| [111]取向镍基单晶合金在蠕变期间组织演化的有限元分析 |
| 张姝1, 2,田素贵1,于慧臣3,于莉丽1,于兴福1 |
1. 沈阳工业大学材料科学与工程学院, 沈阳 110870
2. 沈阳化工大学机械工程学院, 沈阳 110142
3. 北京航空材料研究院, 北京 100095 |
|
| MICROSTRUCTURE EVOLUTION AND FEM ANALYSIS OF [111] ORIENTED SINGLE CRYSTAL OF A NICKEL-BASED SUPERALLOY DURING TENSILE CREEP |
| ZHANG Shu1,2, TIAN Sugui1, YU Huichen3, YU Lili1, YU Xingfu1 |
1. School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870
2. School of Mechanical Engineering, Shenyang University of Chemical Technology, Shenyang 110142
3. Beijing Institute of Aeronautical Material, Beijing 100095 |
引用本文:
张姝,田素贵,于慧臣,于莉丽,于兴福. [111]取向镍基单晶合金在蠕变期间组织演化的有限元分析[J]. 金属学报, 2012, 48(5): 561-568.
,
,
,
,
.
MICROSTRUCTURE EVOLUTION AND FEM ANALYSIS OF [111] ORIENTED SINGLE CRYSTAL OF A NICKEL-BASED SUPERALLOY DURING TENSILE CREEP[J]. Acta Metall Sin, 2012, 48(5): 561-568.
| [1] Peng Z F, Yan Y H. Acta Metall Sin, 1997; 9: 1147 (彭志方, 严演辉. 金属学报, 1997; 9: 1147)[2] Sass V, Glatzel U, Feller--Kniepmeier M. Superalloy 1996, Metals Park: TMS, 1996: 283[3] Tien J K, Copley S M. Metall Trans, 1971; 2: 215[4] Tien J K, Copley S M. Metall Trans, 1971; 2: 543[5] Liu J L, Jin T, Sun X F. Mater Sci Eng, 2008; A479: 277[6] Yue Z F, Lu Z Z. Mater Sci Technol, 1998; 6(2): 48 (岳珠峰, 吕震宙. 材料科学与工艺, 1998; 6(2): 48)[7] Pollock T M, Argon A S. Acta Metall Mater, 1994; 42: 1859[8] Pollock T M, Argon A S. Acta Metall Mater, 1992; 40: 1[9] Muller L, Glatzel U, Feller--Kniepmeier M. Acta Metall Mater, 1992; 40: 1321[10] Glatzel U, Feller--Kniepmeier M. Scr Metall, 1989; 23: 1839[11] Yang Y Q, Zhou L, Zhang J Y. J Shenyang Ligong Univ, 2009; 28(3): 42 (杨永清, 周丽, 张嘉易. 沈阳理工大学学报, 2009; 28(3): 42)[12] Wang M G. PhD Thesis, Shenyang University of Technology, 2010 (王明罡. 沈阳工业大学博士学位论文, 2010)[13] Rao S Q, Meng C L, Wu B. J Aerosp Power, 1998; 13(1): 30 (饶寿期, 孟春玲, 吴斌. 航空动力学报, 1998; 13(1): 30)[14] Rao S Q. Aircr Eng, 2004; 30(1): 10 (饶寿期. 航空发动机, 2004; 30(1): 10)[15] Meng C L, Wu B, Rao S Q. J Beijing Univ Aeronaut Astronaut, 1998; 24(1): 21 (孟春玲, 吴斌, 饶寿期. 北京航空航天大学学报, 1998; 24(1): 21)[16] Tian S G, Chen C R, Zhang J H. Mater Sci Technol, 2001; 17: 736[17] Zhou L, Li S X, Chen C R. Z Metallkd, 2002; 93: 315[18] Tian S G, Zhang J H, Yang H C, Hu Z Q. Mater Sci Technol, 2000; 16: 451[19] Tian S G, Zhou H H, Zhang J H. Acta Metall Sin, 1998; 34: 1261 (田素贵, 周惠华, 张静华. 金属学报, 1998; 34: 1261)[20] Zhang S, Tian S G. Acta Metall Sin, 2011; 47: 61 (张姝, 田素贵. 金属学报, 2011; 47: 61)[21] Tian S G, Zhang J H, Yang H C, Hu Z Q. Mater Sci Technol, 2001; A279: 160 |
|