| 柱状晶对Fe-3%Si电工钢冷轧织构演变规律的影响 |
| 张宁, 杨平, 毛卫民 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| INFLUENCE OF COLUMNAR GRAINS ON THE COLD ROLLING TEXTURE EVOLUTION IN Fe-3%Si\ ELECTRICAL STEEL |
| ZHANG Ning, YANG Ping, MAO Weimin |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
张宁 杨平 毛卫民. 柱状晶对Fe-3%Si电工钢冷轧织构演变规律的影响[J]. 金属学报, 2012, 48(7): 782-788.
,
,
.
INFLUENCE OF COLUMNAR GRAINS ON THE COLD ROLLING TEXTURE EVOLUTION IN Fe-3%Si\ ELECTRICAL STEEL[J]. Acta Metall Sin, 2012, 48(7): 782-788.
| [1] Kovac F, Stoyka V, Petryshynets I. J Magn Magn Mater, 2008; 320: 627[2] Takashima M, Komatsubara M, Morito N. ISIJ Int, 1997; 37: 1263[3] Gobernado P, Petrov R, Ruiz D, Leunis E, Kestens L A I. Mater Sci Forum, 2010; 638–642: 2829[4] Tomida T, Tanaka T. ISIJ Int, 1995; 35: 548[5] Kovac F, Dzubinsky M, Sidor Y. J Magn Magn Mater, 2004; 269: 333[6] Gutierrez–Castaneda E J, Salinas–Rodriguez A. J Magn Magn Mater, 2011; 323: 2524[7] Yoshinaga N, Kestens L, De Cooman B C. Mater Sci Forum, 2005; 495–497: 1267[8] Gautam J P, Petrov R, Kestens L. Mater Sci Forum, 2007; 550: 503[9] Kestens L. Jonas J J, Van Houtte P, Aernoudt E. Metall Mater Trans, 1996; 27A: 2347[10] Abe H, Matsuo M, Ito K. Trans JIM, 1962; 26: 684[11] Walter J L, Koch E F. Acta Metall, 1962; 10: 1059[12] Dorner D, Zaefferer S, Lahn L, Raabe D. J Magn Magn Mater, 2006; 304: 183[13] Koh P K, Dunn C G. J Met, 1955; 7: 401[14] Dunn C G. Acta Metall, 1954; 2: 173[15] Walter J L, Hibbard W L. Trans AIME, 1958; 212: 731[16] Inagaki H, Suda T. Texture, 1972; 1: 129[17] B¨ottcher A, L¨ucke K. Acta Metall Mater, 1993; 41: 2503[18] Mishra S, Darmann C, L¨ucke K. Acta Metall, 1984; 32: 2185[19] Shimizu Y, Ito Y, Iida Y. Metall Trans, 1986; 17A: 1323[20] Xie J X, Fu H D, Zhang Z H, Jiang Y B. Mater Sci Eng, 2012; A538: 315[21] Zhang N, Yang P, Mao W M. Acta Metall Sin, 2012; 48: 307(张宁, 杨平, 毛卫民. 金属学报, 2012; 48:307)[22] Liu H T, Liu Z Y, Qiu Y Q, Cao G M, Li C G, Wang G D. Mater Charact, 2009; 60: 79[23] Tsuji N, Tsuzaki K, Maki T. ISIJ Int, 1992; 32: 1319[24] Quadir M Z, Duggan B J. Acta Mater, 2004; 52: 4011[25] Hutchinson B. Trans R Soc Lond, 1999; 357A: 1471[26] Van Houtte P, Li S, Seefeldt M, Delannay L. Int J Plast, 2005; 21: 589[27] Stojakovic D, Doherty R D, Kalidindi S R, Landgraf F J G. Metall Mater Trans, 2008; 39A: 1738 |
|