| 光电化学法研究镍基合金在288℃高温水中生成氧化膜的半导体性质 |
| 张胜寒, 檀玉, 梁可心 |
| 华北电力大学环境科学与工程学院, 保定 071003 |
|
| PHOTOELECTROCHEMICAL STUDY ON SEMICONDUCTOR PROPERTIES OF Ni-BASED ALLOYS OXIDE FILMS FORMED IN 288℃ HIGH TEMPERATURE WATER |
| ZHANG Shenghan, TAN Yu, LIANG Kexin |
| School of Environmental Science and Engineering, North China Electric Power University, Baoding 071003 |
引用本文:
张胜寒 檀玉 梁可心. 光电化学法研究镍基合金在288℃高温水中生成氧化膜的半导体性质[J]. 金属学报, 2011, 47(9): 1147-1152.
,
,
.
PHOTOELECTROCHEMICAL STUDY ON SEMICONDUCTOR PROPERTIES OF Ni-BASED ALLOYS OXIDE FILMS FORMED IN 288℃ HIGH TEMPERATURE WATER[J]. Acta Metall Sin, 2011, 47(9): 1147-1152.
| [1] Hamadou L, Kadri A, Benbrahim N, Petit J P. J Electrochem Soc, 2007; 154: 291[2] Rangel C M, Silva T M, da Cunha Belo M. Electrochim Acta, 2005; 50: 5076[3] Cheng Y F, Luo J L. Electrochim Acta, 1999; 44: 2947[4] Schmuki P, B¨ohni H. J Electrochem Soc, 1992; 139: 1908[5] Maurice V, YangWP, Marcus P. J Electrochem Soc, 1998; 145: 909[6] Asami K, Hashimoto K, Shimodaira S. Corros Sci, 1978; 18: 151[7] Sennour M, Marchetti L, Perrin S, Molins R, Pijolat M, Raquet O. Mater Sci Forum, 2008; 595: 539[8] Sudensh T L, Wijesinghe L, Blackwood D J. Corros Sci, 2008; 50: 23[9] Mac´ak J, Sajdl P, Kuˇcera P, Novotn´y R, Voˇsta J. Electrochim Acta, 2006; 51: 3566[10] Carette F, Lafont M C, Chataignier G, Guinard L, Pieraggi B. Surf Interface Anal, 2002; 34: 135[11] Carette F, Lafont M C, Guinard L, Pieraggi B. Mater High Temp, 2003; 20: 581[12] Machet A, Galtayries A, Zanna S, Klein L, Maurice V, Jolivet P, Foucault M, Combrade P, Scott P, Marcus P. Electrochim Acta, 2004; 49: 3957[13] Montemor M F, Ferreira M G, Hakiki N E, da Cunha Belo M D. Corros Sci, 2000; 42: 1635[14] Fujimoto S, Chihara O, Shibata T. Mater Sci Forum, 1998; 289–292: 989[15] Tsuchiya H, Fujimoto S, Chihara O, Shibata T. Electrochim Acta, 2002; 47: 4357[16] Henry S, Mougin J,Wouters Y, Petit J P, Galerie A. Mater High Temp, 2000; 17: 231[17] Calvarin G, Huntz A M, Molins R. Mater High Temp, 2000; 17: 257[18] Balaji S, Kalai S R, John B L, Angappan S, Subramanian K, Augustin C O. Mater Sci Eng, 2005; B119: 119[19] Sunseri O, Piazza S, Di Quarto F. J Electrochem Soc, 1990; 137: 2411[20] Carpenter M K, Corrigan D A. J Electrochem Soc, 1989; 136: 1022[21] Marchetti L, Perrin S, Raquet O, Pijolat M. Mater Sci Forum, 2008; 595–598: 529[22] Marchetti L, Perrin S, Wouters Y, Martin F, Pijolat M. Electrochim Acta, 2010; 55: 5384[23] Yves Marfaing. J Cryst Growth, 1996; 1–4: 205[24] Sarrazin P, Galerie A, Fouletier J. Mechanisms of High Temperature Corrosion: A Kinetic Approach, Zurich: Trans Tech Publications Ltd., 2008, 488[25] Macdonald D D. J Electrochem Soc, 1992; 139: 3434 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|