| Ni-xCr-10Al合金于700-800℃的氧化-硫化腐蚀 |
| 卢兰英1,潘太军2,牛焱1 |
1. 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016
2. 常州大学材料科学与工程学院, 常州 213164 |
|
| OXIDIZING–SULFIDIZING CORROSION OF Ni–xCr–10Al ALLOYS AT 700—800 ℃ |
| LU Lanying 1, PAN Taijun 2, NIU Yan 1 |
1. State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2. Department of Material Science and Engineering, Changzhou University, Changzhou 213164 |
引用本文:
卢兰英 潘太军 牛焱. Ni-xCr-10Al合金于700-800℃的氧化-硫化腐蚀[J]. 金属学报, 2011, 47(8): 1026-1031.
,
,
.
OXIDIZING–SULFIDIZING CORROSION OF Ni–xCr–10Al ALLOYS AT 700—800 ℃[J]. Acta Metall Sin, 2011, 47(8): 1026-1031.
| [1] Natesan K. Corrosion, 1985; 41: 646[2] Gesmundo F, Young D J, Roy S K. High Temp Mater Process, 1989; 8: 149[3] Stringer J. In: Embury J D ed., High–Temperature Oxidation and Sulfidation Processes. New York: Pergamon Press, 1990: 257[4] Mrowec S, Przybylski K. High Temp Mater Process, 1984; 6: 1[5] Mrowec S, Przybylski K. Oxid Met, 1985; 23: 107[6] He Y R, Douglass D L, Gesmundo F. Oxid Met, 1992; 37: 413[7] He Y R, Douglass D L, Gesmundo F. Oxid Met, 1992; 37: 217[8] Niu Y, Gesmundo F, Viani F. Corros Sci, 1994; 36: 1885[9] Niu Y, Gesmundo F, Viani F, Rizzo F. Corros Sci, 1994; 36: 1973[10] Fu G Y, Niu Y, Wu W T. Trans Nonferrous Met Soc China, 2002; 12: 874[11] Fu G Y, Niu Y, Wu W T. Chin Rare Earth, 2002; 23: 16(付广艳, 牛焱, 吴维tao. 稀土, 2002; 23: 16)[12] Fu G Y, Niu Y, Wu W T. Rare Met Mater Eng, 2004; 33:417(付广艳, 牛焱, 吴维tao. 稀有金属材料与工程, 2004; 33: 417)[13] Fu G Y, Niu Y, Wu W T. Acta Metall Sin, 1999; 35: 221(付广艳, 牛焱, 吴维tao. 金属学报, 1999; 35: 221)[14] Regina J R, DuPont J N, Marder A R. Mater Sci Eng, 2005; A404: 71[15] Regina J R, DuPont J N, Marder A R. Mater Sci Eng, 2005; A405: 102[16] KaiW, ChangMT, Liu C D, Chiang D L, Chu J P. Mater Sci Eng, 2002; A329: 734[17] Kai W, Chu J P, Huang R T, Lee P Y. Mater Sci Eng, 1997; A39: 859[18] Brady M P, Tortorelli P F, More K L, Walker L R. Oxid Met, 2010; 74: 1[19] Zhang X J, Wang S Y, Gesmundo F, Niu Y. Oxid Met, 2006; 65: 151[20] Niu Y, Zhang X J, Wu Y, Gesmundo F. Corros Sci, 2006; 48: 4020[21] Giggins C S, Petti F S. J Electrochem Soc, 1971; 118: 1782[22] Stott F H, Wood G C. Corros Sci, 1971; 11: 799[23] Kostad p. High Temperature Corrosion, London: Eleviser, 1988: 425[24] Giggins C S, Pettit F S. Oxid Met, 1980; 14: 363[25] He Y R, Douglass D L. Oxid Met, 1993; 40: 337[26] Kai W, Huang R T. Oxid Met, 1997; 48: 59[27] Devan J H, Tortorelli P F. Corros Sci, 1993; 35: 1065 |
|