Oxford: Elseriver, 2004: 10

[2] Ning Y Q, Yao Z K, Fu M W, Guo H Z. Mater Sci Eng, 2011; A528: 8065

[3] Ning Y Q, Fu M W, Yao W. Mater Sci Eng, 2012; A539: 101

[4] Ning Y Q, Yao Z K, Xie X H, Guo H Z, Tan L J, Tao Y. Acta Metall Sin, 2010; 45: 58

(宁永权, 姚泽坤, 谢兴华, 郭鸿镇, 谭立军, 陶宇. 金属学报, 2010; 45: 58)

[5] Ning Y Q, Yao Z K, Yue TW, Guo H Z, Tao Y, Zhang Y W. Rare Met Mater Eng, 2010; 39: 1235

(宁永权, 姚泽坤, 岳太文, 郭鸿镇, 陶 宇, 张义文. 稀有金属材料与工程, 2010; 39: 1235)

[6] Reed R C. The Superalloys Fundamentals and Applications. New York: Cambridge University Press, 2006: 6

[7] Ning Y Q, Yao Z K, Guo H Z, Tao Y, Zhang Y W. Key Eng Mater, 2009; 407–408: 694

[8] Zhao M L, Sun WR, Yang S L, Qi F, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 79

(赵美兰, 孙文儒, 杨树林, 祈峰, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 79)

[9] Viswanathan G B, Sarosi P M, Henry M F, Whitis D D, Milligan W W, Mills M J. Acta Mater, 2005; 53: 3041

[10] Tiley G, Viswanathan G B, Srinivasan R, Banerjee R, Dimiduk D M, Fraser H L. Acta Mater, 2009; 57: 2538

[11] MacSleyne J, Uchic M D, Simmons J P, Graef M D. Acta Mater, 2009; 57: 6251

[12] Dunlavy M A, Shivpuri R, Semiatin S L. Mater Sci Eng, 2003; A359: 210

[13] Viswanathan G B, Sarosi P M, Whitis D H, Mills M J. Mater Sci Eng, 2005; A400–401: 489

[14] Cao F L, Qing H, Gu Y X, Guan C B, Zhou Q. Gas Turbine Exp Res, 2007; 20(3): 15

(曹凤兰, 卿华, 古远兴, 关长波, 周全. 燃气涡轮试验与研究, 2007; 20(3): 15)

[15] Liu F J, Zhang M C, Dong X, Zhang Y W. Acta Metall Sin (Engl Lett), 2007; 20: 102

[16] Zhou X M, Wang W X, Tang D Z, Yan M G. Mater Eng, 2006; (11): 53

(周晓明, 汪武祥, 唐定中, 颜鸣皋. 材料工程, 2006; (11): 53)

[17] Liu J T, Liu G Q, Hu B F, Song Y P, Qin Z R, Zhang Y W. J Univ Sci Technol Beijing, 2006; 13: 319

[18] Tian G F, Jia C C, Wen Y, Hu B F. J Univ Sci Technol Beijing, 2008; 15: 729

[19] Ning Y Q, Yao Z K, Li H, Guo H Z, Tao Y, Zhang Y W. Mater Sci Eng, 2010; A527: 961

[20] Ning Y Q, Yao Z K, Li H, Guo H Z, Tao Y, Zhang Y W. Chin J Mech Eng, 2009; 22: 925

[21] Ning Y Q, Yao Z K, Fu M W, Guo H Z. Mater Sci Eng, 2010; A527: 6968

[22] Xie X H, Yao Z K, Ning Y Q, Guo H Z, Tao Y, Zhang Y W. J Aero Mater, 2011; 31: 22

(谢兴华, 姚泽坤, 宁永权, 郭鸿镇, 陶 宇, 张义文. 航空材料学报, 2011; 31: 22)

[23] Ozols A, Sirkin H R, Vicente E E. Mater Sci Eng, 1999; A262: 64

[24] Sun X Y, Song H M, Lin Q. J Chin Soc Rare Earths, 2004; 22: 177

(孙学义, 宋红梅, 林勤. 中国稀土学报, 2004; 22: 177)

[25] Yang P, Fu Y Y, Cui Y E. Acta Metall Sin, 2001; 37: 601

(杨平, 傅云义, 崔月娥. 金属学报, 2001; 37: 601)

[26] Yi M, Xiong H B, Lin Z. Shougang Sci Technol, 2008; (1): 1

(易敏, 熊化冰, 林志. 首钢科技, 2008; (1): 1)
[1] 赵鹏, 谢光, 段慧超, 张健, 杜奎. 两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] 白佳铭, 刘建涛, 贾建, 张义文. 高W高Ta型粉末高温合金的蠕变性能及溶质原子偏聚[J]. 金属学报, 2023, 59(9): 1230-1242.
[3] 常松涛, 张芳, 沙玉辉, 左良. 偏析干预下体心立方金属再结晶织构竞争[J]. 金属学报, 2023, 59(8): 1065-1074.
[4] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[5] 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响[J]. 金属学报, 2023, 59(7): 855-870.
[6] 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博. 轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能[J]. 金属学报, 2023, 59(11): 1439-1447.
[7] 吴彩虹, 冯迪, 臧千昊, 范诗春, 张豪, 李胤樹. 喷射成形AlSiCuMg合金的热变形组织演变及再结晶行为[J]. 金属学报, 2022, 58(7): 932-942.
[8] 杨秦政, 杨晓光, 黄渭清, 石多奇. 粉末高温合金FGH4096的疲劳小裂纹扩展行为[J]. 金属学报, 2022, 58(5): 683-694.
[9] 任少飞, 张健杨, 张新房, 孙明月, 徐斌, 崔传勇. 新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制[J]. 金属学报, 2022, 58(2): 129-140.
[10] 姜伟宁, 武晓龙, 杨平, 顾新福, 解清阁. 热轧硅钢表层动态再结晶区形成规律及剪切织构特征[J]. 金属学报, 2022, 58(12): 1545-1556.
[11] 胡晨, 潘帅, 黄明欣. 高强高韧异质结构温轧TWIP钢[J]. 金属学报, 2022, 58(11): 1519-1526.
[12] 杨志昆, 王浩, 张义文, 胡本芙. Ta含量对镍基粉末高温合金高温蠕变变形行为和性能的影响[J]. 金属学报, 2021, 57(8): 1027-1038.
[13] 姜巨福, 张逸浩, 刘英泽, 王迎, 肖冠菲, 张颖. RAP法制备AlSi7Mg合金半固态坯料研究[J]. 金属学报, 2021, 57(6): 703-716.
[14] 李彦默, 郭小辉, 陈斌, 李培跃, 郭倩颖, 丁然, 余黎明, 苏宇, 李文亚. GH4169合金与S31042钢线性摩擦焊接头组织及力学性能[J]. 金属学报, 2021, 57(3): 363-374.
[15] 倪珂, 杨银辉, 曹建春, 王刘行, 刘泽辉, 钱昊. 18.7Cr-1.0Ni-5.8Mn-0.2N节Ni型双相不锈钢的大变形热压缩软化行为[J]. 金属学报, 2021, 57(2): 224-236.