| 小冲杆测试辐照对反应堆压力容器钢力学性能的影响 |
| 钟巍华, 佟振峰, 张长义, 乔建生, 杨文 |
| 中国原子能科学研究院, 北京 102413 |
|
| SMALL PUNCH TESTING OF THE EFFECT OF IRRADIATION ON MECHANICAL PROPERTY OF RPV STEEL |
| ZHONG Weihua, TONG Zhenfeng, ZHANG Changyi, QIAO Jiansheng, YANG Wen |
| China Institute of Atomic Energy, Beijing 102413 |
引用本文:
钟巍华 佟振峰 张长义 乔建生 杨文. 小冲杆测试辐照对反应堆压力容器钢力学性能的影响[J]. 金属学报, 2011, 47(9): 1205-1209.
,
.
SMALL PUNCH TESTING OF THE EFFECT OF IRRADIATION ON MECHANICAL PROPERTY OF RPV STEEL[J]. Acta Metall Sin, 2011, 47(9): 1205-1209.
| [1] Mnahan M P, Argon A S, Harling O K. J Nucl Mater, 1981; 103-104: 1545[2] Huang F H, Hamilton M L, Wire G L. J Nucl Technol, 1982; 57: 234[3] Manahan M P. J Nucl Technol, 1983; 63: 295[4] Lucas G E, Sheckherd J W, Odette G R. J Nucl Mater, 1984; 122: 429[5] Misawa T, Adachi T, Satto M, Hamaguchi Y. J Nucl Mater, 1987; 212: 202[6] Kameda J, Mao X. J Mater Sci, 1992; 27: 983[7] Foulds J R, Viswanathan R. J Eng Mater Technol, 1994; 116: 457[8] Ha J S, Fleury E. Int J Press Vessel Pip, 1998; 75: 707[9] Bulloch J H. Eng Fail Analy, 2004; 11: 635[10] Jia X J, Dai Y. J Nucl Mater, 2003; 323: 360[11] Han H, Wang Z W, Guang K S. Press Vessel Technol, 2004; 21(10): 14(韩浩, 王志文, 关凯书. 压力容器, 2004; 21(10): 14)[12] Hui H, Han H,Wang ZW, Li P N. Press Vessel Technol, 2009; 26(1): 1(惠虎, 韩浩, 王志文, 李培宁. 压力容器, 2009; 26(1): 1)[13] Wang Z X, Shi H J, Lu J, Shi P, Ma X F. J Nucl Eng Des, 2008; 238: 3186[14] Ding K Q, Shou B N, Wu Y L. J Exp Mech, 2008; 23(6): 539(丁克勤, 寿比南, 吴永礼. 实验力学, 2008; 23(6): 539)[15] Finarelli D, Carsughi F, Jung P. J Nucl Mater, 2008; 337: 65 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|