金属学报  2012, Vol. 48 Issue (7): 782-788    DOI: 10.3724/SP.J.1037.2011.00659
  论文 本期目录 | 过刊浏览 |
柱状晶对Fe-3%Si电工钢冷轧织构演变规律的影响
张宁, 杨平, 毛卫民
北京科技大学材料科学与工程学院, 北京 100083
INFLUENCE OF COLUMNAR GRAINS ON THE COLD ROLLING TEXTURE EVOLUTION IN Fe-3%Si\ ELECTRICAL STEEL
ZHANG Ning, YANG Ping, MAO Weimin
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
引用本文:

张宁 杨平 毛卫民. 柱状晶对Fe-3%Si电工钢冷轧织构演变规律的影响[J]. 金属学报, 2012, 48(7): 782-788.
, , . INFLUENCE OF COLUMNAR GRAINS ON THE COLD ROLLING TEXTURE EVOLUTION IN Fe-3%Si\ ELECTRICAL STEEL[J]. Acta Metall Sin, 2012, 48(7): 782-788.

全文: PDF(6037 KB)  
摘要: Fe-3%Si电工钢铸锭中普遍存在柱状晶, 其晶体学及形状各向异性对随后的热轧、冷轧及退火织构产生很大的影响. 利用XRD与EBSD技术对长轴分别平行于轧面法向(ND), 轧制方向(RD)和横向(TD)的柱状晶冷轧样品的织构及组织进行了研究, 并对晶界的特殊作用进行了分析. 结果表明, 中等压下量下, 3种柱状晶样品具有不同程度的\{001\}织构遗传性, 即3种样品均不同程度的摆脱了{111}线织构的形成; 柱状晶长轴平行于ND和TD时, {001}取向在冷轧时得到大的保留; 柱状晶长轴平行于RD时, 得到最强的 {111}<112>织构; 柱状晶长轴平行于TD时, 冷轧组织中旋转立方织构及{111}<110>织构较强. 此外, 3种样品的织构均表现出由立方→{001}<130>→{113}<251>的过渡路径, 与等轴多晶样品沿α线和γ线转动的路径不同. 不同方向的柱状晶晶界对冷轧变形过程中晶粒转动的作用不同, 但因晶粒尺寸大而作用有限, 且与初始取向相关.
关键词 : 电工钢,  柱状晶,  织构,  冷轧    
Abstract:Columnar grains exist in nearly all cast slabs of Fe-3%Si electrical steels, their morphological and crystallographic anisotropies strongly influence the microstructure and texture evolution during following hot rolling, cold rolling and final annealing. This work investigates the rolling texture and microstructure of the specimens with columnar grains initially arranged along different directions by means of XRD and EBSD techniques, and the effects of columnar grain boundaries are analyzed. The results show that at intermediate rolling reduction, all three types of specimens show to different extents the inheritance of {001} texture, or in other words, they prevent effectively the formation of {111} texture. The {001} texture is strongly retained in ND specimen (with initial columnar grains' longitudinal axis being along normal direction) and TD specimen (with initial columnar grains' longitudinal axis being along transverse direction), whereas {111}<112> texture is the strongest in RD specimen(with initial columnar grains' longitudinal axis being along rolling direction). In addition, rotated cube and {111}<110> textures develop in TD specimen. All three types of specimens demonstrate an orientation rotation path from cube {001}<100> over 20o rotated cube {001}<130> to {113}<251>, which is in contrast to the conventional rotation path from α fiber to $\gamma$ fiber in equiaxed polycrystalline electrical steels. In spite of the significant difference in grain boundary arrangement in the three types of specimens, their influence on texture formation is limited because of the large grain sizes and the influence is mainly related with initial orientations. To understand rolling texture evolution of columnar grain specimens is of great significance in the development of new type electrical steels with strong {001} texture.
Key words: electrical steel    columnar grain    texture    cold rolling
收稿日期: 2011-10-24     
基金资助:

国家自然科学基金资助项目51071024

作者简介: 张宁, 女, 1982年生, 硕士生
[1] Kovac F, Stoyka V, Petryshynets I. J Magn Magn Mater, 2008; 320: 627

[2] Takashima M, Komatsubara M, Morito N. ISIJ Int, 1997; 37: 1263

[3] Gobernado P, Petrov R, Ruiz D, Leunis E, Kestens L A I. Mater Sci Forum, 2010; 638–642: 2829

[4] Tomida T, Tanaka T. ISIJ Int, 1995; 35: 548

[5] Kovac F, Dzubinsky M, Sidor Y. J Magn Magn Mater, 2004; 269: 333

[6] Gutierrez–Castaneda E J, Salinas–Rodriguez A. J Magn Magn Mater, 2011; 323: 2524

[7] Yoshinaga N, Kestens L, De Cooman B C. Mater Sci Forum, 2005; 495–497: 1267

[8] Gautam J P, Petrov R, Kestens L. Mater Sci Forum, 2007; 550: 503

[9] Kestens L. Jonas J J, Van Houtte P, Aernoudt E. Metall Mater Trans, 1996; 27A: 2347

[10] Abe H, Matsuo M, Ito K. Trans JIM, 1962; 26: 684

[11] Walter J L, Koch E F. Acta Metall, 1962; 10: 1059

[12] Dorner D, Zaefferer S, Lahn L, Raabe D. J Magn Magn Mater, 2006; 304: 183

[13] Koh P K, Dunn C G. J Met, 1955; 7: 401

[14] Dunn C G. Acta Metall, 1954; 2: 173

[15] Walter J L, Hibbard W L. Trans AIME, 1958; 212: 731

[16] Inagaki H, Suda T. Texture, 1972; 1: 129

[17] B¨ottcher A, L¨ucke K. Acta Metall Mater, 1993; 41: 2503

[18] Mishra S, Darmann C, L¨ucke K. Acta Metall, 1984; 32: 2185

[19] Shimizu Y, Ito Y, Iida Y. Metall Trans, 1986; 17A: 1323

[20] Xie J X, Fu H D, Zhang Z H, Jiang Y B. Mater Sci Eng, 2012; A538: 315

[21] Zhang N, Yang P, Mao W M. Acta Metall Sin, 2012; 48: 307

(张宁, 杨平, 毛卫民. 金属学报, 2012; 48:307)

[22] Liu H T, Liu Z Y, Qiu Y Q, Cao G M, Li C G, Wang G D. Mater Charact, 2009; 60: 79

[23] Tsuji N, Tsuzaki K, Maki T. ISIJ Int, 1992; 32: 1319

[24] Quadir M Z, Duggan B J. Acta Mater, 2004; 52: 4011

[25] Hutchinson B. Trans R Soc Lond, 1999; 357A: 1471

[26] Van Houtte P, Li S, Seefeldt M, Delannay L. Int J Plast, 2005; 21: 589

[27] Stojakovic D, Doherty R D, Kalidindi S R, Landgraf F J G. Metall Mater Trans, 2008; 39A: 1738
[1] 常松涛, 张芳, 沙玉辉, 左良. 偏析干预下体心立方金属再结晶织构竞争[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] 王周头, 袁清, 张庆枭, 刘升, 徐光. 冷轧中碳梯度马氏体钢的组织与力学性能[J]. 金属学报, 2023, 59(6): 821-828.
[3] 王长胜, 付华栋, 张洪涛, 谢建新. 冷轧变形对高性能Cu-Ni-Si合金组织性能与析出行为的影响[J]. 金属学报, 2023, 59(5): 585-598.
[4] 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博. 轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能[J]. 金属学报, 2023, 59(11): 1439-1447.
[5] 于少霞, 王麒, 邓想涛, 王昭东. GH3600镍基高温合金极薄带的制备及尺寸效应[J]. 金属学报, 2023, 59(10): 1365-1375.
[6] 郭东伟, 郭坤辉, 张福利, 张飞, 曹江海, 侯自兵. 基于二次枝晶间距变化特征的连铸方坯CET位置判断新方法[J]. 金属学报, 2022, 58(6): 827-836.
[7] 姜伟宁, 武晓龙, 杨平, 顾新福, 解清阁. 热轧硅钢表层动态再结晶区形成规律及剪切织构特征[J]. 金属学报, 2022, 58(12): 1545-1556.
[8] 杨平, 王金华, 马丹丹, 庞树芳, 崔凤娥. 成分对真空脱锰法相变控制高硅电工钢{100}织构的影响[J]. 金属学报, 2022, 58(10): 1261-1270.
[9] 丁宁, 王云峰, 刘轲, 朱训明, 李淑波, 杜文博. 高应变速率多向锻造Mg-8Gd-1Er-0.5Zr合金的微观组织、织构及力学性能[J]. 金属学报, 2021, 57(8): 1000-1008.
[10] 颜孟奇, 陈立全, 杨平, 黄利军, 佟健博, 李焕峰, 郭鹏达. 热变形参数对TC18钛合金β相组织及织构演变规律的影响[J]. 金属学报, 2021, 57(7): 880-890.
[11] 左良, 李宗宾, 闫海乐, 杨波, 赵骧. 多晶Ni-Mn-X相变合金的织构化与功能行为[J]. 金属学报, 2021, 57(11): 1396-1415.
[12] 许占一, 沙玉辉, 张芳, 章华兵, 李国保, 储双杰, 左良. 取向硅钢二次再结晶过程中的取向选择行为[J]. 金属学报, 2020, 56(8): 1067-1074.
[13] 梁孟超, 陈良, 赵国群. 人工时效对2A12铝板力学性能和强化相的影响[J]. 金属学报, 2020, 56(5): 736-744.
[14] 于雷,罗海文. 部分再结晶退火对无取向硅钢的磁性能与力学性能的影响[J]. 金属学报, 2020, 56(3): 291-300.
[15] 程超,陈志勇,秦绪山,刘建荣,王清江. TA32钛合金厚板的微观组织、织构与力学性能[J]. 金属学报, 2020, 56(2): 193-202.